Methods for artificially aging aluminum-zinc-magnesium alloys, and products based on the same
    1.
    发明授权
    Methods for artificially aging aluminum-zinc-magnesium alloys, and products based on the same 有权
    人造老化铝锌镁合金的方法及其制品

    公开(公告)号:US09249487B2

    公开(公告)日:2016-02-02

    申请号:US13827918

    申请日:2013-03-14

    Applicant: Alcoa Inc.

    CPC classification number: C22F1/053 C22C21/10

    Abstract: New methods for aging aluminum alloys having zinc and magnesium are disclosed. The methods may include first aging the aluminum alloy at a first temperature of from about 330° F. to 530° F. and for a first aging time of from 1 minute to 6 hours, and then second aging the aluminum alloy at a second temperature for a second aging time of at least 30 minutes, with the second temperature being lower than the first temperature.

    Abstract translation: 公开了具有锌和镁的老化铝合金的新方法。 所述方法可以包括在约330°F至530°F的第一温度和1分钟至6小时的第一老化时间之前首先老化铝合金,然后在第二温度下对铝合金进行二次老化 第二老化时间至少为30分钟,第二温度低于第一温度。

    WROUGHT 7XXX ALUMINUM ALLOYS, AND METHODS FOR MAKING THE SAME

    公开(公告)号:US20170121795A1

    公开(公告)日:2017-05-04

    申请号:US15336443

    申请日:2016-10-27

    Applicant: ALCOA INC.

    CPC classification number: C22C21/10 C22F1/053

    Abstract: New wrought 7xxx aluminum alloys are disclosed. The new wrought 7xxx aluminum alloys generally include from 3.75 to 8.0 wt. % Zn, from 1.25 to 3.0 wt. % Mg, where the wt. % Zn exceeds the wt. % Mg, from 0.35 to 1.35 wt. % Cu, from 0.04 to 0.20 wt. % V, from 0.06 to 0.20 wt. % Zr, where V+Zr≦0.23 wt. %, from 0.01 to 0.25 wt. % Ti, up to 0.50 wt. % Mn, up to 0.40 wt. % Cr, up to 0.35 wt. % Fe, and up to 0.25 wt. % Si, the balance being aluminum and impurities, wherein the wrought 7xxx aluminum alloy include not greater than 0.10 wt. % each of any one impurity, and wherein the wrought 7xxx aluminum alloy includes not greater than 0.35 wt. % in total of the impurities.

    METHODS FOR ARTIFICIALLY AGING ALUMINUM-ZINC-MAGNESIUM ALLOYS, AND PRODUCTS BASED ON THE SAME
    3.
    发明申请
    METHODS FOR ARTIFICIALLY AGING ALUMINUM-ZINC-MAGNESIUM ALLOYS, AND PRODUCTS BASED ON THE SAME 有权
    用于人造铝镁合金的方法和基于其的产品

    公开(公告)号:US20150376754A1

    公开(公告)日:2015-12-31

    申请号:US13827918

    申请日:2013-03-14

    Applicant: ALCOA INC.

    CPC classification number: C22F1/053 C22C21/10

    Abstract: New methods for aging aluminum alloys having zinc and magnesium are disclosed. The methods may include first aging the aluminum alloy at a first temperature of from about 330° F. to 530° F. and for a first aging time of from 1 minute to 6 hours, and then second aging the aluminum alloy at a second temperature for a second aging time of at least 30 minutes, with the second temperature being lower than the first temperature.

    Abstract translation: 公开了具有锌和镁的老化铝合金的新方法。 所述方法可以包括在约330°F至530°F的第一温度和1分钟至6小时的第一老化时间之前首先老化铝合金,然后在第二温度下对铝合金进行二次老化 第二老化时间至少为30分钟,第二温度低于第一温度。

    7XX ALUMINUM CASTING ALLOYS, AND METHODS FOR MAKING THE SAME
    4.
    发明申请
    7XX ALUMINUM CASTING ALLOYS, AND METHODS FOR MAKING THE SAME 审中-公开
    7XX铝铸造合金及其制造方法

    公开(公告)号:US20150315680A1

    公开(公告)日:2015-11-05

    申请号:US14694109

    申请日:2015-04-23

    Applicant: ALCOA INC.

    CPC classification number: B22D21/04 C22C21/10 C22F1/053

    Abstract: New 7xx aluminum casting alloys are disclosed. The aluminum casting alloys generally include from 3.0 to 8.0 wt. % Zn, from 1.0 to 3.0 wt. % Mg, where the wt. % Zn exceeds the wt. % Mg, from 0.35 to 1.0 wt. % Cu, where the wt. % Mg exceeds the wt. % Cu, from 0.05 to 0.30 wt. % V, from 0.01 to 1.0 wt. % of at least one secondary element (Mn, Cr, Zr, Ti, B, and combinations thereof), up to 0.50 wt. % Fe, and up to 0.25 wt. % Si, the balance being aluminum and other elements, wherein the aluminum casting alloy include not greater than 0.05 wt. % each of the other elements, and wherein the aluminum casting alloy includes not greater than 0.15 wt. % in total of the other elements.

    Abstract translation: 公开了新的7xx铝铸造合金。 铝铸造合金通常包括3.0至8.0重量% %Zn,1.0〜3.0wt。 %Mg,其中wt。 %Zn超过wt。 %Mg,0.35〜1.0wt。 %Cu,其中wt。 %Mg超过wt。 %Cu,0.05-0.30重量% %V,0.01〜1.0wt。 至少一种次要元素(Mn,Cr,Zr,Ti,B及其组合)的%,至多0.50重量% %Fe,至多0.25wt。 %Si,余量为铝和其他元素,其中铝铸造合金包括不大于0.05重量% %的其他元素,其中铝铸造合金包括不大于0.15wt。 其他元素总数的百分比。

    METHODS FOR ARTIFICIALLY AGING ALUMINUM-ZINC-MAGNESIUM ALLOYS, AND PRODUCTS BASED ON THE SAME
    5.
    发明申请
    METHODS FOR ARTIFICIALLY AGING ALUMINUM-ZINC-MAGNESIUM ALLOYS, AND PRODUCTS BASED ON THE SAME 有权
    用于人造铝镁合金的方法和基于其的产品

    公开(公告)号:US20150259774A1

    公开(公告)日:2015-09-17

    申请号:US14206448

    申请日:2014-03-12

    Applicant: ALCOA INC.

    CPC classification number: C22F1/053 C22C21/10 C22F1/002

    Abstract: New methods for aging aluminum alloys having zinc and magnesium are disclosed. The methods may include first aging the aluminum alloy at a first temperature of from about 310° F. to 530° F. and for a first aging time of from 1 minute to 6 hours, and then second aging the aluminum alloy at a second temperature for a second aging time of at least 30 minutes, with the second temperature being lower than the first temperature.

    Abstract translation: 公开了具有锌和镁的老化铝合金的新方法。 所述方法可以包括在约310°F至530°F的第一温度和1分钟至6小时的第一老化时间之前对铝合金进行老化,然后在第二温度下对铝合金进行二次老化 第二老化时间至少为30分钟,第二温度低于第一温度。