Abstract:
Embodiments of the present disclosure are directed to methods for inducing color change in glass and glass-ceramic articles. According to one embodiment, color change may be x-ray induced in glass or glass-ceramic articles. The method for x-ray inducing color change may include exposing the glass or glass-ceramic article to x-rays at a temperature of up to 200° C. to induce a colored area in the glass or glass-ceramic article. The glass or glass-ceramic article may comprise: 50-85 mole % SiO2; 5-25 mole % Al2O3; 0-15 mole % P2O5; 0-15 mole % B2O3; 5-25 mole % R2O, wherein R2O=Li2O+Na2O+K2O.
Abstract:
A method of forming a multi-colored glass substrate comprises: irradiating a first region of a glass substrate with a first high energy source to form a first irradiated glass substrate; and subjecting the irradiated glass substrate to a first heat treatment to form a first heat treated glass substrate, wherein the first heat treated glass substrate comprises a second region having a different transmittance color coordinate in the CIELAB color space, as measured at an article thickness of 1.33 mm under F2 illumination and a 10° standard observer angle, than the first region.
Abstract:
Embodiments of the present disclosure are directed to methods for inducing color change in glass and glass-ceramic articles. According to one embodiment, color change may be x-ray induced in glass or glass-ceramic articles. The method for x-ray inducing color change may include exposing the glass or glass-ceramic article to x-rays at a temperature of up to 200° C. to induce a colored area in the glass or glass-ceramic article. The glass or glass-ceramic article may comprise: 50-85 mole % SiO2; 5-25 mole % Al2O3; 0-15 mole % P2O5; 0-15 mole % B2O3; 5-25 mole % R2O, wherein R2O=Li2O+Na2O+K2O.
Abstract:
Embodiments of the present disclosure are directed to methods for inducing color change in glass and glass-ceramic articles. According to one embodiment, color change may be x-ray induced in glass or glass-ceramic articles. The method for x-ray inducing color change may include exposing the glass or glass-ceramic article to x-rays at a temperature of up to 200° C. to induce a colored area in the glass or glass-ceramic article. The glass or glass-ceramic article may comprise: 50-85 mole % SiO2; 5-25 mole % Al2O3; 0-15 mole % P2O5; 0-15 mole % B2O3; 5-25 mole % R2O, wherein R2O=Li2O+Na2O+K2O.