Abstract:
A patch for a device in an electronic housing including an aluminum layer having a threshold thickness, a non-conductive layer on a first side of the aluminum layer, and a radio-frequency (RF) transparent layer on a second side of the aluminum layer is provided. A method for manufacturing an antenna window including a patch as above is also provided, the method including determining a thickness of the aluminum layer adjacent to an anodized aluminum layer. A method for manufacturing an antenna window including coating an aluminum layer having a threshold thickness on a radio-frequency (RF) transparent layer to form an RF transparent laminate is also provided. A method for manufacturing an antenna window including removing a thickness of aluminum is also provided. A method for manufacturing an antenna window including disposing a mask on an aluminum substrate and anodizing the aluminum substrate to a selected thickness is also provided.
Abstract:
A component for an electronic device can include a metal alloy formed by a metal injection molding process. The metal alloy can have a composition of about 32 wt % to about 38 wt % cobalt and about 62 wt % to about 68 wt % iron.
Abstract:
The disclosure provides an aluminum alloy including having varying ranges of alloying elements. In various aspects, the alloy has a wt % ratio of Zn to Mg ranging from 4:1 to 7:1. The disclosure further includes methods for producing an aluminum alloy and articles comprising the aluminum alloy.
Abstract:
The disclosure provides an aluminum alloy including having varying ranges of alloying elements. In various aspects, the alloy has a wt % ratio of Zn to Mg ranging from 4:1 to 7:1. The disclosure further includes methods for producing an aluminum alloy and articles comprising the aluminum alloy.
Abstract:
The methods including applying a corrosion resistant alloy to a metal substrate to create a bimetal blank. The bimetal blank can undergo a variety of shaping and machining operations to form the net shape and internal structures of the part. Further, the part can undergo a finishing operation (e.g. polishing) to create the desired cosmetic appearance on the exterior surfaces and remove any surface imperfections resulting from the shaping and machining operations.
Abstract:
A patch for a device in an electronic housing including an aluminum layer having a threshold thickness, a non-conductive layer on a first side of the aluminum layer, and a radio-frequency (RF) transparent layer on a second side of the aluminum layer is provided. A method for manufacturing an antenna window including a patch as above is also provided, the method including determining a thickness of the aluminum layer adjacent to an anodized aluminum layer. A method for manufacturing an antenna window including coating an aluminum layer having a threshold thickness on a radio-frequency (RF) transparent layer to form an RF transparent laminate is also provided. A method for manufacturing an antenna window including removing a thickness of aluminum is also provided. A method for manufacturing an antenna window including disposing a mask on an aluminum substrate and anodizing the aluminum substrate to a selected thickness is also provided.
Abstract:
The disclosure provides an aluminum alloy including having varying ranges of alloying elements. In various aspects, the alloy has a wt % ratio of Zn to Mg ranging from 4:1 to 7:1. The disclosure further includes methods for producing an aluminum alloy and articles comprising the aluminum alloy.
Abstract:
The disclosure provides an aluminum alloy including having varying ranges of alloying elements. In various aspects, the alloy has a wt % ratio of Zn to Mg ranging from 4:1 to 7:1. The disclosure further includes methods for producing an aluminum alloy and articles comprising the aluminum alloy.
Abstract:
The methods including applying a corrosion resistant alloy to a metal substrate to create a bimetal blank. The bimetal blank can undergo a variety of shaping and machining operations to form the net shape and internal structures of the part. Further, the part can undergo a finishing operation (e.g. polishing) to create the desired cosmetic appearance on the exterior surfaces and remove any surface imperfections resulting from the shaping and machining operations.