公开(公告)号:US20090217705A1
公开(公告)日:2009-09-03
申请号:US12150484
申请日:2008-04-29
申请人: Andrey V. Filippov , Allan Mark Fredholm , Jacob George , Hilary Tony Godard , Clinton Damon Osterhout , Gary Graham Squier
发明人: Andrey V. Filippov , Allan Mark Fredholm , Jacob George , Hilary Tony Godard , Clinton Damon Osterhout , Gary Graham Squier
CPC分类号: C03B17/064 , C03B13/04 , C03B17/067 , C03B18/02
摘要: Disclosed are systems and methods for forming glass sheets. Methods and systems are provided that comprise a refractory body configured to receive glass-based material and means for transmitting energy to selectively heat at least a portion of the refractory body through the glass-based material. In one aspect, the energy transmitted is of a selected frequency that is not fully absorbed by the glass-based material and is at least partially absorbed by the refractory body. The energy can be transmitted by a laser beam array, a scanning laser beam, a microwave generator, a radio frequency generator, or other means.
摘要翻译: 公开了用于形成玻璃板的系统和方法。 提供了包括构造成容纳玻璃基材料的耐火材料体和用于传递能量以选择性地通过玻璃基材料加热耐火材料体的至少一部分的装置的方法和系统。 在一个方面,透射的能量具有未被玻璃基材料完全吸收并且至少部分被耐火材料体吸收的选定频率。 能量可以通过激光束阵列,扫描激光束,微波发生器,射频发生器或其他装置传输。
-
公开(公告)号:US20130015180A1
公开(公告)日:2013-01-17
申请号:US13183705
申请日:2011-07-15
申请人: Hilary Tony Godard , Gaozhu Peng , Irene Mona Peterson , Rebecca Lynn Schulz , Gary Graham Squier
发明人: Hilary Tony Godard , Gaozhu Peng , Irene Mona Peterson , Rebecca Lynn Schulz , Gary Graham Squier
IPC分类号: H05B6/64
CPC分类号: C03B17/067 , C03B13/10 , C03B17/02 , C03B17/064 , C03B18/12 , C03B23/023 , C03B23/0235 , C03B27/012 , C03C23/0065
摘要: Methods of fabricating a glass laminate is provided. According to one embodiment, a glass laminate comprised of a microwave absorbing layer and a microwave transparent layer is formed. The microwave absorbing layer is characterized by a microwave loss tangent δH that is at least a half order of magnitude larger than a loss tangent δL of the microwave transparent layer. An area of the glass laminate is exposed to microwave radiation. The exposed area comprises a cross-laminate hot zone having a cross-laminate hot zone temperature profile. Substantially all microwave absorbing layer portions of the hot zone temperature profile and substantially all microwave transparent layer portions of the hot zone temperature profile reside above the glass transition temperature TG of the various layers of the glass laminate prior to impingement by the microwave radiation. In accordance with another embodiment, a method of fabricating a glass laminate is provided where the exposed area of the glass laminate is characterized by a viscosity below approximately 1×104 poise.
