METHOD FOR IMPREGNATING REINFORCING FIBRES WITH POLYARYLETHERKETONES AND SEMI-PRODUCTS OBTAINED THEREFROM

    公开(公告)号:US20210130557A1

    公开(公告)日:2021-05-06

    申请号:US16500160

    申请日:2018-04-05

    Applicant: Arkema France

    Abstract: The invention is targeted mainly at a process for the preparation of a semifinished product comprising a PAEK-based resin and reinforcing fibers, comprising the stages of: a. preparation of a dispersion comprising a PAEK-based resin in the pulverulent form dispersed in an aqueous phase comprising a surfactant; b. bringing the reinforcing fibers into contact with said aqueous dispersion; c. drying the fibers impregnated with dispersion; and d. heating the impregnated fibers to a temperature sufficient for the melting of the resin, so as to form a semifinished product, characterized in that the surfactant is a thermally stable surfactant. It is furthermore targeted at the dispersion of use in said process. Finally, it is targeted at the semifinished products capable of being obtained and also at their use in the manufacture of composite materials.

    METHOD FOR IMPREGNATING REINFORCING FIBRES WITH POLYARYLETHERKETONES AND SEMI-FINISHED PRODUCTS OBTAINED IN THIS WAY

    公开(公告)号:US20200262989A1

    公开(公告)日:2020-08-20

    申请号:US16648180

    申请日:2018-09-13

    Applicant: Arkema France

    Abstract: A process for preparing a semifinished product comprising a PAEK-based resin and reinforcing fibers, including: preparing a dispersion comprising a PAEK-based resin in pulverulent form dispersed in an aqueous phase including at least one volatile organic compound and optionally a surfactant; bringing the reinforcing fibers into contact with said aqueous dispersion; drying the fibers impregnated with dispersion; and heating the impregnated fibers to a temperature sufficient for the melting of the resin, so as to form a semifinished product, wherein the aqueous phase of the dispersion has a dynamic viscosity, measured at 25° C. under a shear stress of 6.8 s−1 on a Brookfield DV2T Extra viscometer, is between 0.1 and 25 Pa·s; and wherein when the surfactant is present, its content is less than 1% by weight relative to the mass of dispersed resin.