Abstract:
A process for the manufacture of a pre-painted sheet. The process includes supplying a steel substrate, depositing a metallic coating on at least one face by hot-dipping of the substrate in a bath including 4.4% to 5.25% by weight aluminum and 0.3% to 0.56% by weight magnesium. The rest of the bath includes exclusively zinc, unavoidable impurities resulting from the process and optionally one or more additional elements including Si, Ti, Ca, Mn, La, Ce and Bi. The content by weight of each additional element in the metallic coating is less than 0.3% and the presence of nickel is excluded. The process further includes solidifying the metallic coating, surface preparation of the metallic coating and painting of the metallic coating. The present invention further provides a pre-painted sheet.
Abstract:
A method for manufacturing a high-strength sheet having improved formability and ductility accord which the chemical composition of the steel contains, in percent by weight: 0.25%
Abstract:
A process for the manufacture of a pre-painted sheet. The process includes supplying a steel substrate, depositing a metallic coating on at least one face by hot-dipping of the substrate in a bath including 4.4% to 5.25% by weight aluminum and 0.3% to 0.56% by weight magnesium. The rest of the bath includes exclusively zinc, unavoidable impurities resulting from the process and optionally one or more additional elements including Si, Ti, Ca, Mn, La, Ce and Bi. The content by weight of each additional element in the metallic coating is less than 0.3% and the presence of nickel is excluded. The process further includes solidifying the metallic coating, surface preparation of the metallic coating and painting of the metallic coating. The present invention further provides a pre-painted sheet.
Abstract:
A process for the manufacture of a pre-painted sheet. The process includes supplying a steel substrate, depositing a metallic coating on at least one face by hot-dipping of the substrate in a bath including 4.4% to 5.25% by weight aluminum and 0.3% to 0.56% by weight magnesium. The rest of the bath includes exclusively zinc, unavoidable impurities resulting from the process and optionally one or more additional elements including Si, Ti, Ca, Mn, La, Ce and Bi. The content by weight of each additional element in the metallic coating is less than 0.3% and the presence of nickel is excluded. The process further includes solidifying the metallic coating, surface preparation of the metallic coating and painting of the metallic coating. The present invention further provides a pre-painted sheet.
Abstract:
The present invention provides a process for the manufacture of a pre-painted sheet. The process includes supplying a steel substrate, depositing a metallic coating on at least one face by hot-dipping of the substrate in a bath including 4.4% to 5.6% by weight aluminum and 0.3% to 0.56% by weight magnesium. The rest of the bath includes exclusively zinc, unavoidable impurities resulting from the process and optionally one or more additional elements including Si, Ti, Ca, Mn, La, Ce and Bi. The content by weight of each additional element in the metallic coating is less than 0.3% and the presence of nickel is excluded. The process further includes solidifying the metallic coating, surface preparation of the metallic coating and painting of the metallic coating. The present invention further provides a pre-painted sheet.