公开(公告)号:US07967875B2
公开(公告)日:2011-06-28
申请号:US12791221
申请日:2010-06-01
申请人: Christopher Boczer , Frank M. Delnick , Rosauro Del Rosario , Minkoo Kang , Lucyna M. Pawlowska , Michael Pozin , Dharmendra Rana , Maya Stevanovic , John J. Weckesser
发明人: Christopher Boczer , Frank M. Delnick , Rosauro Del Rosario , Minkoo Kang , Lucyna M. Pawlowska , Michael Pozin , Dharmendra Rana , Maya Stevanovic , John J. Weckesser
IPC分类号: H01M4/13 , H01M4/62 , H01M10/0568 , H01M10/0569
CPC分类号: H01M10/0569 , H01M4/0404 , H01M4/0411 , H01M4/131 , H01M4/1391 , H01M4/505 , H01M4/621 , H01M4/622 , H01M4/661 , H01M10/0525 , Y10T29/49108 , Y10T29/49115
摘要: This disclosure relates to methods of making a cathode for a lithium batter. The methods include: (a) treating a cathode current collector with flame or corona; (b) coating a slurry containing iron disulfide, a first solvent, and a binder onto the cathode current collector obtained from step (a) to form a coated cathode current collector, in which the slurry contains about 73-75% by weight solids and the binder contains a polymer selected from the group consisting of linear di- and tri-block copolymers, linear tri-block copolymers cross-linked with melamine resin, ethylene-propylene copolymers, ethylene-propylene-diene terpolymers, tri-block fluorinated thermoplastics, hydrogenated nitrile rubbers, fluoro-ethylene-vinyl ether copolymers, thermoplastic polyurethanes, thermoplastic olefins, and polyvinylidene fluoride homopolymers; and (c) drying the coated cathode current collector obtained from step (b) to provide a cathode, in which the cathode contains no more than 0.5% by volume of the first solvent and is capable of being bent to 180°. This disclosure also relates to methods of making a lithium battery.
摘要翻译: 本公开涉及制备用于锂电池的阴极的方法。 方法包括:(a)用火焰或电晕处理阴极集电器; (b)将含有二硫化铁,第一溶剂和粘合剂的浆料涂布到从步骤(a)获得的阴极集流体上,以形成涂覆的阴极集电器,其中浆料含有约73-75重量%的固体, 粘合剂含有选自直链二嵌段和三嵌段共聚物,与三聚氰胺树脂交联的直链三嵌段共聚物,乙烯 - 丙烯共聚物,乙烯 - 丙烯 - 二烯三元共聚物,三嵌段氟化热塑性塑料, 氢化丁腈橡胶,氟乙烯 - 乙烯基醚共聚物,热塑性聚氨酯,热塑性烯烃和聚偏氟乙烯均聚物; 和(c)将由步骤(b)获得的涂覆的阴极集电体干燥以提供阴极,其中阴极含有不超过0.5体积%的第一溶剂并且能够弯曲至180°。 本公开还涉及制造锂电池的方法。
-
公开(公告)号:US07753968B2
公开(公告)日:2010-07-13
申请号:US12408869
申请日:2009-03-23
申请人: Christopher Boczer , Frank M. Delnick , Rosauro Del Rosario , Minkoo Kang , Lucyna M. Pawlowska , Michael Pozin , Dharmendra Rana , Maya Stevanovic , John J. Weckesser
发明人: Christopher Boczer , Frank M. Delnick , Rosauro Del Rosario , Minkoo Kang , Lucyna M. Pawlowska , Michael Pozin , Dharmendra Rana , Maya Stevanovic , John J. Weckesser
CPC分类号: H01M10/0569 , H01M4/0404 , H01M4/0411 , H01M4/131 , H01M4/1391 , H01M4/505 , H01M4/621 , H01M4/622 , H01M4/661 , H01M10/0525 , Y10T29/49108 , Y10T29/49115
摘要: This disclosure relates to methods of making a cathode for a lithium batter. The methods include: (a) treating a cathode current collector with flame or corona; (b) coating a slurry containing iron disulfide, a first solvent, and a binder onto the cathode current collector obtained from step (a) to form a coated cathode current collector, in which the slurry contains about 73-75% by weight solids and the binder contains a polymer selected from the group consisting of linear di- and tri-block copolymers, linear tri-block copolymers cross-linked with melamine resin, ethylene-propylene copolymers, ethylene-propylene-diene terpolymers, tri-block fluorinated thermoplastics, hydrogenated nitrile rubbers, fluoro-ethylene-vinyl ether copolymers, thermoplastic polyurethanes, thermoplastic olefins, and polyvinylidene fluoride homopolymers; and (c) drying the coated cathode current collector obtained from step (b) to provide a cathode, in which the cathode contains no more than 0.5% by volume of the first solvent and is capable of being bent to 180°. This disclosure also relates to methods of making a lithium battery.
