Abstract:
A method for producing a metal sheet is provided. The method includes providing a steel substrate having two faces coated by dipping the substrate in a bath, applying an acid solution with a pH comprised between 1 and 4 on the outer surfaces of the metal coatings and applying an adhesive locally on at least one outer surface of a metal coating.
Abstract:
A method is provided. The method includes providing a steel substrate having two faces coated by dipping the substrate in a bath, altering layers of magnesium oxide or magnesium hydroxide formed on the outer surfaces of the metal coatings by applying mechanical forces, rinsing and drying the outer surfaces, applying a conversion solution on the outer surfaces and painting the outer surfaces of the metal coatings. A metal sheet is also provided.
Abstract:
A method is provided. The method includes providing a steel substrate having two faces coated by dipping the substrate in a bath, altering layers of magnesium oxide or magnesium hydroxide formed on the outer surfaces of the metal coatings by applying an acid solution, optionally a conversion solution with a pH between 1 and 2, and/or mechanical forces, and painting the outer surfaces of the metal coatings. Additional methods and a metal sheet are also provided.
Abstract:
A method for manufacturing a steel sheet provided with a coating included from 0.80 to 1.40 wt. % of Al, from 0.80 to 1.40 wt. % of Mg, unavoidable impurities and optionally one or more additional elements selected from Si, Sb, Pb, Ti, Ca, Mn, Sn, La, Ce, Cr, Zr or Bi, the weight content of each additional element in the coating being less than 0.3%, the remainder being Zn, the outer surface of the coated steel sheet having a waviness Wa0.8 before skin-pass of less than or equal to 0.50 μm; the coated steel sheet obtained by this method; the part obtained by deformation of a steel sheet and a land motor vehicle comprising a body, the body including the part.
Abstract:
A metal sheet assembly is provided. The metal sheet assembly includes a first metal sheet having two faces, each face is hot dip coated with a metal coating comprising zinc, from 0.7 to 6 wt % of aluminum and from 0.1 to 10 wt % of magnesium. An acid solution with a pH from 1 to 4 is applied to outer surfaces of the metal coatings. An adhesive locally is applied on at least one acid solution-treated outer surface of the metal coating, the adhesive is selected from structural, reinforced structural or semi-structural adhesives, sealing putties and wedging putties. A second metal sheet is assembled to the first metal sheet via the adhesive.