公开(公告)号:US08051991B2
公开(公告)日:2011-11-08
申请号:US12307670
申请日:2007-06-25
申请人: Bernd Krause , Markus Hornung , Herman Goehl
发明人: Bernd Krause , Markus Hornung , Herman Goehl
CPC分类号: B01D69/087 , A61M1/3496 , B01D67/0011 , B01D69/02 , B01D69/08 , B01D71/44 , B01D71/68 , B01D2323/12 , Y10T428/1376 , Y10T428/139
摘要: A process for manufacturing of an asymmetric hollow fiber membrane, comprising the steps of extruding a polymer solution through the outer ring slit of a hollow fiber spinning nozzle, simultaneously extruding a center fluid through the inner bore of the hollow fiber spinning nozzle, into a precipitation bath, whereby the polymer solution contains 10 to 26 wt-% of polysulfone (PSU), polyethersulfone (PES) or polyarylethersulfone (PAES), 8 to 15 wt-% polyvinylpyrrolidone (PVP), 55 to 75 wt-% N-alkyl-2-pyrrolidone (NAP) and 3 to 9 wt-% water the centre fluid contains 70 to 90 wt-% N-alkyl-2-pyrrolidone (NAP) and 10 to 30 wt-% water, and the precipitation bath contains 0 to 20 wt-% N-alkyl-2-pyrrolidone (NAP) and 80 to 100 wt-% water.
摘要翻译: 一种不对称中空纤维膜的制造方法,其特征在于,包括以下步骤:通过中空纤维纺丝喷嘴的外圈狭缝挤出聚合物溶液,同时将中心流体通过中空纤维纺丝喷嘴的内孔挤出成为沉淀物 由此聚合物溶液含有10-26重量%的聚砜(PSU),聚醚砜(PES)或聚芳醚砜(PAES),8-15重量%的聚乙烯吡咯烷酮(PVP),55-75重量%的N-烷基 - 2-吡咯烷酮(NAP)和3〜9重量%的水,中心流体含有70〜90重量%的N-烷基-2-吡咯烷酮(NAP)和10〜30重量%的水,沉淀浴中含有0〜 20重量%的N-烷基-2-吡咯烷酮(NAP)和80-100重量%的水。
-
公开(公告)号:US20090283470A1
公开(公告)日:2009-11-19
申请号:US12307678
申请日:2007-06-25
申请人: Bernd Krause , Markus Hornung , Herman Goehl
发明人: Bernd Krause , Markus Hornung , Herman Goehl
CPC分类号: B01D67/0011 , B01D69/02 , B01D69/08 , B01D69/081 , B01D69/085 , B01D71/68 , B01D2325/022 , B01D2325/24 , B01D2325/28 , B01D2325/36
摘要: A process for manufacturing of an asymmetric hollow fibre membrane, comprising the steps of extruding a polymer solution through the outer ring slit of a hollow fibre spinning nozzle, simultaneously extruding a centre fluid through the inner bore of the hollow fibre spinning nozzle, into a precipitation bath, whereby the polymer solution contains 10 to 26 wt-% of polysulfone (PSU), polyethersulfone (PES) or polyarylethersulfone (PAES), 8 to 15 wt-% polyvinylpyrrolidone (PVP) and 60 to 80 wt-% N-alkyl-2-pyrrolidone (NAP), the centre fluid contains 60 to 70 wt-% N-alkyl-2-pyrrolidone (NAP) and 30 to 40 wt-% water, and the precipitation bath contains 70 to 82 wt-% N-alkyl-2-pyrrolidone (NAP) and 18 to 30 wt-% water.
