公开(公告)号:US5858315A
公开(公告)日:1999-01-12
申请号:US591660
申请日:1996-04-24
摘要: A portion of the concentrates is roasted and a portion of the resulting calcine is subjected to a neutral leaching step. Another portion of the concentrates is directly leached in an acidic medium in the presence of oxygen and under atmospheric conditions together with at least a portion of the neutral leaching residue. The zinc- and iron-rich solution resulting from acid leaching is neutralised with another portion of the calcine, the iron is removed and the solution is reused in the neutral leaching step. The method enables a gradual increase in the capacity of an existing zinc plant in accordance with demand, while capital costs may advantageously be spread out over time.
摘要翻译: PCT No.PCT / EP94 / 02794 Sec。 371日期:1996年4月24日 102(e)日期1996年4月24日PCT 1994年8月24日PCT公布。 公开号WO95 / 06140 日期1995年3月2日将浓缩物的一部分焙烧,并将一部分所得的煅烧物进行中性浸出步骤。 浓缩物的另一部分在氧气存在下和酸性介质中直接浸出在大气条件下以及至少一部分中性浸出残渣。 由酸浸出产生的富含锌和铁的溶液被另一部分煅烧物中和,除去铁,并将溶液重新用于中性浸出步骤。 该方法能够根据需求逐渐增加现有锌厂的能力,同时资本成本可以有利地随着时间的推移而扩散。