Phase retarder film containing TiO.sub.2
    1.
    发明授权
    Phase retarder film containing TiO.sub.2 失效
    含有TiO2的相延迟膜

    公开(公告)号:US6097460A

    公开(公告)日:2000-08-01

    申请号:US233962

    申请日:1999-01-20

    IPC分类号: B32B7/02 G02B5/30 G02F1/1335

    CPC分类号: G02B5/3083

    摘要: A phase retarder film is provided wherein at least one oblique evaporation layer comprising an inorganic dielectric mainly containing TiO.sub.2 is formed on at least one surface of a transparent polymer film with an intermediate layer between, the evaporation layer having positive refractive index anisotropy and a principal optic axis tilted 20 degrees to 70 degrees from a normal direction to said transparent polymer film. The phase retarder film is suitable for improving viewing angle characteristics of the TN-LCD.

    摘要翻译: 提供了一种相位延迟膜,其中至少一个包含主要含有TiO 2的无机电介质的倾斜蒸发层形成在透明聚合物膜的至少一个表面上,中间层之间具有正折射率各向异性的蒸发层和主光学器件 轴向从所述透明聚合物膜的法线方向倾斜20度至70度。 相位延迟膜适用于改善TN-LCD的视角特性。

    Normally white mode twisted nematic liquid crystal display device having improved viewing angle characteristics
    2.
    发明授权
    Normally white mode twisted nematic liquid crystal display device having improved viewing angle characteristics 失效
    通常具有改进的视角特性的白色模式扭曲向列型液晶显示装置

    公开(公告)号:US06208396B1

    公开(公告)日:2001-03-27

    申请号:US08957780

    申请日:1997-10-24

    IPC分类号: G02F11347

    摘要: A normally white mode twisted nematic liquid crystal display devices having significantly improved viewing angle characteristics of display contrast and gray scale inversion comprising an about 90° twisted nematic liquid crystal cell and a first and a second light polarizing film separately disposed on two sides of said liquid crystal cell, a first and a second optical compensation layer which each comprises at least one optical compensation layer and has almost no refractive index anisotropy in-plane of the optical compensation layer A and has a characteristic wherein a refractive index in the thickness direction of the optical compensation layer A is lower than that in-plane of the optical compensation layer A, and a first and second optical compensation layer B, which each comprises at least one optical compensation layer and has optically positive refractive index anisotropy and has a characteristic wherein a principal optic axis of the optical compensation layer B is tilted 20 to 70° from the normal direction of the optical compensation layer B, wherein said liquid crystal cell, said light polarizing films and said optical compensation layers A and B are laminated in the following order: said first light polarizing film, said first optical compensation layer A, said first optical compensation layer B, said liquid crystal cell, said second optical compensation layer B, said second optical compensation layer A and said second light polarizing film.

    摘要翻译: 具有显着改善的显示对比度和灰度反转的视角特性的常白模式扭曲向列型液晶显示装置,包括大约90°扭曲向列型液晶单元和分别设置在所述液体两侧的第一和第二偏光膜 晶体单元,第一和第二光学补偿层,每个光学补偿层包括至少一个光学补偿层,并且几乎不具有光学补偿层A的平面内的折射率各向异性,并且具有其特征在于,其中,厚度方向的折射率 光学补偿层A比光学补偿层A的面内低,第一和第二光学补偿层B各自包括至少一个光学补偿层,并具有光学正折射率各向异性,并且具有以下特征: 光学补偿层B的主光轴倾斜20° 光学补偿层B的法线方向为70°,其中所述液晶单元,所述光偏振膜和所述光学补偿层A和B按照以下顺序层叠:所述第一光偏移膜,所述第一光学补偿层A 所述第一光学补偿层B,所述液晶单元,所述第二光学补偿层B,所述第二光学补偿层A和所述第二光偏振膜。

    Phase retarder film
    3.
    发明授权
    Phase retarder film 失效
    相延迟膜

    公开(公告)号:US5926313A

    公开(公告)日:1999-07-20

    申请号:US956453

    申请日:1997-10-23

    IPC分类号: G02B5/30 G02F1/13363

    CPC分类号: G02F1/133632 G02B5/3083

    摘要: As a phase retarder film in which at least one oblique evaporation layer of an inorganic dielectric having positive refractive index anisotropy and having its principal optic axis tilted 20 degrees to 70 degrees from the direction of the normal to the film is formed on at least one surface of a transparent polymer film with an intermediate layer between, a large area film is easily and inexpensivly obtained.

