摘要:
A method using a continuous annealing furnace where a cooling method of a cooling zone including part or all of the temperature range of the steel sheet of 600 to 250° C. following the heating for recrystallization is one or more of gas cooling, effusion cooling, and cooling pipe cooling, or a joint cold rolled steel sheet/hot dip galvanized steel sheet facility having such a continuous annealing furnace, to continuously anneal cold rolled steel sheet to produce high strength cold rolled steel sheet, characterized by exposing the steel sheet surface to an iron-oxidizing atmosphere in the steel sheet temperature range to make the surface oxidize, pickling the sheet at the outlet side of the annealing furnace, then iron- or Ni-plating the sheet to 1 to 50 mg/m2.
摘要翻译:使用连续退火炉的方法,其中在再结晶加热之后,包括600-250℃的钢板的部分或全部温度范围的冷却区域的冷却方法是气体冷却,渗出冷却, 冷却管冷却的冷轧钢板或具有这种连续退火炉的接合冷轧钢板/热浸镀锌钢板设备连续退火冷轧钢板以生产高强度冷轧钢板,其特征在于将钢板表面暴露于 在钢板温度范围内的铁氧化气氛,使表面氧化,在退火炉的出口侧酸洗,然后对该片进行铁或镍镀覆至1〜50mg / m 2。
摘要:
A method using a continuous annealing furnace where a cooling method of a cooling zone including part or all of the temperature range of the steel sheet of 600 to 250° C. following the heating for recrystallization is one or more of gas cooling, effusion cooling, and cooling pipe cooling, or a joint cold rolled steel sheet/hot dip galvanized steel sheet facility having such a continuous annealing furnace, to continuously anneal cold rolled steel sheet to produce high strength cold rolled steel sheet, characterized by exposing the steel sheet surface to an iron-oxidizing atmosphere in the steel sheet temperature range to make the surface oxidize, pickling the sheet at the outlet side of the annealing furnace, then iron- or Ni-plating the sheet to 1 to 50 mg/m2.
摘要翻译:使用连续退火炉的方法,其中在再结晶加热之后,包括600-250℃的钢板的部分或全部温度范围的冷却区域的冷却方法是气体冷却,渗出冷却, 冷却管冷却的冷轧钢板或具有这种连续退火炉的接合冷轧钢板/热浸镀锌钢板设备连续退火冷轧钢板以生产高强度冷轧钢板,其特征在于将钢板表面暴露于 在钢板温度范围内的铁氧化气氛,使表面氧化,在退火炉的出口侧酸洗,然后对该片进行铁或镍镀覆至1〜50mg / m 2。