摘要:
Heteropoly acids of tungsten and molybdenum, such as tungstosilicic acid and molybdosilicic acid, are produced by first preparing an aqueous solution of an alkali metal tungstate or molybdate and an alkali metal salt of the hetero atom, and then removing the alkali metal cations from the solution by means of a cation exchange membrane under the influence of an applied electrical potential, whereby the reactive tungstate or molybdate and hetero species anions react to form the desired heteropoly acid.
摘要:
Ammonium tungstate, ammonium paratungstate, ammonium metatungstate or hydrated tungsten trioxide is produced by passing tungstate anions through an anion exchange membrane into an aqueous solution containing ammonium cations under the driving force of an electrical potential for a time sufficient to achieve a pH within the range in which the desired tungsten compound will form.
摘要:
A process is disclosed for recovering tungsten from tungsten bearing material containing arsenic. The process involves adjusting a water slurry of the material to a pH of less than about 4 with an acid to solubilize the major portion of the tungsten, adding an insoluble ferric compound to the slurry to form a two phase system in which the solid phase contains the major portion of the arsenic and of any phosphorus which may be present, and a solution phase containing the major portion of the tungsten. After separation of the solid from the solution, the solution is adjusted to a pH of less than about 2 with an acid and a suffficient amount of hexamethylenetetramine is added to the solution to precipitate the major portion of the tungsten, followed by separating the precipitate from the resulting liquor. The solid phase containing the arsenic and phosphorus, if any, can be contacted with water and a soluble ferric salt to produce a treated solid which passes the EP toxicity test.
摘要:
In a process for producing ammonium metatungstate from ammonium paratungstate, ammonium paratungstate is introduced in the anode chamber of an electrolytic cell which is separated from the cathode chamber by an inert liquid permeable media, when a direct electric current is passed through the cell, ammonium ions migrate to the cathode compartment resulting in an increased concentration of metatungstate in the anode chamber.
摘要:
A method for converting cobalt to cobalt powder is disclosed which comprises heating a starting mixture of cobalt and zinc in a non-reacting atomosphere at a first temperature of below the boiling point of zinc up to about 900.degree. C. in a non-reacting atmosphere for a length of time sufficient to cause the alloying of a portion of the zinc and cobalt, with the weight ratio of zinc to cobalt being less than about 10. The temperature of the resulting partially alloyed mixture is slowly raised to a second temperature of from about 900.degree. C. to about 960.degree. and is maintained for a time sufficient only to form a reaction product in which essentially all of the cobalt is alloyed with zinc and to keep the evaporation of zinc to a minimum. The reaction product is then heated at a pressure below atmospheric pressure at a third temperature of no greater than about 950.degree. C. for a time sufficient to evaporate essentially all of the zinc and produce a cobalt ingot which is pulverizable when cooled to room temperature.
摘要:
A process is disclosed for recovering tungsten, iron, and manganese from tungsten bearing material. The process involves digesting the material in a sufficient amount of sulfuric acid at a temperature of at least about 80.degree. C. for a sufficient time in the presence of coal as a reducing agent to form a digestion solution containing the major portion of the scandium, iron, and manganese and a digestion residue containing the major portion of the tungsten, followed by separating the solution from the residue. The major portion of the scandium can be extracted from the digestion solution with an organic solution consisting essentially of a mixture of tertiary alkyl primary amines which are present in an amount sufficient to extract the major portion of the scandium, and the balance an essentially aromatic solvent. The scandium is stripped from the organic with hydrochloric acid which is then separated from the stripped organic. The extraction can be accomplished by an organic solution consisting essentially of an extracting agent which is a dialkyl phosphoric acid and an essentially aromatic solvent. In this latter case, the stripping agent for the scandium is an aqueous solution of ammonium carbonate.
摘要:
A method is disclosed for recovering tungsten from a relatively dilute ammoniacal tungsten solution. The method involves adding hexamethylenetetramine to the tungsten solution in an amount sufficient to form a hexamethylenetetramine complex then adjusting the pH to from about 1.0 to about 2.0 with a mineral acid to form a precipitate of the complex containing at least about 99% of the tungsten, and separating the precipitate from the resulting mother liquor.
摘要:
A process is disclosed for recovering molybdenum from molybdenum disulfide. The process involves forming a slurry of the molybdenum disulfide in a solution of an alkali metal hydroxide, the amount of hydroxide being sufficient to react with at least a portion of the molybdenum disulfide to form an alkali metal molybdate and an alkali sulfate, heating the slurry in an oxidizing atmosphere at an elevated temperature and pressure and for a sufficient time to effect the conversion to the molybdate, and separating the pregnant liquor containing the molybdate from any residue. To the pregnant liquor is then added a sufficient amount of a hexamine to form a hexamine-molybdenum compound containing the major portion of the molybdenum, followed by adjusting the pH to from about 1.5 to about 3.8 to precipitate the major portion of the hexamine-molybdenum compound, and separating the compound from the resulting mother liquor.
摘要:
A fine cobalt metal powder is produced from pieces of relatively pure cobalt by dissolving the cobalt pieces in an aqueous solution of hydrogen iodide and iodine and forming a cobalt containing solid which is subsequently reduced to a fine cobalt metal powder.
摘要:
A process suitable for recovering refractory metal carbide values from contaminated uncemented refractory metal carbides containing an iron group metal comprises heating an admixture of the powders of the contaminated refractory metal carbides and glacial acetic acid to the boiling point of the admixture for at least about 30 minutes, the weight of the powders divided by the weight of the acid is less than 5, thereafter removing the resulting carbide solids from the acid and washing the solids with sufficient water to remove the residual acid and drying the solids.