1.
公开(公告)号:US20210364384A1
公开(公告)日:2021-11-25
申请号:US17056975
申请日:2019-05-22
申请人: CORNING INCORPORATED
发明人: Petr Gorelchenko , Raymond Miller Karam , Jonathan David Pesansky , Michael David Shorkey , Ming Ying
摘要: In a first aspect, a testing assembly for conducting reliability tests on liquid lenses includes a liquid lens, and a test frame arranged to receive the liquid lens. The liquid lens includes a lens body defining a cavity, a first liquid disposed within the cavity, and a second liquid disposed within the cavity that is substantially immiscible with the first liquid such that an interface between the first liquid and the second liquid forms a lens. The test frame includes a front wall, and a back wall oriented substantially parallel to the front wall. The liquid lens mounts to at least one of the front wall or the back wall and the test frame simulates a smart device incorporating a liquid lens.
-
公开(公告)号:US11084756B2
公开(公告)日:2021-08-10
申请号:US16830889
申请日:2020-03-26
申请人: CORNING INCORPORATED
发明人: Jaymin Amin , Benedict Osobomen Egboiyi , Jonathan David Pesansky , Kevin Barry Reiman , Rostislav Vatchev Roussev , Brian Paul Strines
摘要: Chemically strengthened glass articles having at least one deep compressive layer extending from a surface of the article to a depth of compression DOC of at least about 125 μm within the glass article. The compressive stress profile includes a single linear segment or portion extending from the surface to the depth of compression DOC. Alternatively, the compressive stress profile may include an additional portion extending from the surface to a relatively shallow depth and the linear portion extending from the shallow depth to the depth of compression.
-
公开(公告)号:US10556825B2
公开(公告)日:2020-02-11
申请号:US15416205
申请日:2017-01-26
申请人: CORNING INCORPORATED
发明人: Jaymin Amin , Benedict Osobomen Egboiyi , Pascale Oram , Jonathan David Pesansky , Kevin Barry Reiman , Rostislav Vatchev Roussev , Vitor Marino Schneider , Brian Paul Strines
IPC分类号: C03C21/00 , C03C3/097 , C03C3/087 , C03C3/091 , C03C3/093 , C03C3/095 , C03C4/18 , C03C3/04 , C03C3/085 , G06F1/16 , H04B1/3827
摘要: Chemically strengthened glass articles having at least one deep compressive layer extending from a surface of the article to a depth of layer DOL of about 130 μm up to about 175 μm or, alternatively, to a depth of compression (DOC) in a range from about 90 μm to about 120 μm within the article. The compressive layer has a stress profile that includes a first substantially linear portion extending from a relatively shallow depth to the DOL or DOC and a second portion extending from the surface to the shallow depth. The second portion is substantially linear at a depth from 0 μm to 5 μm and has a steeper slope than that of the first portion of the profile. Methods of achieving such stress profiles are also described.
-
公开(公告)号:US09908810B2
公开(公告)日:2018-03-06
申请号:US15332559
申请日:2016-10-24
申请人: CORNING INCORPORATED
发明人: Jaymin Amin , Benedict Osobomen Egboiyi , Jonathan David Pesansky , Kevin Barry Reiman , Rostislav Vatchev Roussev , Brian Paul Strines
IPC分类号: C03C3/097 , C03C4/18 , C03C21/00 , C03C3/091 , C03C3/093 , C03C3/095 , C03C3/087 , C03C3/04 , C03C3/085 , G06F1/16 , H04B1/3827
CPC分类号: C03C21/002 , C03C3/04 , C03C3/085 , C03C3/087 , C03C3/091 , C03C3/093 , C03C3/095 , C03C3/097 , C03C4/18 , C03C21/00 , C03C2204/00 , G06F1/1637 , G06F2200/1634 , H04B1/3827 , Y10T428/315
摘要: Chemically strengthened glass articles having at least one deep compressive layer extending from a surface of the article to a depth of at least about 45 μm within the article are provided. In one embodiment, the compressive stress profile includes a single linear segment extending from the surface to the depth of compression DOC. Alternatively, the compressive stress profile includes two linear portions: the first portion extending from the surface to a relatively shallow depth and having a steep slope; and a second portion extending from the shallow depth to the depth of compression. The strengthened glass has a 60% survival rate when dropped from a height of 80 cm in an inverted ball drop test and an equibiaxial flexural strength of at least 10 kgf as determined by abraded ring-on-ring testing. Methods of achieving such stress profiles are also described.
