WROUGHT 7XXX ALUMINUM ALLOYS, AND METHODS FOR MAKING THE SAME

    公开(公告)号:US20170121795A1

    公开(公告)日:2017-05-04

    申请号:US15336443

    申请日:2016-10-27

    Applicant: ALCOA INC.

    CPC classification number: C22C21/10 C22F1/053

    Abstract: New wrought 7xxx aluminum alloys are disclosed. The new wrought 7xxx aluminum alloys generally include from 3.75 to 8.0 wt. % Zn, from 1.25 to 3.0 wt. % Mg, where the wt. % Zn exceeds the wt. % Mg, from 0.35 to 1.35 wt. % Cu, from 0.04 to 0.20 wt. % V, from 0.06 to 0.20 wt. % Zr, where V+Zr≦0.23 wt. %, from 0.01 to 0.25 wt. % Ti, up to 0.50 wt. % Mn, up to 0.40 wt. % Cr, up to 0.35 wt. % Fe, and up to 0.25 wt. % Si, the balance being aluminum and impurities, wherein the wrought 7xxx aluminum alloy include not greater than 0.10 wt. % each of any one impurity, and wherein the wrought 7xxx aluminum alloy includes not greater than 0.35 wt. % in total of the impurities.

    METHODS FOR ARTIFICIALLY AGING ALUMINUM-ZINC-MAGNESIUM ALLOYS, AND PRODUCTS BASED ON THE SAME
    3.
    发明申请
    METHODS FOR ARTIFICIALLY AGING ALUMINUM-ZINC-MAGNESIUM ALLOYS, AND PRODUCTS BASED ON THE SAME 有权
    用于人造铝镁合金的方法和基于其的产品

    公开(公告)号:US20150376754A1

    公开(公告)日:2015-12-31

    申请号:US13827918

    申请日:2013-03-14

    Applicant: ALCOA INC.

    CPC classification number: C22F1/053 C22C21/10

    Abstract: New methods for aging aluminum alloys having zinc and magnesium are disclosed. The methods may include first aging the aluminum alloy at a first temperature of from about 330° F. to 530° F. and for a first aging time of from 1 minute to 6 hours, and then second aging the aluminum alloy at a second temperature for a second aging time of at least 30 minutes, with the second temperature being lower than the first temperature.

    Abstract translation: 公开了具有锌和镁的老化铝合金的新方法。 所述方法可以包括在约330°F至530°F的第一温度和1分钟至6小时的第一老化时间之前首先老化铝合金,然后在第二温度下对铝合金进行二次老化 第二老化时间至少为30分钟,第二温度低于第一温度。

    7XX ALUMINUM CASTING ALLOYS, AND METHODS FOR MAKING THE SAME
    4.
    发明申请
    7XX ALUMINUM CASTING ALLOYS, AND METHODS FOR MAKING THE SAME 审中-公开
    7XX铝铸造合金及其制造方法

    公开(公告)号:US20150315680A1

    公开(公告)日:2015-11-05

    申请号:US14694109

    申请日:2015-04-23

    Applicant: ALCOA INC.

    CPC classification number: B22D21/04 C22C21/10 C22F1/053

    Abstract: New 7xx aluminum casting alloys are disclosed. The aluminum casting alloys generally include from 3.0 to 8.0 wt. % Zn, from 1.0 to 3.0 wt. % Mg, where the wt. % Zn exceeds the wt. % Mg, from 0.35 to 1.0 wt. % Cu, where the wt. % Mg exceeds the wt. % Cu, from 0.05 to 0.30 wt. % V, from 0.01 to 1.0 wt. % of at least one secondary element (Mn, Cr, Zr, Ti, B, and combinations thereof), up to 0.50 wt. % Fe, and up to 0.25 wt. % Si, the balance being aluminum and other elements, wherein the aluminum casting alloy include not greater than 0.05 wt. % each of the other elements, and wherein the aluminum casting alloy includes not greater than 0.15 wt. % in total of the other elements.

