ELASTIC EXPANDED POLYMER FOAM BASED ON POLYOLEFIN/STYRENE POLYMER MIXTURES
    2.
    发明申请
    ELASTIC EXPANDED POLYMER FOAM BASED ON POLYOLEFIN/STYRENE POLYMER MIXTURES 失效
    基于聚烯烃/苯乙烯聚合物混合物的弹性膨胀聚合物泡沫

    公开(公告)号:US20110316198A1

    公开(公告)日:2011-12-29

    申请号:US13254174

    申请日:2010-03-01

    IPC分类号: C08L25/06

    摘要: The invention relates to elastic expanded polymer foams and also a process for producing expanded polymer foams by sintering a mixture comprising foam particles P1 and P2 composed of different thermoplastic polymers or polymer blends, wherein the foam particles P1 are obtained by prefoaming expandable, thermoplastic polymer particles comprising A) from 45 to 97.9 percent by weight of a styrene polymer, B1) from 1 to 45 percent by weight of a polyolefin having a melting point in the range from 105 to 140° C., B2) from 0 to 25 percent by weight of a polyolefin having a melting point below 105° C., C1) from 0.1 to 25 percent by weight of a styrene-butadiene or styrene-isoprene block copolymer, C2) from 0.0 to 10 percent by weight of a styrene-ethylene-butylene block copolymer, D) from 1 to 15 percent by weight of a blowing agent, E) from 0 to 5 percent by weight of a nucleating agent, where the sum of A) to E) is 100% by weight.

    摘要翻译: 本发明涉及弹性膨胀聚合物泡沫,还涉及通过烧结由不同的热塑性聚合物或聚合物共混物组成的泡沫颗粒P1和P2的混合物来生产发泡聚合物泡沫的方法,其中泡沫颗粒P1是通过预发泡的可发泡热塑性聚合物颗粒 包括A)45至97.9重量%的苯乙烯聚合物,B1)1至45重量%的熔点在105-140℃的聚烯烃,B2)0-25重量% 熔点低于105℃的聚烯烃的重量,C1)0.1至25重量%的苯乙烯 - 丁二烯或苯乙烯 - 异戊二烯嵌段共聚物,C2)0.0至10重量%的苯乙烯 - 乙烯 - 丁烯嵌段共聚物,D)1〜15重量%的发泡剂,E)0〜5重量%的成核剂,其中A)与E)之和为100重量%。

    Elastic expanded polymer foam based on polyolefin/styrene polymer mixtures
    4.
    发明授权
    Elastic expanded polymer foam based on polyolefin/styrene polymer mixtures 失效
    基于聚烯烃/苯乙烯聚合物混合物的弹性膨胀聚合物泡沫

    公开(公告)号:US08741973B2

    公开(公告)日:2014-06-03

    申请号:US13254174

    申请日:2010-03-01

    IPC分类号: C08L25/06 C08J9/16

    摘要: The invention relates to elastic expanded polymer foams and also a process for producing expanded polymer foams by sintering a mixture comprising foam particles P1 and P2 composed of different thermoplastic polymers or polymer blends, wherein the foam particles P1 are obtained by prefoaming expandable, thermoplastic polymer particles comprising A) from 45 to 97.9 percent by weight of a styrene polymer, B1) from 1 to 45 percent by weight of a polyolefin having a melting point in the range from 105 to 140° C., B2) from 0 to 25 percent by weight of a polyolefin having a melting point below 105° C., C1) from 0.1 to 25 percent by weight of a styrene-butadiene or styrene-isoprene block copolymer, C2) from 0.0 to 10 percent by weight of a styrene-ethylene-butylene block copolymer, D) from 1 to 15 percent by weight of a blowing agent, E) from 0 to 5 percent by weight of a nucleating agent, where the sum of A) to E) is 100% by weight.

    摘要翻译: 本发明涉及弹性膨胀聚合物泡沫,还涉及通过烧结由不同的热塑性聚合物或聚合物共混物构成的泡沫颗粒P1和P2的混合物来生产发泡聚合物泡沫的方法,其中泡沫颗粒P1是通过预发泡的可发泡热塑性聚合物颗粒 包括A)45至97.9重量%的苯乙烯聚合物,B1)1至45重量%的熔点在105-140℃的聚烯烃,B2)0-25重量% 熔点低于105℃的聚烯烃的重量,C1)0.1至25重量%的苯乙烯 - 丁二烯或苯乙烯 - 异戊二烯嵌段共聚物,C2)0.0至10重量%的苯乙烯 - 乙烯 - 丁烯嵌段共聚物,D)1〜15重量%的发泡剂,E)0〜5重量%的成核剂,其中A)与E)之和为100重量%。