公开(公告)号:US5588977A
公开(公告)日:1996-12-31
申请号:US467638
申请日:1995-06-06
CPC分类号: C03B19/108 , C03B19/1095 , C03B32/02 , C03B5/005 , C03C1/002 , C03C11/00 , C03C3/085
摘要: A method of obtaining glass materials from ash-slag. Waste wherein the waste is heated to a melting point temperature and melted in a reducing medium. The obtained melt is cooled by a thermal shock to form a foamed glass material. Prior to heating the charge, the carbon content therein is brought to 3.0-8.0 wt %, and the foamed glass material is foamed under a flow of a gaseous medium resulting form decomposition of carbides formed in the melt as a result of carbon content adjustment. Carbon addition also reduces iron oxide present in the waste, this reduction facilitating iron separation from the foamed material.
摘要翻译: 从灰渣获得玻璃材料的方法。 将废物加热到熔点温度并在还原介质中熔化的废物。 将获得的熔体通过热冲击冷却以形成泡沫玻璃材料。 在加热电荷之前,将其中的碳含量设为3.0-8.0重量%,并且由于碳含量调节,发泡玻璃材料在气态介质的流动下发泡,从而形成在熔体中形成的碳化物分解。 碳添加还减少废物中存在的氧化铁,这种还原促进了铁与泡沫材料的分离。