公开(公告)号:US11885998B2
公开(公告)日:2024-01-30
申请号:US17759938
申请日:2021-02-01
Applicant: Corning Incorporated
Inventor: Joy Banerjee , Indrani Bhattacharyya , Prantik Mazumder , Wanda Janina Walczak
CPC classification number: G02B6/0043 , C03C17/3405 , G02B6/0061 , G02B6/0065 , C03C2218/32
Abstract: A display backlight unit is disclosed including a glass substrate with a first major surface and a second major surface opposite the first major surface, the first major surface coated with at least one of 3-mercaptopropyl trimethoxysilane, aminopropyl triethoxysilane, or silanated PMMA, and a plurality of PMMA-containing light extraction dots deposited on the coated first major surface.
-
公开(公告)号:US20230103045A1
公开(公告)日:2023-03-30
申请号:US17787014
申请日:2021-01-05
Applicant: Corning Incorporated
Inventor: Gabriel Pierce Agnello , Joy Banerjee , Aize Li , Robert George Manley , Huan-Hung Sheng , Siva Venkatachalam
Abstract: Apparatus and method for treating a substrate, for example texturing a substrate. In some embodiments, a masking material is applied to a surface of the substrate in a predetermined pattern, the surface thereafter contacted with an etchant that removes the masking material. Contacting the surface with the etchant produces multiple co-located textures. In other embodiments, the masking step can be eliminated, and the etchant is applied in a predetermined pattern to produce multiple co-located textures. In still other embodiments, the substrate has a chemical composition, and the substrate is exposed to a leachant that leaches at least one constituent of the chemical composition to produce a substrate with a varying chemical composition at the substrate surface.
-
公开(公告)号:US12275666B2
公开(公告)日:2025-04-15
申请号:US17787014
申请日:2021-01-05
Applicant: Corning Incorporated
Inventor: Gabriel Pierce Agnello , Joy Banerjee , Aize Li , Robert George Manley , Huan-Hung Sheng , Siva Venkatachalam
Abstract: Apparatus and method for treating a substrate, for example texturing a substrate. In some embodiments, a masking material is applied to a surface of the substrate in a predetermined pattern, the surface thereafter contacted with an etchant that removes the masking material. Contacting the surface with the etchant produces multiple co-located textures. In other embodiments, the masking step can be eliminated, and the etchant is applied in a predetermined pattern to produce multiple co-located textures. In still other embodiments, the substrate has a chemical composition, and the substrate is exposed to a leachant that leaches at least one constituent of the chemical composition to produce a substrate with a varying chemical composition at the substrate surface.
-
公开(公告)号:US20230152506A1
公开(公告)日:2023-05-18
申请号:US17759938
申请日:2021-02-01
Applicant: Corning Incorporated
Inventor: Joy Banerjee , Indrani Bhattacharyya , Prantik Mazumder , Wanda Janina Walczak
CPC classification number: G02B6/0043 , C03C17/3405 , G02B6/0061 , G02B6/0065 , C03C2218/32
Abstract: A display backlight unit is disclosed including a glass substrate with a first major surface and a second major surface opposite the first major surface, the first major surface coated with at least one of 3-mercaptopropyl trimethoxysilane, aminopropyl triethoxysilane, or silanated PMMA, and a plurality of PMMA-containing light extraction dots deposited on the coated first major surface.
-
公开(公告)号:US12240781B2
公开(公告)日:2025-03-04
申请号:US18408113
申请日:2024-01-09
Applicant: CORNING INCORPORATED
Inventor: Gabriel Pierce Agnello , Joy Banerjee , Vitor Marino Schneider , Ian David Tracy
IPC: C03C21/00 , G02F1/1333 , G06F1/16
Abstract: In aspects, a concentration of lithium oxide at a surface is greater than a concentration of lithium oxide at a midpoint by from about 0.2 mol % to about 2 mol %. In aspects, a concentration of lithium oxide at a surface is from about 0.2 mol % to about 2 mol %. In aspects, a total concentration of potassium oxide, rubidium oxide, cesium oxide, and francium oxide at a surface is from about 5 mol % to about 15 mol %. In aspects, a ratio of the total concentration of potassium oxide, rubidium oxide, cesium oxide, and francium oxide at a surface to a concentration of lithium oxide at the surface is from about 1 to about 20. Methods include immersing a substrate in a molten salt bath at 380° C. or more for from about 1 minute to about 10 minutes or for from about 3 minutes to about 2 hours.
-
-
-
-