摘要翻译: 一种不对称中空纤维膜的制造方法,其特征在于,包括以下步骤:通过中空纤维纺丝喷嘴的外圈狭缝挤出聚合物溶液,同时将中心流体通过中空纤维纺丝喷嘴的内孔挤出成为沉淀物 由此聚合物溶液含有10-26重量%的聚砜(PSU),聚醚砜(PES)或聚芳醚砜(PAES),8-15重量%聚乙烯吡咯烷酮(PVP)和60-80重量%N-烷基 - 2-吡咯烷酮(NAP),中心流体含有60〜70重量%的N-烷基-2-吡咯烷酮(NAP)和30〜40重量%的水,沉淀浴含有70〜82重量%的N-烷基 -2-吡咯烷酮(NAP)和18-30wt%水。
-
公开(公告)号:US07931154B2
公开(公告)日:2011-04-26
申请号:US12307678
申请日:2007-06-25
申请人: Bernd Krause , Markus Hornung , Herman Goehl
发明人: Bernd Krause , Markus Hornung , Herman Goehl
CPC分类号: B01D67/0011 , B01D69/02 , B01D69/08 , B01D69/081 , B01D69/085 , B01D71/68 , B01D2325/022 , B01D2325/24 , B01D2325/28 , B01D2325/36
摘要: A process for manufacturing of an asymmetric hollow fiber membrane, comprising the steps of extruding a polymer solution through the outer ring slit of a hollow fiber spinning nozzle, simultaneously extruding a center fluid through the inner bore of the hollow fiber spinning nozzle, into a precipitation bath, whereby the polymer solution contains 10 to 26 wt-% of polysulfone (PSU), polyethersulfone (PES) or polyarylethersulfone (PAES), 8 to 15 wt-% polyvinylpyrrolidone (PVP) and 60 to 80 wt-% N-alkyl-2-pyrrolidone (NAP), the center fluid contains 60 to 70 wt-% N-alkyl-2-pyrrolidone (NAP) and 30 to 40 wt-% water, and the precipitation bath contains 70 to 82 wt-% N-alkyl-2-pyrrolidone (NAP) and 18 to 30 wt-% water.
摘要翻译: 一种不对称中空纤维膜的制造方法,其特征在于,包括以下步骤:通过中空纤维纺丝喷嘴的外圈狭缝挤出聚合物溶液,同时将中心流体通过中空纤维纺丝喷嘴的内孔挤出成为沉淀物 由此聚合物溶液含有10-26重量%的聚砜(PSU),聚醚砜(PES)或聚芳醚砜(PAES),8-15重量%聚乙烯吡咯烷酮(PVP)和60-80重量%N-烷基 - 2-吡咯烷酮(NAP),中心流体含有60〜70重量%的N-烷基-2-吡咯烷酮(NAP)和30〜40重量%的水,沉淀浴含有70〜82重量%的N-烷基 -2-吡咯烷酮(NAP)和18-30wt%水。
-
公开(公告)号:US20100012577A1
公开(公告)日:2010-01-21
申请号:US12307670
申请日:2007-06-25
申请人: Bernd Krause , Markus Hornung , Herman Goehl
发明人: Bernd Krause , Markus Hornung , Herman Goehl
CPC分类号: B01D69/087 , A61M1/3496 , B01D67/0011 , B01D69/02 , B01D69/08 , B01D71/44 , B01D71/68 , B01D2323/12 , Y10T428/1376 , Y10T428/139
摘要: A process for manufacturing of an asymmetric hollow fibre membrane, comprising the steps of extruding a polymer solution through the outer ring slit of a hollow fibre spinning nozzle, simultaneously extruding a centre fluid through the inner bore of the hollow fibre spinning nozzle, into a precipitation bath, whereby the polymer solution contains 10 to 26 wt-% of polysulfone (PSU), polyethersulfone (PES) or polyarylethersulfone (PAES), 8 to 15 wt-% polyvinylpyrrolidone (PVP), 55 to 75 wt-% N-alkyl-2-pyrrolidone (NAP) and 3 to 9 wt-% w ater the centre fluid contains 70 to 90 wt-% N-alkyl-2-pyrrolidone (NAP) and 10 to 30 wt-% water, and the precipitation bath contains 0 to 20 wt-% N-alkyl-2-pyrrolidone (NAP) and 80 to 100 wt-% water.
摘要翻译: 一种不对称中空纤维膜的制造方法,其特征在于,包括以下步骤:通过中空纤维纺丝喷嘴的外圈狭缝挤出聚合物溶液,同时将中心流体通过中空纤维纺丝喷嘴的内孔挤出成为沉淀物 由此聚合物溶液含有10-26重量%的聚砜(PSU),聚醚砜(PES)或聚芳醚砜(PAES),8-15重量%的聚乙烯吡咯烷酮(PVP),55-75重量%的N-烷基 - 2-吡咯烷酮(NAP)和3至9重量%的中心流体含有70-90重量%的N-烷基-2-吡咯烷酮(NAP)和10-30重量%的水,沉淀浴含有0 至20重量%的N-烷基-2-吡咯烷酮(NAP)和80至100重量%的水。
-
-
-