Abstract:
An aluminum alloy and application thereof are disclosed. Based on a total mass of the aluminum alloy, the aluminum alloy includes: 7%-11% Si, 0.4%-1.0% Fe, 0.001%-0.2% Mg, 0.001%-0.2% Cu, 0.001%-0.2% Zn, 0.005%-0.1% Mn, 0.01%-0.06% Sr, 0.003%-0.05% B, 0.01%-0.02% Ga, 0.001%-0.01% Mo, 0.001%-0.2% Ce, 0.0003%-0.02% La, and balanced by aluminum and impurity elements, where a total amount of the impurity elements is less than 0.1%.
Abstract:
An aluminum alloy is provided. Based on the total weight of the aluminum alloy, in percentage by weight, the aluminum alloy includes: 11-15% of Zn; 7.5-9% of Si; 1.2-2% of Cu; 0.3-0.5% of Mn; 0.05-0.3% of Mg; 0.1-0.2% of Ni; 0.001-0.04% of Sr; 0.05-0.3% of Ti; 0.01-0.15% of Fe; and 72.51-79.79% of Al.
Abstract:
A metal composite, a method of preparing the metal composite, a metal-resin composite, and a method of preparing the metal-resin composite are provided. The metal composite comprises: a metal substrate comprising a first layer formed on a surface of the metal substrate and an anodic oxidation layer formed on the first layer. The first layer comprises a first pore having an average diameter of about 10 nanometers to about 1 millimeter, and the metal composite comprises aluminum alloy or aluminum. The anodic oxidation layer comprises a second layer contacted with the first layer of the metal substrate and a third layer formed on an outer surface of the second layer, and the second layer comprises a second pore having an average diameter of about 10 nanometers to about 800 microns, and the third layer comprises a third pore having an average diameter of about 10 nanometers to about 800 microns.
Abstract:
A conductive sheet, a conductive strip, and an electrical connector for a vehicle are disclosed. The conductive sheet includes a conductive sheet body, the conductive sheet body is a flat ribbon structure, and the conductive sheet body satisfies the following condition:
ω ∈
{
[
1 +
(
-
0
)
/
]
0
/
k (
δ + 8
)
]
,
50 [
1 +
(
-
0
)
/
]
0
/
k (
δ + 8
)
]
}
ω is the width of the conductive sheet body, measured in mm. δ represents the thickness of the conductive sheet body, measured in mm. represents a standard conductivity percentage of a pure copper material, and has a value of 100% IACS. 0 represents a conductivity percentage of the conductive sheet body, measured in % IACS. k is 1.07% IACS/mm2.
The conductivity percentage of the conductive sheet body is 55% IACS to 80% IACS.
Abstract:
An aluminum alloy based on a total weight of the aluminum alloy, in percentages by weight, includes 9.12% of Si, 8-11% of Zn, 0.5-1.5% of Mg, 0.2-0.8% of Cu, 0-0.6% of Fe, 0.08-0.25% of Mn, 0-0.10% of Sr, 0-0.05% of Sc, 0-0.5% of Er, and 73.2-82.22% of Al.
Abstract:
A die-cast aluminum alloy and a preparation method and application thereof are disclosed. Based on the total weight of the aluminum alloy, the aluminum alloy includes: 8-11 wt % of Si, 2.5-5 wt % of Cu, 0.5-1.5 wt % of Mg, 0.1-0.3 wt % of Ni, 0.6-1.2 wt % of Fe, 0.1-0.3 wt % of Cr, 0.03-0.05 wt % of Sr, 0-0.3 wt % of Er, 80.25-88.1 wt % of Al, and 0.1 wt % or below of impurities.
Abstract:
A magnesium alloy with high thermal conductivity, an inverter housing, an inverter and a vehicle are provided. Based on the total mass of the magnesium alloy with high thermal conductivity, the magnesium alloy with high thermal conductivity includes: 2.0-4.0 wt % of Al, 0.1-0.3 wt % of Mn, 1.0-2.0 wt % of La, 2.0-4.0 wt % of Ce, 0.1-1.0 wt % of Nd, 0.5-2.0 wt % of Zn, 0.1-0.5 wt % of Ca, less than 0.1 wt % of Sr, less than 0.1 wt % of Cu, and magnesium.
Abstract:
The present disclosure discloses an aluminum alloy, based on a total mass of the aluminum alloy, including: 9-12% Si; 3.0-5.0% Zn; 1.5-2.6% Cu; 0.4-0.9% Mn; 0.2-0.6% Mg; 0.1-0.25% Fe; 0.03-0.35% Zr; 0.05-0.2% Ti; 0.005-0.04% Sr; 0.01-0.02% Ga; 0.005-0.01% Mo; 0.001-0.02% Cr; 0.005-0.3% Ni; 78.01-85.624% Al; and an impurity element.
Abstract:
An aluminum alloy and a preparation method thereof are provided. In percentage by mass, the aluminum alloy includes: 8-11% of Si, 2-3% of Cu, 0.7-1.1% of Mg, 0.7-1.5% of Mn, 0.01-0.015% of Sr, 0.01-0.015% of Cr, 0-0.4% of Fe, 0.02-0.1% of Ti, 0.01-0.02% of Ga, 0.004-0.02% of B, 0-2% of Zn, and the balance of Al and less than 0.1% of other elements.
Abstract:
A die-cast aluminum alloy and a preparation method and use thereof are disclosed. Based on the total mass of the die-cast aluminum alloy, the die-cast aluminum alloy includes: 4-9 wt % of Mg; 1.6-2.8 wt % of Si; 1.1-2 wt % of Zn; wt % of Mn; 0.1-0.3 wt % of Ti; 0.009-0.05 wt % of Be; the balance of Al; and less than 0.2 wt % of inevitable impurities.