摘要:
A non-aqueous electrolyte secondary battery including: an electrode group in which a positive electrode and a negative electrode are spirally wound with a separator interposed therebetween; and a non-aqueous electrolyte including a non-aqueous solvent and a lithium salt dissolved in the non-aqueous solvent, the positive electrode including a positive electrode material mixture layer containing a nickel-containing lithium composite metal oxide, wherein a product of A and B equals 150 to 350, A equals 15 to 20%, and B equals 8 to 25%, where A (%) represents a porosity of the positive electrode material mixture layer, and B (%) represents a volume percentage of ethylene carbonate in the non-aqueous solvent.
摘要:
A lithium-containing composite oxide represented by the formula 1: LixNi1-y-z-v-wCoyAlzM1vM2wO2 is used as a positive electrode active material for a non-aqueous electrolyte secondary battery. The element M1 is at least one selected from the group consisting of Mn, Ti, Y, Nb, Mo, and W. The element M2 includes at least two selected from the group consisting of Mg, Ca, Sr, and Ba, and the element M2 includes at least Mg and Ca. The formula 1 satisfies 0.97≦x≦1.1, 0.05≦y≦0.35, 0.005≦z≦0.1, 0.0001≦v≦0.05, and 0.0001≦w≦0.05. The primary particles have a mean particle size of 0.1 μm or more and 3 μm or less, and the secondary particles have a mean particle size of 8 μm or more and 20 μm or less.
摘要翻译:作为非水电解质二次电池用正极活性物质,使用由式1表示的含锂复合氧化物:LixNi1-y-z-v-wCoyAlzM1vM2wO2。 元素M1是选自Mn,Ti,Y,Nb,Mo和W中的至少一种元素。元素M2包括选自Mg,Ca,Sr和Ba中的至少两种元素,并且 元素M2至少包括Mg和Ca。 式1满足0.97 <= x <= 1.1,0.05 <= y <=0.35,0.005≤z≤0.1,0.0001≤v≤0.05,0.0001≤w≤0.05。 初级粒子的平均粒径为0.1μm以上3μm以下,二次粒子的平均粒径为8μm以上且20μm以下。
摘要:
A non-aqueous electrolyte secondary battery including: an electrode group in which a positive electrode and a negative electrode are spirally wound with a separator interposed therebetween; and a non-aqueous electrolyte including a non-aqueous solvent and a lithium salt dissolved in the non-aqueous solvent, the positive electrode including a positive electrode material mixture layer containing a nickel-containing lithium composite metal oxide, wherein a product of A and B equals 150 to 350, A equals 15 to 20%, and B equals 8 to 25%, where A (%) represents a porosity of the positive electrode material mixture layer, and B (%) represents a volume percentage of ethylene carbonate in the non-aqueous solvent.
摘要:
A non-aqueous electrolyte secondary battery including: an electrode group in which a positive electrode and a negative electrode are spirally wound with a separator interposed therebetween; and a non-aqueous electrolyte including a non-aqueous solvent and a lithium salt dissolved in the non-aqueous solvent, the positive electrode including a positive electrode material mixture layer containing a nickel-containing lithium composite metal oxide, wherein a product of A and B equals 150 to 350, A equals 15 to 20%, and B equals 10 to 25%, where A (%) represents a porosity of the positive electrode material mixture layer, and B (%) represents a volume percentage of ethylene carbonate in the non-aqueous solvent.
摘要:
A non-aqueous electrolyte secondary battery including: an electrode group in which a positive electrode and a negative electrode are spirally wound with a separator interposed therebetween; and a non-aqueous electrolyte including a non-aqueous solvent and a lithium salt dissolved in the non-aqueous solvent, the positive electrode including a positive electrode material mixture layer containing a nickel-containing lithium composite metal oxide, wherein a product of A and B equals 150 to 350, A equals 15 to 20%, and B equals 10 to 25%, where A (%) represents a porosity of the positive electrode material mixture layer, and B (%) represents a volume percentage of ethylene carbonate in the non-aqueous solvent.
摘要:
A lithium-containing composite oxide represented by the formula 1: LixNi1-y-z-v-wCoyAlzM1vM2wO2 is used as a positive electrode active material for a non-aqueous electrolyte secondary battery. The element M1 is at least one selected from the group consisting of Mn, Ti, Y, Nb, Mo, and W. The element M2 includes at least two selected from the group consisting of Mg, Ca, Sr, and Ba, and the element M2 includes at least Mg and Ca. The formula 1 satisfies 0.97≦x≦1.1, 0.05≦y≦0.35, 0.005≦z≦0.1, 0.0001≦v≦0.05, and 0.0001≦w≦0.05. The primary particles have a mean particle size of 0.1 μm or more and 3 μm or less, and the secondary particles have a mean particle size of 8 μm or more and 20 μm or less.
摘要:
Disclosed is a non-aqueous electrolyte secondary battery having an electrode group in which a positive electrode and a negative electrode are spirally wound with a separator interposed therebetween. The positive electrode contains a positive electrode active material and a binder. The positive electrode active material contains a mixture of two different particulate substances having different average particle sizes. The two different particulate substances are lithium composite metal oxides containing nickel as an essential element. The binder includes fluorocarbon resin and rubber particles. The fluorocarbon resin contains at least a vinylidene fluoride unit. The amount of the rubber particles per 100 parts by weight of the fluorocarbon resin is 1 to 25 parts by weight.
摘要:
Disclosed is a non-aqueous electrolyte secondary battery having an electrode group in which a positive electrode and a negative electrode are spirally wound with a separator interposed therebetween. The positive electrode contains a positive electrode active material and a binder. The positive electrode active material contains a mixture of two different particulate substances having different average particle sizes. The two different particulate substances are lithium composite metal oxides containing nickel as an essential element. The binder includes fluorocarbon resin and rubber particles. The fluorocarbon resin contains at least a vinylidene fluoride unit. The amount of the rubber particles per 100 parts by weight of the fluorocarbon resin is 1 to 25 parts by weight.
摘要:
Provided is a deterioration determination circuit configured by including: an SOC detection unit for detecting an SOC of a secondary battery; an internal resistance detection unit for detecting an internal resistance value of the secondary battery; a first determination unit for determining the status of deterioration of the secondary battery based on the internal resistance value detected by the internal resistance detection unit when the SOC detected by the SOC detection unit is within a range of a pre-set first range; a second determination unit for determining the status of deterioration of the secondary battery based on the internal resistance value detected by the internal resistance detection unit when the SOC detected by the SOC detection unit is within a range of a pre-set second range as a range of an SOC, in which a variation of the internal resistance of the second battery in relation to a variation of the SOC of the secondary battery is different from the first range; and a final determination unit for ultimately determining that the secondary battery is deteriorated when the first determination unit determines that the secondary battery is of the deteriorated status and the second determination unit additionally determines that the secondary battery is of the deteriorated status.
摘要:
An SOF measuring system that can continuously measure SOF and a soot measuring system that can continuously measure soot are connected with an exhaust gas line. The soot measuring system comprises a diluter that selectively dilutes either one of the exhaust gas and standard gas whose hydrocarbon concentration is known with diluent gas and extrudes it. A dilution ratio adjusting device can adjust a dilution ratio of the diluter. A soot detector continuously detects soot in the exhaust gas or the standard gas diluted by the diluter. The SOF measuring system can be connected with the diluter so that an exhaust gas analyzer can measure the hydrocarbon concentration in the standard gas diluted by the diluter.