公开(公告)号:US10726550B2
公开(公告)日:2020-07-28
申请号:US15563064
申请日:2016-03-30
Applicant: Amorepacific Corporation
Inventor: Choon Bok Jeong , Se Jun Park , Yu Jin Kang , Kyung Ho Choi , Yeong Jin Choi
Abstract: The present invention provides a method for proposing personalized cosmetics and a system for implementing the same, the method comprising the steps of: photographing the visible spectrum of the skin of a subject to be measured; mapping a personalized visible spectrum to the measured visible spectrum of the skin so as to generate a spectral comparison table; matching a personalized composition to the spectral comparison table; and displaying the matched personalized composition on an image display unit.
-
公开(公告)号:US10278903B2
公开(公告)日:2019-05-07
申请号:US15555863
申请日:2015-11-24
Applicant: AMOREPACIFIC CORPORATION
Inventor: Hyun Suk Lee , Yong Jin Kim , Jon Hwan Lee , Se Jun Park , Kyung Ho Choi , Yeong Jin Choi , Sung-Wook Choi , Dong-Hyun Paik
IPC: A61K8/29 , A61K8/02 , A61K8/27 , A61K8/19 , A61K8/81 , A61Q1/02 , C08J3/12 , A61K8/26 , A61Q1/00 , A61Q1/12
Abstract: The present invention relates to composite powder having enhanced water repellency and oil absorbency by means of even impregnation of inorganic powder particles with a super-water-repellent porous polymer. The composite powder prepared by means of a one-step spraying procedure of electro-spraying or spray drying, according to the present invention, shows super water repellency and maximized oil absorbency by means of increased porosity of porous polymethyl methacrylate (PMMA) and even impregnation with titanium dioxide (TiO2) nanoparticles.
-
公开(公告)号:US10576024B2
公开(公告)日:2020-03-03
申请号:US15740398
申请日:2016-06-30
Applicant: Amorepacific Corporation
Inventor: Se Jun Park
Abstract: A makeup cosmetic composition contains a first composite powder and a second composite powder, wherein the first composite powder and the second composite powder are plate-like powders coated in a coating layer. The first composite powder contains a coating layer having an average thickness of 20 to 70 nm, and the second composite powder contains a coating layer having an average thickness of 74 to 104 nm.
-
-