公开(公告)号:US08058093B2
公开(公告)日:2011-11-15
申请号:US11211656
申请日:2005-08-26
Applicant: Aaron Wadell , Jiangeng Xue
Inventor: Aaron Wadell , Jiangeng Xue
IPC: H01L21/00 , H01L21/31 , H01L21/469 , B05D5/12 , B28B19/00 , B29B15/10 , C23C18/00 , C23C20/00 , C23C24/00 , C23C26/00 , C23C28/00 , C23C30/00 , H01C21/06
CPC classification number: H01L51/448 , H01L27/301 , H01L51/424 , H01L51/441 , Y02E10/549
Abstract: An organic photosensitive optoelectronic device is formed in which the organic photoconductive materials are encapsulated by an electrode of the device. A first transparent film is provided that comprises a first electrically conductive material, arranged on a transparent substrate. A first photoconductive organic material is deposited over the first electrically conductive material. A metal is deposited at an initial rate of no more than 1 nm/s over the first photoconductive organic material, completely covering any exposed portions of the first photoconductive organic material and any exposed interfaces with the first photoconductive organic material to a thickness of no less than 10 nm. After the thickness of no less than 10 nm is obtained, the metal is sputtered at an increased rate at least three times the initial rate until a cumulative thickness of the metal completely covering the previously exposed portions of the first photoconductive organic material and the previously exposed interfaces with the first conductive organic material is at least 250 nm.
Abstract translation: 形成有机光敏光电器件,其中有机光电导材料被器件的电极封装。 提供了第一透明膜,其包括设置在透明基板上的第一导电材料。 第一光导有机材料沉积在第一导电材料上。 在第一光导有机材料上以不超过1nm / s的初始速率沉积金属,完全覆盖第一光电导有机材料的任何暴露部分和与第一光电导有机材料的任何暴露界面,其厚度不小于 超过10nm。 在获得不小于10nm的厚度之后,以增加的速率溅射金属至少是初始速率的三倍,直到金属的累积厚度完全覆盖第一光导有机材料的先前暴露部分和先前暴露的 与第一导电有机材料的界面为至少250nm。
-
公开(公告)号:US20070048892A1
公开(公告)日:2007-03-01
申请号:US11211656
申请日:2005-08-26
Applicant: Aaron Wadell , Jiangeng Xue
Inventor: Aaron Wadell , Jiangeng Xue
IPC: H01L51/40
CPC classification number: H01L51/448 , H01L27/301 , H01L51/424 , H01L51/441 , Y02E10/549
Abstract: An organic photosensitive optoelectronic device is formed in which the organic photoconductive materials are encapsulated by an electrode of the device. A first transparent film is provided that comprises a first electrically conductive material, arranged on a transparent substrate. A first photoconductive organic material is deposited over the first electrically conductive material. A metal is deposited at an initial rate of no more than 1 nm/s over the first photoconductive organic material, completely covering any exposed portions of the first photoconductive organic material and any exposed interfaces with the first photoconductive organic material to a thickness of no less than 10 nm. After the thickness of no less than 10 nm is obtained, the metal is sputtered at an increased rate at least three times the initial rate until a cumulative thickness of the metal completely covering the previously exposed portions of the first photoconductive organic material and the previously exposed interfaces with the first conductive organic material is at least 250 nm.
Abstract translation: 形成有机光敏光电器件,其中有机光电导材料被器件的电极封装。 提供了第一透明膜,其包括设置在透明基板上的第一导电材料。 第一光导有机材料沉积在第一导电材料上。 在第一光导有机材料上以不超过1nm / s的初始速率沉积金属,完全覆盖第一光电导有机材料的任何暴露部分和与第一光电导有机材料的任何暴露界面,其厚度不小于 超过10nm。 在获得不小于10nm的厚度之后,以增加的速率溅射金属至少是初始速率的三倍,直到金属的累积厚度完全覆盖第一光导有机材料的先前暴露部分和先前暴露的 与第一导电有机材料的界面为至少250nm。
-