    Abstract translation: 公开了新的7xx铝铸造合金。 铝铸造合金通常包括3.0至8.0重量% %Zn,1.0〜3.0wt。 %Mg,其中wt。 %Zn超过wt。 %Mg,0.35〜1.0wt。 %Cu,其中wt。 %Mg超过wt。 %Cu,0.05-0.30重量% %V,0.01〜1.0wt。 至少一种次要元素(Mn,Cr,Zr,Ti,B及其组合)的%,至多0.50重量% %Fe,至多0.25wt。 %Si,余量为铝和其他元素,其中铝铸造合金包括不大于0.05重量% %的其他元素,其中铝铸造合金包括不大于0.15wt。 其他元素总数的百分比。

    Methods for artificially aging aluminum-zinc-magnesium alloys, and products based on the same
    5.
    发明授权
    Methods for artificially aging aluminum-zinc-magnesium alloys, and products based on the same 有权
    人造老化铝锌镁合金的方法及其制品

    公开(公告)号:US09249487B2

    公开(公告)日:2016-02-02

    申请号:US13827918

    申请日:2013-03-14

    Applicant: Alcoa Inc.

    CPC classification number: C22F1/053 C22C21/10

    Abstract: New methods for aging aluminum alloys having zinc and magnesium are disclosed. The methods may include first aging the aluminum alloy at a first temperature of from about 330° F. to 530° F. and for a first aging time of from 1 minute to 6 hours, and then second aging the aluminum alloy at a second temperature for a second aging time of at least 30 minutes, with the second temperature being lower than the first temperature.

    Abstract translation: 公开了具有锌和镁的老化铝合金的新方法。 所述方法可以包括在约330°F至530°F的第一温度和1分钟至6小时的第一老化时间之前首先老化铝合金,然后在第二温度下对铝合金进行二次老化 第二老化时间至少为30分钟,第二温度低于第一温度。

    NEW 6XXX ALUMINUM ALLOYS AND METHODS OF MAKING THE SAME
    6.
    发明申请
    NEW 6XXX ALUMINUM ALLOYS AND METHODS OF MAKING THE SAME 审中-公开
    新的6XXX铝合金及其制备方法

    公开(公告)号:US20160348225A1

    公开(公告)日:2016-12-01

    申请号:US15165595

    申请日:2016-05-26

    Applicant: Alcoa, Inc.

    Abstract: New 6xxx aluminum alloy sheet products and methods of making the same are disclosed. The new methods may include preparing a 6xxx aluminum alloy sheet product for solution heat treatment, solution heat treating and then quenching the 6xxx aluminum alloy sheet product, and then exposing the 6xxx aluminum alloy sheet product to a treatment temperature of from 30° C. to 60° C. for 0.2 to 300 seconds. After the exposing step, the 6xxx aluminum alloy sheet product may be coiled and then placed in an ambient environment. Due to the post-quench heating and subsequent exposure to ambient, a preselected amount of Newtonian cooling may be induced, thereby creating a unique and consistent microstructure within the 6xxx aluminum alloy sheet products.

    Abstract translation: 公开了新的6xxx铝合金板产品及其制造方法。 新方法可能包括制备6xxx铝合金板材,用于固溶热处理,固溶热处理,然后淬火6xxx铝合金板材产品,然后将6xxx铝合金板材产品的处理温度从30°C暴露于 60℃下0.2至300秒。 在暴露步骤之后,6xxx铝合金板材产品可能被卷起,然后放置在周围环境中。 由于后淬火加热并随后暴露于环境中,可能会引起预选量的牛顿冷却,从而在6xxx铝合金板材产品内形成独特且一致的微观结构。

    METHODS FOR ARTIFICIALLY AGING ALUMINUM-ZINC-MAGNESIUM ALLOYS, AND PRODUCTS BASED ON THE SAME
    7.
    发明申请
    METHODS FOR ARTIFICIALLY AGING ALUMINUM-ZINC-MAGNESIUM ALLOYS, AND PRODUCTS BASED ON THE SAME 有权
    用于人造铝镁合金的方法和基于其的产品

    公开(公告)号:US20150259774A1

    公开(公告)日:2015-09-17

    申请号:US14206448

    申请日:2014-03-12

    Applicant: ALCOA INC.

    CPC classification number: C22F1/053 C22C21/10 C22F1/002

    Abstract: New methods for aging aluminum alloys having zinc and magnesium are disclosed. The methods may include first aging the aluminum alloy at a first temperature of from about 310° F. to 530° F. and for a first aging time of from 1 minute to 6 hours, and then second aging the aluminum alloy at a second temperature for a second aging time of at least 30 minutes, with the second temperature being lower than the first temperature.

    Abstract translation: 公开了具有锌和镁的老化铝合金的新方法。 所述方法可以包括在约310°F至530°F的第一温度和1分钟至6小时的第一老化时间之前对铝合金进行老化,然后在第二温度下对铝合金进行二次老化 第二老化时间至少为30分钟,第二温度低于第一温度。