摘要:
An arc welding method relates to consumable electrode arc welding in which a welding wire feeding rate suitable for a welding current is determined as an average feeding rate, and the short circuit state and the arc generation state are alternately generated by changing the wire feeding periodically and repeatedly between the forward feeding and the reverse feeding. The method offers arc welding with the average feeding rate according to a welding current, a predetermined frequency, and a predetermined velocity amplitude. In the method, at least any one of the frequency and the velocity amplitude is set to a value suitable for the welding current.
摘要:
An arc welding method of the present invention controls a short-circuit current increasing gradient (di/dt), an inflection point at which the short-circuit current increasing gradient (di/dt) changes, the current in a peak period and in a base period, and the time of the peak period in accordance with a difference between a set voltage and an output voltage. This allows the output voltage to be matched with the set voltage, and stabilizes the arc. Thereby, a stable arc welding method can be implemented, even as a method for outputting a welding current based on a welding voltage.
摘要:
An arc welding method relates to consumable electrode arc welding in which a welding wire feeding rate suitable for a welding current is determined as an average feeding rate, and the short circuit state and the arc generation state are alternately generated by changing the wire feeding periodically and repeatedly between the forward feeding and the reverse feeding. The method offers arc welding with the average feeding rate according to a welding current, a predetermined frequency, and a predetermined velocity amplitude. In the method, at least any one of the frequency and the velocity amplitude is set to a value suitable for the welding current.
摘要:
Disclosed here is a pulse welding control method and a pulse arc welding device capable of improving arc stability, and decreasing the amount of spatters. The structure contains arc short-circuit judging section (13) for judging a welding state; setting section (21) for defining parameters used for a short-circuit period and an arc period; secondary control section (25); and driving section (18). Secondary control section (25) sharply decreases welding current on detecting a moment when the tip of a wire has a neck just before recovery from the short circuit, according to at least any one of outputs from a welding current value detector, a welding voltage value detector, and the setting section. Driving section (18) selects from outputs of a pulse-waveform circuit section and a dip-waveform circuit section according to the signal from the setting section and the output from the arc short-circuit section, and outputs the selected data to a switching element.
摘要:
An arc welding method comprising the steps of accelerating a feeding speed of a welding wire to cause shorting between the welding wire and a base metal when a welding end signal is input during a period of arcing, retracting the welding wire backward thereafter until a wire retracting speed reaches a predetermined rate, controlling the wire retracting speed constant at this speed for a predetermined duration of time, then stopping the backward retraction of the welding wire, and then terminating a welding power output after supplying a predetermined amount of welding current for a predetermined duration of time starting from a time when opening of the shorting occurs during the backward retraction of the welding wire.
摘要:
An arc welding method comprising the steps of accelerating a feeding speed of a welding wire to cause shorting between the welding wire and a base metal when a welding end signal is input during a period of arcing, retracting the welding wire backward thereafter until a wire retracting speed reaches a predetermined rate, controlling the wire retracting speed constant at this speed for a predetermined duration of time, then stopping the backward retraction of the welding wire, and then terminating a welding power output after supplying a predetermined amount of welding current for a predetermined duration of time starting from a time when opening of the shorting occurs during the backward retraction of the welding wire.
摘要:
An arc welding control method for carrying out welding by generating an arc between a wire and a base material. The wire is fed at wire feed speed (Wf) of periodically repeating forward feeding and reverse feeding with predetermined frequency and amplitude from time point (100) at which start of the welding is instructed, or from a certain time point (101) after the start of the welding is instructed, and then the wire feed speed is changed to a constant speed. Since the wire feed speed is controlled by periodically repeating forward feeding and reverse feeding at the arc start, short-circuit can be opened regardless of the electromagnetic pinch force, and spatters, which are generated at the early stage of the arc start because a molten pool is not preset, can be reduced.
摘要:
An arc welding method of the present invention controls a short-circuit current increasing gradient (di/dt), an inflection point at which the short-circuit current increasing gradient (di/dt) changes, the current in a peak period and in a base period, and the time of the peak period in accordance with a difference between a set voltage and an output voltage. This allows the output voltage to be matched with the set voltage, and stabilizes the arc. Thereby, a stable arc welding method can be implemented, even as a method for outputting a welding current based on a welding voltage.
摘要:
If a short circuit does not occur during deceleration of a wire feed speed in forward feed of a welding wire before the wire feed speed reaches a predetermined wire feed speed, a cyclic change is stopped and the wire feed speed is constantly controlled at the first feed speed. If a short circuit occurs during forward feed at the first feed speed, deceleration from the first feed speed starts, and the cyclic change is resumed for welding. This achieves uniform weld bead without increasing spatters even if any external disturbance such as change of distance between a tip and base material occurs.
摘要:
If a short circuit does not occur during deceleration of a wire feed speed in forward feed of a welding wire before the wire feed speed reaches a predetermined wire feed speed, a cyclic change is stopped and the wire feed speed is constantly controlled at the first feed speed. If a short circuit occurs during forward feed at the first feed speed, deceleration from the first feed speed starts, and the cyclic change is resumed for welding. This achieves uniform weld bead without increasing spatters even if any external disturbance such as change of distance between a tip and base material occurs.