Abstract:
A composition comprising an ethylene/alpha-olefin/non-conjugated polyene, and wherein the ethylene/alpha-olefin/non-conjugated polyene comprises the following property: a “13C NMR % iCB Peak Area,” which is the {[(13C NMR peak area from 34.4 ppm to 34.6 ppm) divided by (the 13C NMR sum integral area from 160.0 to 100.0 and from 60.0 ppm to 0.00 ppm)]×100}, that is >0.010%, as determined by 13C NMR.
Abstract:
A composition comprises (A) an ethylene/alpha-olefin/diene interpolymer; (B) a peroxide comprising at least one peroxide bond; and (C) a bis-TEMPO compound having the Structure (I), wherein R1-4 are each independently H or a C1-C6 alkyl group; X is S, O, N, P, Se, a carbonyl group, a carboxyl group, an amide group, an azo group, an imino group, a carbamate group, a peroxy group, a phosphono group, a phosphate group, a sulfonyl group, a sulfinyl group, a sulfonate ester group, a sulfonate ester group, or combinations thereof; Y is a substitute or unsubstituted aliphatic alkyl group or aromatic alkyl group, a heterocyclic group, a siloxane group, an ethylene glycol group, an imide group, or combinations thereof; and n is greater than 1. The ratio of the molar amount of nitroxide groups of component (C) to the molar amount of the peroxide bonds of component (B) is from 0.100:1.000 to 2.000:1.000.
Abstract:
A composition comprising from 10 wt % to 90 wt % of an ethylene component including at least one ethylene based polymer having an ethylene content of at least 50.0 wt %, a melt index from 0.1 g/10 min to 100.0 g/10 min, and a density from 0.935 g/cm3 to 0.965 g/cm3; from 10 wt % to 90 wt % of a propylene component including at least one propylene based polymer having a propylene content of at least 50.0 wt % and a melt flow rate from 0.5 g/10 min to 200.0 g/10 min; and from 1 wt % to 20 wt % of a composite component including a specified block composite, derived from at least ethylene and an alpha-olefin.
Abstract:
The invention provides a composition comprising the following components: A) an anhydride and/or carboxylic acid functionalized ethylene/alpha-olefin interpolymer having the following properties: i) a melt viscosity (177 C) less than, or equal to, 50,000 cP, ii) a density from 0.855 to 0.900 g/cc; B) a tackifier selected from the following: a) a hydrocarbon tackifier that has a cloud point (DACP) temperature greater than, or equal to, 20 C, b) a rosin ester tackifier with an acid number of less than 25, c) a terpene tackifier, or d) a combination thereof.
Abstract:
The invention provides a solution polymerization process to form an ethylene/α-olefin/nonconjugated polyene interpolymer, said process comprising polymerizing ethylene, an α-olefin, and a nonconjugated polyene in at least one reactor in the presence of a catalyst selected from Formula I, as described herein; and wherein the polymerization is conducted in a continuous process; and wherein the interpolymer has a rheology ratio (V0.1/V100 at 19° C.) greater than, or equal to, 20.
Abstract:
A composition is composed of (A) an ethylene/alpha-olefin/diene TEMPO compound having the Structure (I) and (D) a peroxide. The molar ratio of isocyanate groups of Component (B) to the functional groups of Component (C) is from 0.80 to 1.10. A composition is composed of (A) an ethylene/alpha-olefin/diene interpolymer; a second composition comprising a reaction mixture comprising (B) an isocyanate comprising at least two isocyanate groups and (C) a TEMPO compound having the Structure (I) and (D) a peroxide, wherein the molar ratio of isocyanate groups of Component (B) to the functional groups of Component (C) is from 0.80 to 1.10. In Structure I, R1, R2, R3 and R4 are each independently selected from H and C1-C6 alkyl groups and X is a functional group selected from OH and NH2.
Abstract:
The present disclosure provides a plastic living hinge. The plastic living hinge includes a blend containing (A) an ethylene-based polymer; (B) a propylene-based polymer; and (C) a composite component selected from the group consisting of a block composite, a crystalline block composite, and a combination thereof.
Abstract:
The present disclosure provides a primer composition. In an embodiment, the primer composition includes a functionalized polyolefin, a functionalized styrenic block copolymer containing greater than or equal to 20 wt % polymerized styrene, a solvent composition and an isocyanate component. The primer composition is suitable for use as an adhesive layer between a substrate and a polyolefin layer.
Abstract:
A composition comprising from 10 wt % to 90 wt % of an ethylene component including at least one ethylene based polymer having an ethylene content of at least 50.0 wt %, a melt index from 0.1 g/10 min to 100.0 g/10 min, and a density from 0.935 g/cm3 to 0.965 g/cm3; from 10 wt % to 90 wt % of a propylene component including at least one propylene based polymer having a propylene content of at least 50.0 wt % and a melt flow rate from 0.5 g/10 min to 200.0 g/10 min; and from 1 wt % to 20 wt % of a composite component including a specified block composite, derived from at least ethylene and an alpha-olefin.
Abstract:
The invention provides a composition comprising a first composition that comprises at least one ethylene/alpha-olefin/nonconjugated polyene interpolymer; and wherein the first composition has a Mooney Viscosity (ML1+4, 125C) greater than, or equal to, 10, and wherein the first composition has a “13C NMR % Peak Area,” which is the {[(13C NMR peak area from 21.3 ppm to 21.8 ppm) divided by the (total integral area from 19.5 ppm to 22.0 ppm)]×100}, that is greater than 3.5 percent, as determined by 13C NMR.