公开(公告)号:US20250135256A1
公开(公告)日:2025-05-01
申请号:US18837169
申请日:2023-02-10
Applicant: Drexel University , MURATA MANUFACTURING CO., LTD.
Inventor: Michel W BARSOUM , Hussein O. BADR , Kaho KOTANI , Yuki KIMURA , Akimaro YANAGIMACHI , Takeshi TORITA
IPC: A62D3/17 , A62D101/20
Abstract: Provided is a method, comprising contacting a composition that comprises metal oxide nanofilaments to a dye and/or an organic compound under such conditions that the dye and/or the organic compound undergoes at least partial decomposition or degradation, the metal oxide nanofilaments the metal oxide nanofilaments optionally comprising titanium, the metal oxide nanofilaments optionally comprising carbon, the structure of the oxide nanofilaments optionally being an lepidocrocite structure; and further optionally comprising illuminating the composition and the dye and/or the organic compound. Also provided is a system, the system comprising a conduit and an amount of a composition that comprises a metal oxide nanofilaments, the conduit placing the composition into fluid communication with a process stream, the process stream comprising a dye and/or an organic compound.
-
公开(公告)号:US20250091029A1
公开(公告)日:2025-03-20
申请号:US18832624
申请日:2023-02-10
Applicant: DREXEL UNIVERSITY
Inventor: Michel W. BARSOUM , Hussein O. BADR , Joshua SNYDER
Abstract: A method, comprising: to an initial sample that has an initial concentration of urea in solution, contacting a composition comprising metal oxide nanofilaments under such conditions that at least some of the urea adsorbs to the metal oxide nanofilaments so as to give rise to a final concentration of urea in the solution A device for removing urea from an initial aqueous solution of urea, the device comprising an exchangeable cartridge of metal oxide nanofilaments composition through which the initial aqueous solution is directed to pass, the passage adapted to allow the initial aqueous urea solution to contact the metal oxide nanofilaments contained in the cartridge. Contacting a composition comprising metal oxide-based nanofilaments to an initial sample that comprises a metal ion and/or a metal under such conditions that at least some of the metal ion and/or the metal associates with the metal oxide nanofilaments.
-
公开(公告)号:US20240274831A1
公开(公告)日:2024-08-15
申请号:US18568358
申请日:2022-06-10
Applicant: DREXEL UNIVERSITY
Inventor: Rahul Nagesh PAI , Vibha KALRA , Michel W. BARSOUM , Hussein O. BADR
IPC: H01M4/62 , H01M4/02 , H01M4/13 , H01M10/052
CPC classification number: H01M4/628 , H01M4/13 , H01M4/623 , H01M10/052 , H01M2004/028
Abstract: By combining two-dimensional (2D) transition metal oxide and/or carbo-oxides with sulfur, one can form cathodes for use in Li—S batteries, which batteries in turn exhibit high capacity and other attractive characteristics. Accordingly, provided herein are methods, comprising: forming an admixture that comprises sulfur, a 2D transition metal carbo-oxide, and optionally a conductive material. Also provided are electrodes, comprising sulfur, a 2D transition metal carbo-oxide, and optionally a conductive material. Further provided are energy cells, the energy cell comprising a first electrode according to the present disclosure. Additionally provided are methods, the methods comprising discharging an energy cell according to the present disclosure or charging an energy cell according to the present disclosure. Also provided are electrical devices, comprising an energy cell according to the present disclosure.
-
-