摘要翻译: 本公开涉及制备用于锂电池的阴极的方法。 方法包括:(a)用火焰或电晕处理阴极集电器; (b)将含有二硫化铁,第一溶剂和粘合剂的浆料涂布到从步骤(a)获得的阴极集流体上,以形成涂覆的阴极集电器,其中浆料含有约73-75重量%的固体, 粘合剂含有选自直链二嵌段和三嵌段共聚物,与三聚氰胺树脂交联的直链三嵌段共聚物,乙烯 - 丙烯共聚物,乙烯 - 丙烯 - 二烯三元共聚物,三嵌段氟化热塑性塑料, 氢化丁腈橡胶,氟乙烯 - 乙烯基醚共聚物,热塑性聚氨酯,热塑性烯烃和聚偏氟乙烯均聚物; 和(c)将由步骤(b)获得的涂覆的阴极集电体干燥以提供阴极,其中阴极含有不超过0.5体积%的第一溶剂并且能够弯曲至180°。 本公开还涉及制造锂电池的方法。
-
公开(公告)号:US20100236056A1
公开(公告)日:2010-09-23
申请号:US12791221
申请日:2010-06-01
申请人: Christopher Boczer , Frank M. Delnick , Rosauro Del Rosario , Minkoo Kang , Lucyna M. Pawlowska , Michael Pozin , Dharmendra Rana , Maya Stevanovic , John J. Weckesser
发明人: Christopher Boczer , Frank M. Delnick , Rosauro Del Rosario , Minkoo Kang , Lucyna M. Pawlowska , Michael Pozin , Dharmendra Rana , Maya Stevanovic , John J. Weckesser
IPC分类号: H01M10/04
CPC分类号: H01M10/0569 , H01M4/0404 , H01M4/0411 , H01M4/131 , H01M4/1391 , H01M4/505 , H01M4/621 , H01M4/622 , H01M4/661 , H01M10/0525 , Y10T29/49108 , Y10T29/49115
摘要: This disclosure relates to methods of making a cathode for a lithium batter. The methods include: (a) treating a cathode current collector with flame or corona; (b) coating a slurry containing iron disulfide, a first solvent, and a binder onto the cathode current collector obtained from step (a) to form a coated cathode current collector, in which the slurry contains about 73-75% by weight solids and the binder contains a polymer selected from the group consisting of linear di- and tri-block copolymers, linear tri-block copolymers cross-linked with melamine resin, ethylene-propylene copolymers, ethylene-propylene-diene terpolymers, tri-block fluorinated thermoplastics, hydrogenated nitrile rubbers, fluoro-ethylene-vinyl ether copolymers, thermoplastic polyurethanes, thermoplastic olefins, and polyvinylidene fluoride homopolymers; and (c) drying the coated cathode current collector obtained from step (b) to provide a cathode, in which the cathode contains no more than 0.5% by volume of the first solvent and is capable of being bent to 180°. This disclosure also relates to methods of making a lithium battery.
摘要翻译: 本公开涉及制备用于锂电池的阴极的方法。 方法包括:(a)用火焰或电晕处理阴极集电器; (b)将含有二硫化铁,第一溶剂和粘合剂的浆料涂布到从步骤(a)获得的阴极集流体上,以形成涂覆的阴极集电器,其中浆料含有约73-75重量%的固体, 粘合剂含有选自直链二嵌段和三嵌段共聚物,与三聚氰胺树脂交联的直链三嵌段共聚物,乙烯 - 丙烯共聚物,乙烯 - 丙烯 - 二烯三元共聚物,三嵌段氟化热塑性塑料, 氢化丁腈橡胶,氟乙烯 - 乙烯基醚共聚物,热塑性聚氨酯,热塑性烯烃和聚偏氟乙烯均聚物; 和(c)将由步骤(b)获得的涂覆的阴极集电体干燥以提供阴极,其中阴极含有不超过0.5体积%的第一溶剂并且能够弯曲至180°。 本公开还涉及制造锂电池的方法。
-
公开(公告)号:US07033698B2
公开(公告)日:2006-04-25
申请号:US10290832
申请日:2002-11-08
申请人: Christopher Boczer , Frank M. Delnick , Rosauro Del Rosario , Minkoo Kang , Lucyna M. Pawlowska , Michael Pozin , Dharmendra Rana , Maya Stevanovic , John J. Weckesser
发明人: Christopher Boczer , Frank M. Delnick , Rosauro Del Rosario , Minkoo Kang , Lucyna M. Pawlowska , Michael Pozin , Dharmendra Rana , Maya Stevanovic , John J. Weckesser
CPC分类号: H01M10/0569 , H01M4/0404 , H01M4/0411 , H01M4/131 , H01M4/1391 , H01M4/505 , H01M4/621 , H01M4/622 , H01M4/661 , H01M10/0525 , Y10T29/49108 , Y10T29/49115
摘要: A cathode for a lithium battery is described. The cathode includes: (a) a current collector including aluminum foil; and (b) an active cathode material including: (i) manganese dioxide; (ii) conductive materials; and (iii) a binder selected from the group consisting of linear di- and tri-block polymers, linear tri-block polymers cross-linked with melamine resin, ethylene-propylene copolymers, ethylene-propylene-diene terpolymers, tri-block fluorinated thermoplastics, hydrogenated nitrile rubbers, fluoro-ethylene-vinyl ether copolymers, thermoplastic polyurethanes, thermoplastic olefins, and polyvinylidine fluoride homopolymers.
