公开(公告)号:US09902641B2
公开(公告)日:2018-02-27
申请号:US15071889
申请日:2016-03-16
Applicant: CORNING INCORPORATED
Inventor: Jill Marie Hall , Nicholas Scott Ryan , Wenchao Wang , Kim E Womer
IPC: C03B23/035 , C03B23/023 , C23C8/10 , C22C19/03 , C22F1/10 , C03B11/08
CPC classification number: C03B23/0357 , C03B11/086 , C03B23/0235 , C03B2215/03 , C03B2215/11 , C03B2215/20 , C03B2215/32 , C22C19/03 , C22F1/10 , C23C8/10 , Y02P40/57
Abstract: A mold for shaping glass-based material can include a mold body having a surface, wherein at least a portion of the mold body near the surface comprises at least about 90% by weight nickel and from about 0.2% to about 0.35% by weight manganese; and a nickel oxide layer on the surface of the mold body. The nickel oxide layer has first and second opposing surfaces wherein the first surface of the nickel oxide layer contacts and faces the surface of the mold body and the second surface of the nickel oxide layer includes a plurality of grains. The plurality of grains has an average grain size of about 150 μm or less.
-
公开(公告)号:US10029936B2
公开(公告)日:2018-07-24
申请号:US14310665
申请日:2014-06-20
Applicant: Corning Incorporated
Inventor: Paul Richard Grzesik , Ahdi El Kahlout , Nicolas LeBlond , Gaozhu Peng , Kim E Womer
IPC: C03B17/06
Abstract: An apparatus for downwardly drawing glass ribbon comprises edge directors, wherein an outer portion defining a first pair of surfaces and a second pair of surfaces. In one example, the first and second pair of surfaces of each edge director includes a glass wettability with a static contact angle within a range of from about 30° to about 60°. In another example, the outer portion comprises a platinum alloy including from about 0.05 weight % tin to about 5 weight % tin. Methods for forming glass include the step of providing the edge director with a desired glass wettability and/or a desired platinum alloy.
-
3.
公开(公告)号:US09738555B2
公开(公告)日:2017-08-22
申请号:US13904123
申请日:2013-05-29
Applicant: CORNING INCORPORATED
Inventor: Terry Lee Taft , Kim E Womer
CPC classification number: C03B5/1672 , C03B5/027 , H05B3/03 , Y10T29/49083
Abstract: A method of making an electrode assembly for a furnace includes providing a heating element within the furnace. The method further includes providing a power feedthrough having an end portion that extends into the furnace to couple with the heating element. The power feedthrough includes a conductive member for transmitting electricity to the heating element. The method includes cleaning an exterior surface of the conductive member proximate the end portion of the power feedthrough. The method further includes a step of applying an electroless nickel plating to the exterior surface of the conductive member for preventing corrosion of the conductive member within the furnace. The method also includes connecting the end portion of the power feedthrough to the heating element.
-
4.
公开(公告)号:US09145323B2
公开(公告)日:2015-09-29
申请号:US14158262
申请日:2014-01-17
Applicant: Corning Incorporated
Inventor: Kristen Marie Horn , David Myron Lineman , Kevin Thomas Morris , Wenchao Wang , Kim E Womer
IPC: C03B11/08 , C03B11/00 , C03B23/035 , C23C8/10 , C03B40/02 , C03B23/025 , C03B23/03
CPC classification number: C03B40/00 , C03B11/00 , C03B23/002 , C03B23/023 , C03B23/0252 , C03B23/0302 , C03B23/0355 , C03B23/0357 , C03B40/02 , C23C8/10 , Y02P40/57
Abstract: A mold for shaping glass can be made by a method that includes providing a mold body having a shaping surface comprising at least about 90% nickel and modifying the composition of the shaping surface of the mold body by exposing the shaping surface to an oxidizing heat treatment. The oxidizing heat treatment may include a ramping heat treatment, a fixed heat treatment, or both the ramping heat treatment and the fixed heat treatment. The ramping heat treatment may include increasing a heating temperature at a rate from about 20° C./hour to about 500° C./hour to a temperature from about 700° C. to about 1000° C. The fixed heat treatment may include holding the heating temperature from about 700° C. to about 1000° C. for a holding time of at least about 5 minutes.
Abstract translation: 用于成形玻璃的模具可以通过包括提供具有包括至少约90%的镍的成形表面的模具主体并通过将成形表面暴露于氧化热处理来改变模制体的成形表面的组成的方法来制备 。 氧化热处理可以包括斜坡热处理,固定热处理,或斜坡加热处理和固定热处理两者。 升温热处理可以包括以约20℃/小时至约500℃/小时的速度升高加热温度至约700℃至约1000℃的温度。固定热处理可包括 将加热温度保持在约700℃至约1000℃,保持时间至少约5分钟。
-
-
-