摘要翻译: 提供制造玻璃层压板的方法。 根据一个实施例,形成由微波吸收层和微波透明层组成的玻璃层压体。 微波吸收层的特征在于微波损耗角正切δH比微波透明层的损耗角正切δL至少大一个数量级。 玻璃层压板的一个区域暴露于微波辐射。 曝光区域包括具有交叉层压热区温度曲线的交叉层压热区。 热区温度分布的基本上所有的微波吸收层部分和热区温度曲线的基本上所有的微波透明层部分都位于玻璃层压板的各个层的玻璃化转变温度TG之上,微波辐射在撞击之前。 根据另一个实施例,提供一种制造玻璃层压体的方法,其中玻璃层压板的暴露面积的特征在于低于约1×104泊的粘度。
-
公开(公告)号:US09090505B2
公开(公告)日:2015-07-28
申请号:US13183705
申请日:2011-07-15
申请人: Hilary Tony Godard , Gaozhu Peng , Irene Mona Peterson , Rebecca Lynn Schulz , Gary Graham Squier
发明人: Hilary Tony Godard , Gaozhu Peng , Irene Mona Peterson , Rebecca Lynn Schulz , Gary Graham Squier
IPC分类号: B32B17/00 , C03B17/00 , C03C23/00 , C03B13/10 , C03B17/02 , C03B17/06 , C03B18/12 , C03B23/023
CPC分类号: C03B17/067 , C03B13/10 , C03B17/02 , C03B17/064 , C03B18/12 , C03B23/023 , C03B23/0235 , C03B27/012 , C03C23/0065
摘要: Methods of fabricating a glass laminate is provided. According to one embodiment, a glass laminate comprised of a microwave absorbing layer and a microwave transparent layer is formed. The microwave absorbing layer is characterized by a microwave loss tangent δH that is at least a half order of magnitude larger than a loss tangent δL of the microwave transparent layer. An area of the glass laminate is exposed to microwave radiation. The exposed area comprises a cross-laminate hot zone having a cross-laminate hot zone temperature profile. Substantially all microwave absorbing layer portions of the hot zone temperature profile and substantially all microwave transparent layer portions of the hot zone temperature profile reside above the glass transition temperature TG of the various layers of the glass laminate prior to impingement by the microwave radiation. In accordance with another embodiment, a method of fabricating a glass laminate is provided where the exposed area of the glass laminate is characterized by a viscosity below approximately 1×104 poize.
摘要翻译: 提供制造玻璃层压板的方法。 根据一个实施例,形成由微波吸收层和微波透明层组成的玻璃层压体。 微波吸收层的特征在于微波损耗角正切δH比微波透明层的损耗角正切δL至少大一个数量级。 玻璃层压板的一个区域暴露于微波辐射。 曝光区域包括具有交叉层压热区温度曲线的交叉层压热区。 热区温度分布的基本上所有的微波吸收层部分和热区温度曲线的基本上所有的微波透明层部分都位于玻璃层压板的各个层的玻璃化转变温度TG之上,微波辐射在撞击之前。 根据另一个实施例,提供一种制造玻璃层压体的方法,其中玻璃层压板的暴露面积的特征在于低于约1×10 4泊的粘度。
-
公开(公告)号:US20090131241A1
公开(公告)日:2009-05-21
申请号:US11922580
申请日:2005-12-21
CPC分类号: C04B35/447 , C03B17/064 , C04B35/481 , C04B35/495 , C04B35/6262 , C04B2235/3224 , C04B2235/3225 , C04B2235/3239 , C04B2235/3244 , C04B2235/3248 , C04B2235/3286 , C04B2235/3418 , C04B2235/3427 , C04B2235/447 , C04B2235/6021 , C04B2235/604 , C04B2235/656 , C04B2235/76 , C04B2235/761 , C04B2235/80 , C04B2235/96 , C04B2235/9669
摘要: Refractory materials are provided which contain P2O5/R2O3 constituents, where R is Y, Sc, Er, Lu, Yb, Tm, Ho, Dy, Tb, Gd, or a combination thereof, and/or V2O5/R′2O3 constituents where R′ is Y, Sc, one or more rare earth elements, or a combination thereof. In certain embodiments, the refractory materials are xenotime-type materials and/or xenotime-stabilized zircon-type materials. The refractory materials can be used in the manufacture of glass and glass-ceramics. For example, the refractory materials, especially those that contain P2O5/R2O3 constituents, can be used as forming structures (“isopipes”) in the fusion process for making flat sheets of glass such as the glass sheets used as substrates in the manufacture of flat panel displays.