摘要翻译: 描述了用于锂电池的阴极。 阴极包括:(a)集电体,包括铝箔; 和(b)活性阴极材料,包括:(i)二氧化锰; (ii)导电材料; 和(iii)选自线性二嵌段和三嵌段聚合物的粘合剂,与三聚氰胺树脂交联的直链三嵌段聚合物,乙烯 - 丙烯共聚物,乙烯 - 丙烯 - 二烯三元共聚物,三嵌段氟化热塑性塑料 氢化丁腈橡胶,氟乙烯 - 乙烯基醚共聚物,热塑性聚氨酯,热塑性烯烃和聚偏二氟乙烯均聚物。
-
公开(公告)号:US20110254509A1
公开(公告)日:2011-10-20
申请号:US13150538
申请日:2011-06-01
申请人: Christopher Boczer , Frank M. Delnick , Rosauro Del Rosario , Minkoo Kang , Lucyna M. Pawlowska , Michael Pozin , Dharmendra Rana , Maya Stevanovic , John J. Weckesser
发明人: Christopher Boczer , Frank M. Delnick , Rosauro Del Rosario , Minkoo Kang , Lucyna M. Pawlowska , Michael Pozin , Dharmendra Rana , Maya Stevanovic , John J. Weckesser
CPC分类号: H01M10/0569 , H01M4/0404 , H01M4/0411 , H01M4/131 , H01M4/1391 , H01M4/505 , H01M4/621 , H01M4/622 , H01M4/661 , H01M10/0525 , Y10T29/49108 , Y10T29/49115
摘要: This disclosure relates to methods of making a cathode for a lithium batter. The batterys include: (a) treating a cathode current collector with flame or corona; (b) coating a slurry containing iron disulfide, a first solvent, and a binder onto the cathode current collector obtained from step (a) to form a coated cathode current collector, in which the slurry contains about 73-75% by weight solids and the binder contains a polymer selected from the group consisting of linear di- and tri-block copolymers, linear tri-block copolymers cross-linked with melamine resin, ethylene-propylene copolymers, ethylene-propylene-diene terpolymers, tri-block fluorinated thermoplastics, hydrogenated nitrile rubbers, fluoro-ethylene-vinyl ether copolymers, thermoplastic polyurethanes, thermoplastic olefins, and polyvinylidene fluoride homopolymers; and (c) drying the coated cathode current collector obtained from step (b) to provide a cathode, in which the cathode contains no more than 0.5% by volume of the first solvent and is capable of being bent to 180°. This disclosure also relates to methods of making a lithium battery.
