A POLYOLEFIN BLEND COMPOSITION AND ARTICLES MADE THEREFROM
    1.
    发明申请
    A POLYOLEFIN BLEND COMPOSITION AND ARTICLES MADE THEREFROM 有权
    POLYOLEFIN混合组合物及其制品

    公开(公告)号:US20160083571A1

    公开(公告)日:2016-03-24

    申请号:US14391318

    申请日:2013-04-02

    Abstract: The instant invention provides a polyolefin blend composition, process for producing the same, and articles made therefrom. The polyolefin blend composition according to the present invention comprises: (a) from 75 to 97 percent by weight of one or more random propylene copolymers having a DSC melting point in the range of from 120° C. to 160° C., and a melt flow rate (MFR) in the range of from 1 to 120 g/10 minutes; (b) from 3 to 25 percent by weight of one or more ethylene ?-olefin copolymers having a melt index (I2) in the range of from 100 to 1500 g/10 minutes, a density in the range of 0.860 to 0.910 g/cm3, and a molecular weight (Mw) in the range of from 10,000 to 50,000 g/mole, wherein said ethylene ?-olefin copolymer is homogenously branched copolymer, and wherein said ethylene ?-olefin copolymer is linear or substantially linear; (c) optionally from 5 to 15 percent by weight of one or more propylene ?-olefin interpolymers having a DSC melting point in the range of less than 110° C., a heat of fusion in the range of less than 50 Joules/gram, and a crystallinity in the range of from at least 1 percent by to 40 percent by weight, and a melt flow rate in the range of less than 80 g/10 minutes.

    Abstract translation: 本发明提供了一种聚烯烃共混组合物,其制备方法和由其制成的制品。 根据本发明的聚烯烃共混物组合物包含:(a)75至97重量%的一种或多种DSC熔点在120℃至160℃范围内的无规丙烯共聚物,和 熔体流动速率(MFR)在1至120g / 10分钟的范围内; (b)3至25重量%的一种或多种熔体指数(I 2)在100至1500g / 10分钟范围内的乙烯α-烯烃共聚物,密度在0.860至0.910g / cm 3,分子量(Mw)在10,000〜50,000g / mol范围内,其中所述乙烯α-烯烃共聚物是均匀支化的共聚物,并且其中所述乙烯α-烯烃共聚物是线性或基本上线性的; (c)任选的5至15重量%的一种或多种DSC熔点在小于110℃范围内的丙烯α-烯烃互聚物,熔融热在小于50焦耳/克 ,结晶度在至少1重量%至40重量%的范围内,熔体流动速率在小于80克/ 10分钟的范围内。

    Polyolefin blend composition and articles made therefrom

    公开(公告)号:US09982122B2

    公开(公告)日:2018-05-29

    申请号:US14391318

    申请日:2013-04-02

    Abstract: The instant invention provides a polyolefin blend composition, process for producing the same, and articles made therefrom. The polyolefin blend composition according to the present invention comprises: (a) from 75 to 97 percent by weight of one or more random propylene copolymers having a DSC melting point in the range of from 120° C. to 160° C., and a melt flow rate (MFR) in the range of from 1 to 120 g/10 minutes; (b) from 3 to 25 percent by weight of one or more ethylene ?-olefin copolymers having a melt index (I2) in the range of from 100 to 1500 g/10 minutes, a density in the range of 0.860 to 0.910 g/cm3, and a molecular weight (Mw) in the range of from 10,000 to 50,000 g/mole, wherein said ethylene ?-olefin copolymer is homogenously branched copolymer, and wherein said ethylene ?-olefin copolymer is linear or substantially linear; (c) optionally from 5 to 15 percent by weight of one or more propylene ?-olefin interpolymers having a DSC melting point in the range of less than 110° C., a heat of fusion in the range of less than 50 Joules/gram, and a crystallinity in the range of from at least 1 percent by to 40 percent by weight, and a melt flow rate in the range of less than 80 g/10 minutes.