Methods for preparing positive electrode material for rechargeable lithium ion batteries

    公开(公告)号:US12255326B2

    公开(公告)日:2025-03-18

    申请号:US17041022

    申请日:2019-03-13

    Abstract: A method for preparing a powderous positive electrode material comprising single crystal monolithic particles and having a general formula
    Li1+a((Niz(Ni1/2Mn1/2)yCox)1-k Ak)1-aO2, wherein A is a dopant, −0.03≤a≤0.06, 0.05≤x≤0.35, 0.10≤z≤0.95, x+y+z=1 and k≤0.05 is described. The method comprises providing a mixture comprising a Ni- and Co- bearing precursor and a Li bearing precursor, subjecting the mixture to a multiple step sintering process whereby in the final sintering step a sintered lithiated intermediate material is obtained comprising agglomerated primary particles having a primary particle size distribution with a D50 between 2.0 and 8.0 μm, subjecting the lithiated intermediate material to a wet ball milling step to deagglomerate the agglomerated primary particles and obtain a slurry comprising deagglomerated primary particles, separating the deagglomerated primary particles from the slurry, and heat treating the deagglomerated primary particles at a temperature between 300° C. and at least 20° C. below the temperature in the final sintering step.

    LITHIUM NICKEL MANGANESE COBALT COMPOSITE OXIDE AS A POSITIVE ELECTRODE ACTIVE MATERIAL FOR RECHARGEABLE LITHIUM ION BATTERIES

    公开(公告)号:US20220271328A1

    公开(公告)日:2022-08-25

    申请号:US17623720

    申请日:2020-07-02

    Abstract: A positive electrode active material powder suitable for lithium-ion batteries, comprising lithium transition metal-based oxide particles, said particles comprising a core and a surface layer, said surface layer being on top of said core, said particles comprising the elements: Li, M′ and oxygen, wherein M′ has a formula: M′=NizMnyCoxAk, wherein A is a dopant, 0.60≤z≤0.90, 0.05≤y≤0.20, 0.05≤x≤0.20, x+y+z+k=1, and k≥0.01, said positive electrode active material powder having a median particle size D50 ranging from 5 μm to 15 μm, a span ranging from 0.25 to 0.90, and a surface layer thickness ranging from 10 nm to 200 nm, said surface layer comprising: sulfur in a content superior or equal to 0.150 wt % and inferior or equal to 0.375 wt % with respect to the total weight of the positive electrode active material powder, and sulfate ion (SO42−) in a content superior or equal to 4500 ppm and inferior or equal to 11250 ppm.