CRACK-CONTAINING HOT-STAMPED COATED STEEL PART WITH EXCELLENT SPOT-WELDABILITY AND EXCELLENT PAINTING ADHESION

    公开(公告)号:US20250034684A1

    公开(公告)日:2025-01-30

    申请号:US18811753

    申请日:2024-08-21

    Applicant: ArcelorMittal

    Abstract: A hot-stamped coated steel part includes a steel substrate and an aluminum alloy coating comprising, proceeding from steel substrate outwards, an interdiffusion layer and an outer layer. The total thickness of the coating ecoating and the thickness of the interdiffusion layer eIDL satisfy the following condition: with 40 ≤ E pc ≤ 80 E pc = ( 33.3 - e IDL 0.9 + e IDL - e coating ) 2 - 148 ⁢ ( e IDL - e coating ) - ( 33.3 - e IDL 0.9 + e IDL - E coating ) The hot-stamped coated steel part comprises an undeformed portion having a thickness ePflat from 0.6 mm to 3.5 mm, and at least one deformed portion. A lineic density of cracks dC in the coating in the undeformed portion is higher than or equal to a minimum lineic density of cracks dCmin(ePflat) defined as: dc min ( e pflat ) - 15.5 + 91 * e - 7.44 - 2.88 * arctan ⁡ ( 5.49 * ( e pflat - 1.71 ) ) - 106.5 * e - 8.62 - 3.34 * arctan ⁡ ( 5.49 * ( e pflat - 1.71 ) )

    HOT FORMED PRE-COATED STEEL PART
    3.
    发明申请

    公开(公告)号:US20210395853A1

    公开(公告)日:2021-12-23

    申请号:US17463128

    申请日:2021-08-31

    Applicant: ArcelorMittal

    Abstract: A hot formed pre-coated steel part includes a steel sheet precoated with a metallic coating and hot formed, the coating including: 2.0 to 24.0% by weight of zinc; 1.1 to 7.0% by weight of silicon; optionally from 0.5 to 3.0% by weight of magnesium when the amount of silicon is between 1.1 and 4.0%, and optionally additional elements chosen from Pb, Ni, Zr or Hf, a content by weight of each additional element being less than 0.3% by weight, a balance being aluminum, unavoidable impurities and residual elements resulting from feeding ingots or from a passage of the steel sheet in a molten bath; and a ratio Al/Zn by weight greater than 2.9, where a microstructure in the steel after said hot forming being martensitic or martensitic-bainitic or made of at least 75% of equiaxed ferrite, 5 to 20% of martensite and bainite in an amount less than or equal to 10%.

    CRACK-CONTAINING HOT-STAMPED COATED STEEL PART WITH EXCELLENT SPOT-WELDABILITY AND EXCELLENT PAINTING ADHESION

    公开(公告)号:US20250114837A1

    公开(公告)日:2025-04-10

    申请号:US18757440

    申请日:2024-02-09

    Applicant: ArcelorMittal

    Abstract: A hot-stamped coated steel part includes a steel substrate and an aluminum alloy coating comprising, proceeding from steel substrate outwards, an interdiffusion layer and an outer layer. The total thickness of the coating ecoating and the thickness of the interdiffusion layer eIDL satisfy the following condition: 4 ⁢ 0 ≤ E p ⁢ c ≤ 80 with E p ⁢ c = ( 3 ⁢ 3 . 3 - e IDL 0 . 9 + e IDL - e c ⁢ o ⁢ a ⁢ t ⁢ i ⁢ n ⁢ g ) 2 - 1 ⁢ 4 ⁢ 8 ⁢ ( e IDL - e c ⁢ o ⁢ a ⁢ t ⁢ i ⁢ n ⁢ g ) - ( 3 ⁢ 3 . 3 - e IDL 0 . 9 + e IDL - e c ⁢ o ⁢ a ⁢ t ⁢ i ⁢ n ⁢ g ) The hot-stamped coated steel part comprises an undeformed portion having a thickness ePflat from 0.6 mm to 3.5 mm, and at least one deformed portion. A lineic density of cracks dC in the coating in the undeformed portion is higher than or equal to a minimum lineic density of cracks dCmin(ePflat) defined as: d ⁢ C min ( e p ⁢ flat ) = 1 ⁢ 5 . 5 + 9 ⁢ 1 * e - 7.44 - 2 . 8 ⁢ 8 * arctan ( 5.49 * ( e pflat - 1.7 1 ) ) - 1 ⁢ 0 6.5 * e - 8.62 - 3 . 3 ⁢ 4 * arctan ( 5.49 * ( e pflat - 1.71 ) )