Method of Producing Polyurethane Dispersion by Solvent Free Process

    公开(公告)号:US20180265619A1

    公开(公告)日:2018-09-20

    申请号:US15460323

    申请日:2017-03-16

    摘要: A method of producing PUD by a solvent free process includes drying polyol in vacuum; placing the dried polyol and DMBA in a reaction vessel to mix until a first mixture becomes transparent; adding diisocyanate which having functional group of isocyanate(—NCO) to the first mixture to react until —NCO terminated first prepolymer is formed; decreasing temperature of the —NCO terminated first prepolymer to 65° C.; adding a neutralizing agent to the —NCO terminated first prepolymer until —NCO terminated second prepolymer is formed; adding the remaining diisocyanate having isocyanate functional group to the —NCO terminated second prepolymer to form a second mixture; adding deionized water to the second mixture to form prepolymer dispersion; and adding chain extension agent to the prepolymer dispersion to rotate at a range of 200 to 2,000 rpm for chain extension for 1-3 hours until solid content 40.0 wt. % solvent free PUD is produced.

    Method of producing polyurethane dispersion by solvent free process

    公开(公告)号:US10077329B1

    公开(公告)日:2018-09-18

    申请号:US15460323

    申请日:2017-03-16

    摘要: A method of producing PUD by a solvent free process includes drying polyol in vacuum; placing the dried polyol and DMBA in a reaction vessel to mix until a first mixture becomes transparent; adding diisocyanate which having functional group of isocyanate (—NCO) to the first mixture to react until —NCO terminated first prepolymer is formed; decreasing temperature of the —NCO terminated first prepolymer to 65° C.; adding a neutralizing agent to the —NCO terminated first prepolymer until —NCO terminated second prepolymer is formed; adding the remaining diisocyanate having isocyanate functional group to the —NCO terminated second prepolymer to form a second mixture; adding deionized water to the second mixture to form prepolymer dispersion; and adding chain extension agent to the prepolymer dispersion to rotate at a range of 200 to 2,000 rpm for chain extension for 1-3 hours until solid content 40.0 wt. % solvent free PUD is produced.

    Process of Applying Water-based Rubber Copolyer to Textile
    5.
    发明申请
    Process of Applying Water-based Rubber Copolyer to Textile 审中-公开
    将水性橡胶共聚物应用于纺织品的工艺

    公开(公告)号:US20120251732A1

    公开(公告)日:2012-10-04

    申请号:US13074075

    申请日:2011-03-29

    IPC分类号: B05D1/18

    摘要: A process of making a textile comprising dropping a predetermined amount of rubber copolymer in a reactor filled with a solvent including 90-100 wt % of toluene, 0-10 wt % of acetone, and 0-10 wt % of ethanol; adjusting conditions of the reactor to a predetermined range of temperature and a predetermined atmospheric pressure so as to reduce sizes of molecules of the rubber copolymer; adding water to the reactor to disperse the rubber copolymer in the solvent to make an aqueous solution with dispersing rubber copolymer; and penetrating the water-based rubber copolymer through fibers of the textile for permanently attaching thereto.

    摘要翻译: 一种制造纺织品的方法,包括在填充有包括90-100重量%甲苯,0-10重量%丙酮和0-10重量%乙醇的溶剂的反应器中滴加预定量的橡胶共聚物; 将反应器的条件调节到预定的温度范围和预定的大气压,以减小橡胶共聚物分子的尺寸; 向反应器中加入水以将橡胶共聚物分散在溶剂中以制备具有分散橡胶共聚物的水溶液; 并通过纺织品的纤维穿透水性橡胶共聚物以永久地附着在其上。