摘要翻译: 本公开涉及制备用于锂电池的阴极的方法。 电池包括:(a)用火焰或电晕处理阴极集电器; (b)将含有二硫化铁,第一溶剂和粘合剂的浆料涂布到从步骤(a)获得的阴极集流体上,以形成涂覆的阴极集电器,其中浆料含有约73-75重量%的固体, 粘合剂含有选自直链二嵌段和三嵌段共聚物,与三聚氰胺树脂交联的直链三嵌段共聚物,乙烯 - 丙烯共聚物,乙烯 - 丙烯 - 二烯三元共聚物,三嵌段氟化热塑性塑料, 氢化丁腈橡胶,氟乙烯 - 乙烯基醚共聚物,热塑性聚氨酯,热塑性烯烃和聚偏氟乙烯均聚物; 和(c)将由步骤(b)获得的涂覆的阴极集电体干燥以提供阴极,其中阴极含有不超过0.5体积%的第一溶剂并且能够弯曲至180°。 本公开还涉及制造锂电池的方法。
-
公开(公告)号:US20090199394A1
公开(公告)日:2009-08-13
申请号:US12408869
申请日:2009-03-23
申请人: Christopher Boczer , Frank M. Delnick , Rosauro Del Rosario , Minkoo Kang , Lucyna M. Pawlowska , Michael Pozin , Dharmendra Rana , Maya Stevanovic , John J. Weckesser
发明人: Christopher Boczer , Frank M. Delnick , Rosauro Del Rosario , Minkoo Kang , Lucyna M. Pawlowska , Michael Pozin , Dharmendra Rana , Maya Stevanovic , John J. Weckesser
CPC分类号: H01M10/0569 , H01M4/0404 , H01M4/0411 , H01M4/131 , H01M4/1391 , H01M4/505 , H01M4/621 , H01M4/622 , H01M4/661 , H01M10/0525 , Y10T29/49108 , Y10T29/49115
摘要: This disclosure relates to methods of making a cathode for a lithium batter. The methods include: (a) treating a cathode current collector with flame or corona; (b) coating a slurry containing iron disulfide, a first solvent, and a binder onto the cathode current collector obtained from step (a) to form a coated cathode current collector, in which the slurry contains about 73-75% by weight solids and the binder contains a polymer selected from the group consisting of linear di- and tri-block copolymers, linear tri-block copolymers cross-linked with melamine resin, ethylene-propylene copolymers, ethylene-propylene-diene terpolymers, tri-block fluorinated thermoplastics, hydrogenated nitrile rubbers, fluoro-ethylene-vinyl ether copolymers, thermoplastic polyurethanes, thermoplastic olefins, and polyvinylidene fluoride homopolymers; and (c) drying the coated cathode current collector obtained from step (b) to provide a cathode, in which the cathode contains no more than 0.5% by volume of the first solvent and is capable of being bent to 180°. This disclosure also relates to methods of making a lithium battery.
摘要翻译: 本公开涉及制备用于锂电池的阴极的方法。 方法包括:(a)用火焰或电晕处理阴极集电器; (b)将含有二硫化铁,第一溶剂和粘合剂的浆料涂布到从步骤(a)获得的阴极集流体上,以形成涂覆的阴极集电器,其中浆料含有约73-75重量%的固体, 粘合剂含有选自直链二嵌段和三嵌段共聚物,与三聚氰胺树脂交联的直链三嵌段共聚物,乙烯 - 丙烯共聚物,乙烯 - 丙烯 - 二烯三元共聚物,三嵌段氟化热塑性塑料, 氢化丁腈橡胶,氟乙烯 - 乙烯基醚共聚物,热塑性聚氨酯,热塑性烯烃和聚偏氟乙烯均聚物; 和(c)将由步骤(b)获得的涂覆的阴极集电体干燥以提供阴极,其中阴极含有不超过0.5体积%的第一溶剂并且能够弯曲至180°。 本公开还涉及制造锂电池的方法。
-
公开(公告)号:US07527895B2
公开(公告)日:2009-05-05
申请号:US11375537
申请日:2006-03-14
申请人: Christopher Boczer , Frank M. Delnick , Rosauro Del Rosario , Minkoo Kang , Lucyna M. Pawlowska , Michael Pozin , Dharmendra Rana , Maya Stevanovic , John J. Weckesser
发明人: Christopher Boczer , Frank M. Delnick , Rosauro Del Rosario , Minkoo Kang , Lucyna M. Pawlowska , Michael Pozin , Dharmendra Rana , Maya Stevanovic , John J. Weckesser
CPC分类号: H01M10/0569 , H01M4/0404 , H01M4/0411 , H01M4/131 , H01M4/1391 , H01M4/505 , H01M4/621 , H01M4/622 , H01M4/661 , H01M10/0525 , Y10T29/49108 , Y10T29/49115
摘要: A cathode for a lithium battery is described. The cathode includes: (a) a current collector including aluminum foil; and (b) an active cathode material including: (i) manganese dioxide; (ii) conductive materials; and (iii) a binder selected from the group consisting of linear di- and tri-block polymers, linear tri-block polymers cross-linked with melamine resin, ethylene-propylene copolymers, ethylene-propylene-diene terpolymers, tri-block fluorinated thermoplastics, hydrogenated nitrile rubbers, fluoro-ethylene-vinyl ether copolymers, thermoplastic polyurethanes, thermoplastic olefins, and polyvinylidine fluoride homopolymers.
摘要翻译: 描述了用于锂电池的阴极。 阴极包括:(a)集电体,包括铝箔; 和(b)活性阴极材料,包括:(i)二氧化锰; (ii)导电材料; 和(iii)选自线性二嵌段和三嵌段聚合物的粘合剂,与三聚氰胺树脂交联的直链三嵌段聚合物,乙烯 - 丙烯共聚物,乙烯 - 丙烯 - 二烯三元共聚物,三嵌段氟化热塑性塑料 氢化丁腈橡胶,氟乙烯 - 乙烯基醚共聚物,热塑性聚氨酯,热塑性烯烃和聚偏二氟乙烯均聚物。
-
-
-
-
-
-