公开(公告)号:US20140179812A1
公开(公告)日:2014-06-26
申请号:US14136278
申请日:2013-12-20
申请人: BASF SE
发明人: Michael L. JACKSON
CPC分类号: C08G18/6637 , C08G18/4236 , C08G18/6622 , C08G2101/0025 , C08J9/141 , C08J2203/14 , C08J2205/10 , C08J2375/04
摘要: A rigid polyurethane foam includes the reaction product of an isocyanate and an isocyanate reactive component in the presence of a blowing agent. The isocyanate reactive component includes an aromatic polyester polyol, a rigid polyol, and an aliphatic polyester polyol. The rigid polyurethane foam has a tensile adhesion of greater than 35 kPa (5 psi) when disposed on a metal substrate or a polyester, polyurethane, or epoxy coated metal substrate, each having a substrate temperature of greater than 41° C. (105° F.), and tested in accordance with ASTM D1623-09. A method of forming a composite article comprising a substrate and the rigid polyurethane foam includes the steps of combining the isocyanate reactive component and the isocyanate in the presence of the blowing agent to form a reaction mixture and applying the reaction mixture to the substrate having a substrate temperature of greater than 41° C. (105° F.) to form the composite article.
摘要翻译: 硬质聚氨酯泡沫包括异氰酸酯和异氰酸酯反应性组分在发泡剂存在下的反应产物。 异氰酸酯反应性组分包括芳族聚酯多元醇,刚性多元醇和脂族聚酯多元醇。 硬质聚氨酯泡沫塑料在设置在金属基材或聚酯,聚氨酯或环氧树脂涂覆的金属基材上时具有大于35kPa(5psi)的拉伸粘合力,每个基材温度大于41℃(105° F.),并根据ASTM D1623-09测试。 一种形成包含基材和硬质聚氨酯泡沫的复合制品的方法包括在发泡剂存在下将异氰酸酯反应性组分和异氰酸酯组合以形成反应混合物并将反应混合物施加到具有基材的基材 温度大于41℃(105°F)以形成复合制品。