Abstract:
An optical film having high anti-glare properties and favorable fingerprints wiping off properties is provided. The optical film has a first surface, and a second surface which is a surface opposite to the first surface, wherein the optical film comprises an anti-reflection layer and an anti-glare layer in this order from the first surface to the second surface, the first surface has a profile of depressions and projections, the first surface has an arithmetic mean height Sa of 0.05 μm or more specified in ISO 25178-2:2012, and the first surface satisfies the relation represented by the following Expression 1: Sw×Vmp≤2.00 (Expression 1) wherein “Sw” represents a tilt angle (degrees) of 30 μl pure water droplet flowing down on the first surface; and “Vmp” represents a value of a peak material volume (ml/m2) of the first surface specified in ISO 25178-2:2012.
Abstract:
Provided is an anti-glare film excellent in anti-glare properties and capable of suppressing reflected scattered light. An anti-glare film including an anti-glare layer, the anti-glare film having an uneven surface, wherein for amplitude spectrum of elevation of the uneven surface, when a sum of amplitudes corresponding to spatial frequencies of 0.005 μm−1, 0.010 μm−1, and 0.015 μm−1 is defined as AM1 and an amplitude at a spatial frequency of 0.300 μm−1 is defined as AM2, AM1 is 0.070 μm or more and 0.400 μm or less, AM2 is 0.0050 μm or more, and AM2
Abstract:
Provided is an optical film which has high anti-glare properties, enables a suppress of a reduction in jet-black appearance by reflected scattered light, and has favorable scratch resistance. An optical film having a surface with depressions and projections, wherein the surface with depressions and projections has a peak material volume Vmp of 0.010 ml/m2 or more and 0.050 ml/m2 or less specified in ISO 25178-2:2012, and a minimum autocorrelation length Sal of 4.0 μm or more and 12.0 μm or less specified in ISO 25178-2:2012.
Abstract:
Provided is an anti-glare film excellent in anti-glare properties and scratch resistance and capable of suppressing reflected scattered light. An anti-glare film including an anti-glare layer, the anti-glare film having an uneven surface, wherein for an amplitude spectrum of elevation of the uneven surface, when a sum of amplitudes corresponding to spatial frequencies of 0.005 μm−1, 0.010 μm−1, and 0.015 μm−1 is defined as AM1 and an amplitude at a spatial frequency of 0.300 μm−1 is defined as AM2, AM1 is more than 0.4000 μm and 1.0000 μm or less, and AM2 is 0.0050 μm or more and 0.0500 μm or less.
Abstract:
An optical film having high anti-glare properties and favorable fingerprints wiping off properties is provided. The optical film has a first surface, and a second surface which is a surface opposite to the first surface, wherein the optical film comprises an anti-reflection layer and an anti-glare layer in this order from the first surface to the second surface, the first surface has a profile of depressions and projections, the first surface has an arithmetic mean height Sa of 0.05 μm or more specified in ISO 25178-2:2012, and the first surface satisfies the relation represented by the following Expression 1: Sw×Vmp≤2.00 (Expression 1) wherein “Sw” represents a tilt angle (degrees) of 30 μl pure water droplet flowing down on the first surface; and “Vmp” represents a value of a peak material volume (ml/m2) of the first surface specified in ISO 25178-2:2012.
Abstract:
Provided is an anti-glare film excellent in anti-glare properties and capable of suppressing reflected scattered light. An anti-glare film including an anti-glare layer, the anti-glare film having an uneven surface, wherein for amplitude spectrum of elevation of the uneven surface, when a sum of amplitudes corresponding to spatial frequencies of 0.005 μm−1, 0.010 μm−1, and 0.015 μm−1 is defined as AM1 and an amplitude at a spatial frequency of 0.300 μm−1 is defined as AM2, AM1 is 0.070 μm or more and 0.400 μm or less, AM2 is 0.0050 μm or more, and AM2
Abstract:
A touch panel capable of imparting a variety of characteristics such as anti-glare properties and preventing the scintillation of image light in ultrahigh-definition display elements having a pixel density of 300 ppi or more is provided.The touch panel includes an optical sheet as a component, in which the optical sheet has an uneven shape on a surface, the uneven shape satisfies at least one condition selected from the following (A) to (C), and the touch panel is used for a front surface of a display element having a pixel density of 300 ppi or more, Condition (A); a gap between inclination angles indicating a half value of a peak value of an inclination angle distribution curve of the uneven shape is in a range of 5 degrees to 15 degrees, Condition (B); an inclination angle indicating an inflection point on a positive direction side of the inclination angle indicating the peak value of the inclination angle distribution curve of the uneven shape is in a range of 4 degrees to 15 degrees, and a difference between the inclination angle indicating the inflection point on the positive direction side and the inclination angle indicating the peak value of the inclination angle distribution curve is in a range of 2.2 degrees to 10 degrees, and Condition (C); the inclination angle indicating the peak value of the inclination angle distribution curve of the uneven shape is in a range of 2 degrees to 8 degrees, skewness of the inclination angle distribution curve of the uneven shape is in a range of 0 degrees to 1.5 degrees, and/or kurtosis of the inclination angle distribution curve of the uneven shape is in a range of 1.5 to 6.
Abstract:
An optical film having high anti-glare properties and favorable fingerprints wiping off properties is provided. The optical film has a first surface, and a second surface which is a surface opposite to the first surface, wherein the optical film comprises an anti-reflection layer and an anti-glare layer in this order from the first surface to the second surface, the first surface has a profile of depressions and projections, the first surface has an arithmetic mean height Sa of 0.05 μm or more specified in ISO 25178-2:2012, and the first surface satisfies the relation represented by the following Expression 1: Sw×Vmp≤2.00 (Expression 1) wherein “Sw” represents a tilt angle (degrees) of 30 μl pure water droplet flowing down on the first surface; and “Vmp” represents a value of a peak material volume (ml/m2) of the first surface specified in ISO 25178-2:2012.
Abstract:
Provided is an optical film which has high anti-glare properties and high scratch resistance and enables a suppression in reflected scattered light. An optical film having a surface with depressions and projections, wherein the surface with depressions and projections has a developed interfacial area ratio Sdr of 0.010 or more and 0.060 or less specified in ISO 25178-2:2012, and a minimum autocorrelation length Sa1 of 4.0 μm or more and 12.0 μm or less specified in ISO 25178-2:2012.
Abstract:
Provided is an optical film which has high anti-glare properties, enables a suppress of a reduction in jet-black appearance by reflected scattered light, and has favorable scratch resistance. An optical film having a surface with depressions and projections, wherein the surface with depressions and projections has a reduced peak height Spk of 0.20 μm or more and 1.00 μm or less specified in ISO 25178-2:2012, and a minimum autocorrelation length Sal of 4.0 μm or more and 12.0 μm or less specified in ISO 25178.