Lubricant for the hot forming of metals

    公开(公告)号:US11485929B2

    公开(公告)日:2022-11-01

    申请号:US17310710

    申请日:2020-02-21

    摘要: A lubricant for the hot forming of metals, with respect to the solid constituents, contains at least the following constituents: 55 to 85 wt % of a solid lubricating agent comprising a mixture of talc and a potassium mica, wherein the ratio of talc to potassium mica in the solid lubricating agent is 2.0 to 5.0, 10 to 30 wt % of an adhesive agent selected from a polyvinyl acetate, sodium water glass and dextrin or a mixture of same, 2 to 10 wt % of a thickener selected from hydroxy cellulose, hydroxyethyl cellulose, hydroxyproply cellulose, carboxymethyl cellulose, methyl cellulose, ethyl cellulose, methylethyl cellulose, hydroxyethylmethyl cellulose, hydroxypropylmethyl cellulose, ethylhydroxymethyl cellulose, carboxymethylhydroxy cellulose, dextrin, starch, organically modified bentonite, smectite and xanthan gum, 0 to 10 wt % of further auxiliary agents, and not more than 10 wt % of graphite.

    Composition for protection from scale and as lubricant for hot processing metals

    公开(公告)号:US10995297B2

    公开(公告)日:2021-05-04

    申请号:US14778322

    申请日:2014-03-11

    摘要: A composition for protection from scale and as a lubricant for the hot processing of metals is disclosed. The composition includes a mixture of fine-powder materials containing at least the following constituents: (a) 0 to 15% by weight of secondary or tertiary calcium phosphate compound, hydroxyapatite or a mixture thereof, (b) 0.1 to 35% by weight of fatty acid, fatty acid salt or a mixture thereof, (c) 1 to 90% by weight of ground borosilicate glass which in relation to the borosilicate glass contains Na, B, Si and Al in the following proportions by weight expressed by their respective oxides: 1 to 30% by weight of Na2O, 2 to 70% by weight of B2O3, 10 to 70% by weight of SiO2, and 0 to 10% by weight of Al2O3, (d) 9 to 85% by weight of condensed alkali metal phosphates, (e) boric acid, boric acid salt or a mixture thereof in an amount corresponding to a boron content, expressed by the oxide, of 0 to 3.2% by weight of B2O3, and (f) 0 to 10% by weight of graphite. The mixture has a mean particle size D50 of