摘要翻译: 提供含有P2O5 / R2O3组分的耐火材料,其中R是Y,Sc,Er,Lu,Yb,Tm,Ho,Dy,Tb,Gd或它们的组合,和/或V 2 O 5 / R' '是Y,Sc,一种或多种稀土元素,或它们的组合。 在某些实施方案中,耐火材料是堇青石型材料和/或堇青石稳定的锆石型材料。 耐火材料可用于制造玻璃和玻璃陶瓷。 例如,耐火材料,特别是含有P 2 O 5 / R 2 O 3成分的耐火材料,可用于制造平板玻璃的熔融工艺中的成形结构(“等压槽”),例如在制造平面时用作基板的玻璃板 面板显示。
-
5.
公开(公告)号:US20100212359A1
公开(公告)日:2010-08-26
申请号:US12390663
申请日:2009-02-23
申请人: Hilary Tony Godard , Mark E. Mack
发明人: Hilary Tony Godard , Mark E. Mack
IPC分类号: C03B17/06 , C04B35/443
CPC分类号: C03B17/064
摘要: A glass manufacturing system and method are described herein that use a forming apparatus (isopipe) made from or at least coated with a magnesium aluminate spinel material which is a chemically stable and compatible refractory material when used for forming an alkali-containing glass sheet.
摘要翻译: 本文描述了一种玻璃制造系统和方法,其使用由用于形成含碱玻璃片的化学稳定且相容的耐火材料制成或至少涂覆有铝酸镁尖晶石材料的成形装置(等压槽)。
-
公开(公告)号:US08383537B2
公开(公告)日:2013-02-26
申请号:US13275868
申请日:2011-10-18
CPC分类号: C04B35/447 , C03B17/064 , C04B35/481 , C04B35/495 , C04B35/6262 , C04B2235/3224 , C04B2235/3225 , C04B2235/3239 , C04B2235/3244 , C04B2235/3248 , C04B2235/3286 , C04B2235/3418 , C04B2235/3427 , C04B2235/447 , C04B2235/6021 , C04B2235/604 , C04B2235/656 , C04B2235/76 , C04B2235/761 , C04B2235/80 , C04B2235/96 , C04B2235/9669
摘要: Refractory materials are provided which contain P2O5/R2O3 constituents, where R is Y, Sc, Er, Lu, Yb, Tm, Ho, Dy, Tb, Gd, or a combination thereof, and/or V2O5/R′2O3 constituents where R′ is Y, Sc, one or more rare earth elements, or a combination thereof. In certain embodiments, the refractory materials are xenotime-type materials and/or xenotime-stabilized zircon-type materials. The refractory materials can be used in the manufacture of glass and glass-ceramics. For example, the refractory materials, especially those that contain P2O5/R2O3 constituents, can be used as forming structures (“isopipes”) in the fusion process for making flat sheets of glass such as the glass sheets used as substrates in the manufacture of flat panel displays.
摘要翻译: 提供含有P2O5 / R2O3组分的耐火材料,其中R是Y,Sc,Er,Lu,Yb,Tm,Ho,Dy,Tb,Gd或它们的组合,和/或V 2 O 5 / R' '是Y,Sc,一种或多种稀土元素,或它们的组合。 在某些实施方案中,耐火材料是堇青石型材料和/或堇青石稳定的锆石型材料。 耐火材料可用于制造玻璃和玻璃陶瓷。 例如,耐火材料,特别是含有P 2 O 5 / R 2 O 3成分的耐火材料,可以用于制造平板玻璃的熔融过程中的成形结构(等压槽),例如在制造平板显示器时用作基板的玻璃板 。
-
公开(公告)号:US20120125048A1
公开(公告)日:2012-05-24
申请号:US13275868
申请日:2011-10-18
CPC分类号: C04B35/447 , C03B17/064 , C04B35/481 , C04B35/495 , C04B35/6262 , C04B2235/3224 , C04B2235/3225 , C04B2235/3239 , C04B2235/3244 , C04B2235/3248 , C04B2235/3286 , C04B2235/3418 , C04B2235/3427 , C04B2235/447 , C04B2235/6021 , C04B2235/604 , C04B2235/656 , C04B2235/76 , C04B2235/761 , C04B2235/80 , C04B2235/96 , C04B2235/9669
摘要: Refractory materials are provided which contain P2O5/R2O3 constituents, where R is Y, Sc, Er, Lu, Yb, Tm, Ho, Dy, Tb, Gd, or a combination thereof, and/or V2O5/R′2O3 constituents where R′ is Y, Sc, one or more rare earth elements, or a combination thereof. In certain embodiments, the refractory materials are xenotime-type materials and/or xenotime-stabilized zircon-type materials. The refractory materials can be used in the manufacture of glass and glass-ceramics. For example, the refractory materials, especially those that contain P2O5/R2O3 constituents, can be used as forming structures (“isopipes”) in the fusion process for making flat sheets of glass such as the glass sheets used as substrates in the manufacture of flat panel displays.