    摘要翻译: 作为相位延迟膜,其中至少一个具有正折射率各向异性且其主光轴从膜的法线方向倾斜20度至70度的无机电介质的倾斜蒸发层形成在至少一个表面上 具有中间层之间的透明聚合物膜,容易且廉价地获得大面积的膜。

    Layered inorganic compound-containing phase retarder
    6.
    发明授权
    Layered inorganic compound-containing phase retarder 失效
    含层状无机化合物的相缓凝剂

    公开(公告)号:US5631755A

    公开(公告)日:1997-05-20

    申请号:US415254

    申请日:1995-04-03

    摘要: A phase retarder including a layered inorganic compound-containing sheet or layered inorganic compound-containing film, the inorganic compound being selected from the group consisting of a clay mineral, a chalcogen compound, a zirconium phosphate compound, an oxyacid salt of a transition metal, a layered polysilicate, a metal oxyhalogenide, and an intercalary decoration thereof intercalated with ions or molecules between crystalline layer units, the inorganic compound having a mean particle size of 5000 nm or less and a stratified structure with a plurality of crystalline layer units wherein the phase retarder has a refractive index in the plane of the phase retarder that is different from a refractive index in the thickness direction of the phase retarder.

    摘要翻译: 一种含有含层状无机化合物的片材或层状无机化合物的膜的相变缓凝剂,所述无机化合物选自粘土矿物,硫属化合物,磷酸锆化合物,过渡金属的含氧酸盐, 层状聚硅酸盐,金属卤氧化物,以及在结晶层单元之间插入离子或分子的嵌入式装饰物,所述无机化合物具有5000nm以下的平均粒径和具有多个结晶层单元的分层结构,其中所述相 延迟器在相位延迟器的平面中具有与相位延迟器的厚度方向上的折射率不同的折射率。

    Process for making a phase retarder film
    8.
    发明授权
    Process for making a phase retarder film 失效
    制备相延迟膜的方法

    公开(公告)号:US5658505A

    公开(公告)日:1997-08-19

    申请号:US394494

    申请日:1995-02-27

    IPC分类号: G02B5/30 B29D11/00

    摘要: A phase retarder film made of a thermoplastic resin having an in-plane retardation of 50 to 300 nm and a ratio of the in-plane retardation to the retardation normal to the plane of not less than 0.5 but not more than 1.8, a process for the production thereof and a laminate phase retarder film using said phase retarder film above.

    摘要翻译: 由面内延迟为50〜300nm的热塑性树脂制成的相位延迟膜和面内延迟与平面相位差的比例为0.5以上1.8以下的工序 使用上述相延迟膜的层压相延迟膜。

    Phase retarder and liquid crystal display device using the same
    9.
    发明授权
    Phase retarder and liquid crystal display device using the same 失效
    相位延迟器和使用其的液晶显示装置

    公开(公告)号:US6060183A

    公开(公告)日:2000-05-09

    申请号:US887892

    申请日:1997-07-03

    IPC分类号: G02B5/30 G02F1/13363 B32B9/00

    CPC分类号: G02B5/3083 G02F1/13363

    摘要: A phase retarder film comprising a layer of polyvinyl alcohol or a derivative thereof and a water-swellable layered inorganic compound, wherein the in-plane retardation value is smaller than the retardation value in the thickness direction, sometimes causes durability failures, that is, the layer is peeled off from a transparent resin substrate in high temperature and high humidity environment. Therefore, the present invention provides a phase retarder film which is superior in durability.With respect to a phase retarder film comprising at least one layer containing at least one organic clay compound which can be dispersed in an organic solvent, wherein the in-plane retardation value is smaller than the retardation value in the thickness direction, the durability is remarkably improved.

    摘要翻译: 包含聚乙烯醇或其衍生物层和水溶胀性层状无机化合物的相延迟膜,其中面内延迟值小于厚度方向上的延迟值,有时会导致耐久性故障,即, 在高温高湿环境下,从透明树脂基板剥离层。 因此,本发明提供耐久性优异的相位延迟膜。 关于包含至少一层含有可分散在有机溶剂中的有机粘土化合物的相延迟膜,其中面内延迟值小于厚度方向上的延迟值,耐久性显着地 改进。

    Phase retarder film
    10.
    发明授权
    Phase retarder film 失效
    相延迟膜

    公开(公告)号:US5888634A

    公开(公告)日:1999-03-30

    申请号:US845471

    申请日:1997-04-25

    IPC分类号: G02B5/30

    摘要: Disclosed is a phase retarder film made of a thermoplastic resin having an in-plane retardation of 50 to 300 nm and a ratio of the in-plane retardation to the retardation normal to the plane of not less than 0.5, but not more than 1.8, a process for the production thereof and a laminate phase retarder film using said phase retarder film above.