Abstract:
Polyurethane elastomers are prepared by reacting a prepolymer (A) of a polyether diol and a diisocyanate with a mixture (B) of a polyester diol and a lower molecular weight glycol at a temperature of from about 60*C. to about 180*C. The reaction product of (A) and (B) is resistant to separation and the polyurethane elastomers combine all of the advantageous properties of both polyether polyurethanes and polyester polyurethanes and are useful as foils and coatings and can be molded into a variety of elastomeric products.