公开(公告)号:US20240360032A1
公开(公告)日:2024-10-31
申请号:US18768142
申请日:2024-07-10
Applicant: AGC Inc.
Inventor: Yusuke FUJIWARA , Yoichi TAKATO , Yusuke KOBAYASHI , Masao OZEKI , Yusuke MORISHIMA , Takumi NAGASAKO
IPC: C03C21/00 , C03C3/076 , H01L31/048
CPC classification number: C03C21/002 , C03C3/076 , H01L31/0481 , C03C2204/00
Abstract: A chemically strengthened glass has a thickness of more than 2 mm, a surface compressive stress CS0 of 400 MPa to 1200 MPa, a depth of compressive stress layer DOL-tail of 2.7 μm to 30.0 μm, an absolute value of an average slope of a stress profile from a surface to the DOL-tail of 20 MPa/μm to 500 MPa/μm, and a tensile stress CT of 1.0 MPa to 16 MPa.
-
公开(公告)号:US20240368032A1
公开(公告)日:2024-11-07
申请号:US18775847
申请日:2024-07-17
Applicant: AGC Inc.
Inventor: Yusuke FUJIWARA , Yoichi TAKATO , Yusuke KOBAYASHI , Masao OZEKI , Yusuke MORISHIMA , Takumi NAGASAKO
IPC: C03C21/00 , C03C3/083 , C03C19/00 , H01L31/048
Abstract: A chemically strengthened glass has a thickness of more than 2 mm, a surface compressive stress CS0 of 400 MPa to 1200 MPa, a depth of compressive stress layer DOL-tail of 2.7 μm to 30.0 μm, an absolute value of an average slope of a stress profile from a surface to the DOL-tail of 20 MPa/μm to 500 MPa/μm, and a tensile stress CT of 1.0 MPa to 16 MPa.
-