公开(公告)号:US20240368032A1
公开(公告)日:2024-11-07
申请号:US18775847
申请日:2024-07-17
Applicant: AGC Inc.
Inventor: Yusuke FUJIWARA , Yoichi TAKATO , Yusuke KOBAYASHI , Masao OZEKI , Yusuke MORISHIMA , Takumi NAGASAKO
IPC: C03C21/00 , C03C3/083 , C03C19/00 , H01L31/048
Abstract: A chemically strengthened glass has a thickness of more than 2 mm, a surface compressive stress CS0 of 400 MPa to 1200 MPa, a depth of compressive stress layer DOL-tail of 2.7 μm to 30.0 μm, an absolute value of an average slope of a stress profile from a surface to the DOL-tail of 20 MPa/μm to 500 MPa/μm, and a tensile stress CT of 1.0 MPa to 16 MPa.
-
公开(公告)号:US20230271879A1
公开(公告)日:2023-08-31
申请号:US18174179
申请日:2023-02-24
Applicant: AGC Inc.
Inventor: Yusuke FUJIWARA , Yoichi TAKATO , Yusuke KOBAYASHI
CPC classification number: C03C21/002 , C03C10/0027
Abstract: The present invention relates to a chemically strengthened glass, satisfying: a ratio ICS (≥400)/ICS being more than 0.13 in a stress profile, the ICS representing an integrated value of compressive stress in a region from a surface of the glass to a depth where the compressive stress becomes 0 in the stress profile, and the ICS (≥400) representing an integrated value of compressive stress in a region from a depth of 400 μm from the surface of the glass to the depth where the compressive stress becomes 0 in the stress profile.
-
公开(公告)号:US20210147279A1
公开(公告)日:2021-05-20
申请号:US17093121
申请日:2020-11-09
Applicant: AGC Inc.
Inventor: Yusuke KOBAYASHI , Izuru KASHIMA , Kazutaka ONO , Seiji INABA , Hirofumi YAMAMOTO , Kiyoshi TAMAI
Abstract: A supporting glass substrate includes a compression stress layer on a surface thereof, and has an average thermal expansion coefficient at 50° C. to 200° C. that is 7 ppm/° C. to 15 ppm/° C., an internal tensile stress that is 5 MPa to 55 MPa, and a depth of the compression stress layer that is 10 μm to 60 μm.
-
公开(公告)号:US20240360032A1
公开(公告)日:2024-10-31
申请号:US18768142
申请日:2024-07-10
Applicant: AGC Inc.
Inventor: Yusuke FUJIWARA , Yoichi TAKATO , Yusuke KOBAYASHI , Masao OZEKI , Yusuke MORISHIMA , Takumi NAGASAKO
IPC: C03C21/00 , C03C3/076 , H01L31/048
CPC classification number: C03C21/002 , C03C3/076 , H01L31/0481 , C03C2204/00
Abstract: A chemically strengthened glass has a thickness of more than 2 mm, a surface compressive stress CS0 of 400 MPa to 1200 MPa, a depth of compressive stress layer DOL-tail of 2.7 μm to 30.0 μm, an absolute value of an average slope of a stress profile from a surface to the DOL-tail of 20 MPa/μm to 500 MPa/μm, and a tensile stress CT of 1.0 MPa to 16 MPa.
-
-
-