-
公开(公告)号:US20170129803A1
公开(公告)日:2017-05-11
申请号:US15416205
申请日:2017-01-26
申请人: CORNING INCORPORATED
发明人: Jaymin Amin , Benedict Osobomen Egboiyi , Pascale Oram , Jonathan David Pesansky , Kevin Barry Reiman , Rostilav Vatchev Roussev , Vitor Marino Schneider , Brian Paul Strines
CPC分类号: C03C21/002 , C03C3/04 , C03C3/085 , C03C3/087 , C03C3/091 , C03C3/093 , C03C3/095 , C03C3/097 , C03C4/18 , C03C21/00 , C03C2204/00 , G06F1/1637 , G06F2200/1634 , H04B1/3827 , Y10T428/315
摘要: Chemically strengthened glass articles having at least one deep compressive layer extending from a surface of the article to a depth of layer DOL of about 130 μm up to about 175 μm or, alternatively, to a depth of compression (DOC) in a range from about 90 μm to about 120 μm within the article. The compressive layer has a stress profile that includes a first substantially linear portion extending from a relatively shallow depth to the DOL or DOC and a second portion extending from the surface to the shallow depth. The second portion is substantially linear at a depth from 0 μm to 5 μm and has a steeper slope than that of the first portion of the profile. Methods of achieving such stress profiles are also described.
-
公开(公告)号:US09517968B2
公开(公告)日:2016-12-13
申请号:US14530155
申请日:2014-10-31
申请人: Corning Incorporated
发明人: Jaymin Amin , Benedict Osobomen Egboiyi , Jonathan David Pesansky , Kevin Barry Reiman , Rostislav Vatchev Roussev , Brian Paul Strines
CPC分类号: C03C21/002 , C03C3/04 , C03C3/085 , C03C3/087 , C03C3/091 , C03C3/093 , C03C3/095 , C03C3/097 , C03C4/18 , C03C21/00 , C03C2204/00 , G06F1/1637 , G06F2200/1634 , H04B1/3827 , Y10T428/315
摘要: Chemically strengthened glass articles having at least one deep compressive layer extending from a surface of the article to a depth of at least about 45 μm within the article are provided. In one embodiment, the compressive stress profile includes a single linear segment extending from the surface to the depth of compression DOC. Alternatively, the compressive stress profile includes two linear portions: the first portion extending from the surface to a relatively shallow depth and having a steep slope; and a second portion extending from the shallow depth to the depth of compression. The strengthened glass has a 60% survival rate when dropped from a height of 80 cm in an inverted ball drop test and an equibiaxial flexural strength of at least 10 kgf as determined by abraded ring-on-ring testing. Methods of achieving such stress profiles are also described.