摘要翻译: 提供含有P2O5 / R2O3组分的耐火材料,其中R是Y,Sc,Er,Lu,Yb,Tm,Ho,Dy,Tb,Gd或它们的组合,和/或V 2 O 5 / R' '是Y,Sc,一种或多种稀土元素,或它们的组合。 在某些实施方案中,耐火材料是堇青石型材料和/或堇青石稳定的锆石型材料。 耐火材料可用于制造玻璃和玻璃陶瓷。 例如,耐火材料,特别是含有P 2 O 5 / R 2 O 3成分的耐火材料,可以用于制造平板玻璃的熔融方法中的成形结构(“等压槽”),例如在制造平面时用作基板的玻璃板 面板显示。
-
公开(公告)号:US08067326B2
公开(公告)日:2011-11-29
申请号:US11922580
申请日:2005-12-21
IPC分类号: C04B35/50 , C04B35/505 , C04B35/48
CPC分类号: C04B35/447 , C03B17/064 , C04B35/481 , C04B35/495 , C04B35/6262 , C04B2235/3224 , C04B2235/3225 , C04B2235/3239 , C04B2235/3244 , C04B2235/3248 , C04B2235/3286 , C04B2235/3418 , C04B2235/3427 , C04B2235/447 , C04B2235/6021 , C04B2235/604 , C04B2235/656 , C04B2235/76 , C04B2235/761 , C04B2235/80 , C04B2235/96 , C04B2235/9669
摘要: Refractory materials are provided which contain P2O5/R2O3 constituents, where R is Y, Sc, Er, Lu, Yb, Tm, Ho, Dy, Tb, Gd, or a combination thereof, and/or V2O5/R′2O3 constituents where R′ is Y, Sc, one or more rare earth elements, or a combination thereof. In certain embodiments, the refractory materials are xenotime-type materials and/or xenotime-stabilized zircon-type materials. The refractory materials can be used in the manufacture of glass and glass-ceramics. For example, the refractory materials, especially those that contain P2O5/R2O3 constituents, can be used as forming structures (“isopipes”) in the fusion process for making flat sheets of glass such as the glass sheets used as substrates in the manufacture of flat panel displays.
摘要翻译: 提供含有P2O5 / R2O3组分的耐火材料,其中R是Y,Sc,Er,Lu,Yb,Tm,Ho,Dy,Tb,Gd或它们的组合,和/或V 2 O 5 / R' '是Y,Sc,一种或多种稀土元素,或它们的组合。 在某些实施方案中,耐火材料是堇青石型材料和/或堇青石稳定的锆石型材料。 耐火材料可用于制造玻璃和玻璃陶瓷。 例如,耐火材料,特别是含有P 2 O 5 / R 2 O 3成分的耐火材料,可用于制造平板玻璃的熔融工艺中的成形结构(“等压槽”),例如在制造平面时用作基板的玻璃板 面板显示。
-
-
-
-
-
-
-