公开(公告)号:US06835250B2
公开(公告)日:2004-12-28
申请号:US10258954
申请日:2002-10-29
申请人: Yutaka Hiratsu , Toshio Kiyokawa , Atsuo Toutsuka
发明人: Yutaka Hiratsu , Toshio Kiyokawa , Atsuo Toutsuka
IPC分类号: B23K3524
CPC分类号: C01F5/02 , C01P2004/40 , C01P2004/50 , C01P2006/14 , C01P2006/16 , C21D8/1283 , H01F1/18
摘要: An object of the present invention is to provide a magnesium oxide particle aggregate having a controlled particle aggregation structure so that the solid phase-solid phase reaction between magnesium oxide and the SiO2 film on the surface can be appropriately controlled. The object can be achieved by a magnesium oxide particle aggregate characterized in that a first inflection point diameter is 0.30×10−6 m or less, an interparticle void volume is 1.40×10−3 to 2.20×10−3 m3/kg and a particle void volume is 0.55×10−3 to 0.80×10−3 m3/kg in a cumulative intrusion volume curve of the particle aggregate.
-
公开(公告)号:US06899768B2
公开(公告)日:2005-05-31
申请号:US10415168
申请日:2001-10-25
申请人: Atsuo Toutsuka , Yutaka Hiratsu
发明人: Atsuo Toutsuka , Yutaka Hiratsu
CPC分类号: C21D8/1283 , C01F5/02 , C01P2004/50 , C01P2006/14 , C01P2006/16 , H01F1/18
摘要: The present invention is related to a magnesium oxide particle aggregate with the requirement of a first inflection point diameter is more than 0.30×10−6 to 0.60×10−6 m, a particle void volume is 0.50×10−3 to 0.90×10−3 m3·kg−1, and a micropore volume is 0.04×10−3 to 0.11×10−3 m3·kg−1 in the cumulative intrusion volume curve of said particle by having controlled particle aggregation structure so that the solid phase-solid phase reaction between magnesium oxide and the SiO2 film on the surface can be appropriately controlled.
摘要翻译: 本发明涉及氧化镁颗粒聚集体,其要求第一拐点直径大于0.30×10 -6至0.60×10 -6 m,颗粒 空隙体积为0.50×10 -3至0.90×10 -3 -3 3×10 -3,以及微孔 在累积入侵体积中的体积为0.04×10 -3 -3.0×10 -3 -3 / 所述颗粒的曲线通过具有受控的颗粒聚集结构使得可以适当地控制表面上的氧化镁和SiO 2膜之间的固相 - 固相反应。
-