摘要翻译: 提供了具有从制品表面延伸到制品内至少约45μm深度的至少一个深度压缩层的化学强化的玻璃制品。 在一个实施例中,压缩应力分布包括从表面延伸到压缩DOC深度的单个线性段。 或者,压缩应力分布包括两个线性部分:第一部分从表面延伸到相对较浅的深度并且具有陡峭的斜率; 以及从浅深度延伸到压缩深度的第二部分。 加强玻璃在倒置球滴试验中从80厘米的高度下降至60厘米的存活率,并且通过磨损的环上环试验确定的至少10kgf的等轴弯曲强度。 还描述了实现这种应力分布的方法。
-
公开(公告)号:US20160264452A1
公开(公告)日:2016-09-15
申请号:US15158230
申请日:2016-05-18
申请人: CORNING INCORPORATED
发明人: Jaymin Amin , Benedict Osobomen Egboiyi , Jonathan David Pesansky , Kevin Barry Reiman , Rostislav Vatchev Roussev , Brian Paul Strines
CPC分类号: C03C21/002 , C03C3/04 , C03C3/085 , C03C3/087 , C03C3/091 , C03C3/093 , C03C3/095 , C03C3/097 , C03C4/18 , C03C21/00 , C03C2204/00 , G06F1/1637 , G06F2200/1634 , H04B1/3827 , Y10T428/315
摘要: Chemically strengthened glass articles having at least one deep compressive layer extending from a surface of the article to a depth of at least about 45 μm within the article are provided. In one embodiment, the compressive stress profile includes a single linear segment extending from the surface to the depth of compression DOC. Alternatively, the compressive stress profile includes two linear portions: the first portion extending from the surface to a relatively shallow depth and having a steep slope; and a second portion extending from the shallow depth to the depth of compression. The strengthened glass has a 60% survival rate when dropped from a height of 80 cm in an inverted ball drop test and an equibiaxial flexural strength of at least 10 kgf as determined by abraded ring-on-ring testing. Methods of achieving such stress profiles are also described.
-
8.
公开(公告)号:US11852560B2
公开(公告)日:2023-12-26
申请号:US17056975
申请日:2019-05-22
申请人: CORNING INCORPORATED
发明人: Petr Gorelchenko , Raymond Miller Karam , Jonathan David Pesansky , Michael David Shorkey , Ming Ying
摘要: In a first aspect, a testing assembly for conducting reliability tests on liquid lenses includes a liquid lens, and a test frame arranged to receive the liquid lens. The liquid lens includes a lens body defining a cavity, a first liquid disposed within the cavity, and a second liquid disposed within the cavity that is substantially immiscible with the first liquid such that an interface between the first liquid and the second liquid forms a lens. The test frame includes a front wall, and a back wall oriented substantially parallel to the front wall. The liquid lens mounts to at least one of the front wall or the back wall and the test frame simulates a smart device incorporating a liquid lens.
-
公开(公告)号:US11634359B2
公开(公告)日:2023-04-25
申请号:US16165312
申请日:2018-10-19
申请人: CORNING INCORPORATED
发明人: Jaymin Amin , Benedict Osobomen Egboiyi , Jonathan David Pesansky , Kevin Barry Reiman , Rostislav Vatchev Roussev , Brian Paul Strines
IPC分类号: C03C3/04 , C03C4/18 , C03C21/00 , C03C3/097 , C03C3/087 , C03C3/091 , C03C3/093 , C03C3/095 , C03C3/085 , G06F1/16 , H04B1/3827
摘要: Chemically strengthened glass articles having at least one deep compressive layer extending from a surface of the article to a depth of at least about 45 μm within the article are provided. In one embodiment, the compressive stress profile includes a single linear segment extending from the surface to the depth of compression DOC. Alternatively, the compressive stress profile includes two linear portions: the first portion extending from the surface to a relatively shallow depth and having a steep slope; and a second portion extending from the shallow depth to the depth of compression. The strengthened glass has a 60% survival rate when dropped from a height of 80 cm in an inverted ball drop test and a peak load at failure of at least 10 kgf as determined by abraded ring-on-ring testing. Methods of achieving such stress profiles are also described.
-
公开(公告)号:US20190071350A1
公开(公告)日:2019-03-07
申请号:US16182004
申请日:2018-11-06
申请人: CORNING INCORPORATED
发明人: Jaymin Amin , Benedict Osobomen Egboiyi , Jonathan David Pesansky , Kevin Barry Reiman , Rostislav Vatchev Roussev , Brian Paul Strines
摘要: Chemically strengthened glass articles having at least one deep compressive layer extending from a surface of the article to a depth of compression DOC of at least about 125 μm within the glass article. The compressive stress profile includes a single linear segment or portion extending from the surface to the depth of compression DOC. Alternatively, the compressive stress profile may include an additional portion extending from the surface to a relatively shallow depth and the linear portion extending from the shallow depth to the depth of compression.
-
-
-
-
-
-
-
-
-