公开(公告)号:US20230235156A1
公开(公告)日:2023-07-27
申请号:US18007814
申请日:2021-06-04
Applicant: Dow Global Technologies LLC , PBBPolisur S.R.L.
Inventor: Alexander Williamson , Shadid Askar , Joel D. Wieliczko , Cornelis F.J. Den Doelder , Mridula Kapur , Kurt F. Hirsekorn , Evelyn Auyeung , Bo Liu , Maria C. Zandueta , John P. O'Brien , Stephanie M. Whited
CPC classification number: C08L23/0815 , C08L23/06 , C08L2205/025 , C08L2314/02
Abstract: Embodiments are directed towards polyolefin compositions including a high molecular weight polyolefin and a low molecular weight polyolefin.
-
公开(公告)号:US11685798B2
公开(公告)日:2023-06-27
申请号:US17260271
申请日:2019-07-18
Applicant: Dow Global Technologies LLC
Inventor: Peter S. Martin , Yijian Lin , Angela I. Padilla-Acevedo , Roger L. Kuhlman , Shadid Askar , Mridula Kapur , Todd A. Hogan , Joel D. Wieliczko , Chuan C. He
IPC: C08F210/16 , C08F10/02 , C08F4/6592
CPC classification number: C08F210/16 , C08F4/65922 , C08F2500/01 , C08F2500/02 , C08F2500/05 , C08F2500/07 , C08F2500/12 , C08F2500/13 , C08F2500/19
Abstract: In various embodiments, a polyethylene formulation has a density of greater than 0.940 g/cm3 when measured according to ASTM D792, and a high load melt index (I21) of 1.0 g/10 min to 10.0 g/10 min when measured according to ASTM D1238 at 190° C. and a 21.6 kg load. Moreover, the polyethylene formulation has a peak molecular weight (Mp(GPC)) of less than 50,000 g/mol, a number average molecular weight (Mn(GPC)) of less than 30,000 g/mol, and a weight fraction (w1) of molecular weight (MW) less than 10,000 g/mol of less than or equal to 10.5 wt %, as determined by Gel Permeation Chromatography (GPC). Articles made from the polyethylene formulation, such as articles made by blow molding processes are also provided.
-
公开(公告)号:US20210301049A1
公开(公告)日:2021-09-30
申请号:US17260271
申请日:2019-07-18
Applicant: Dow Global Technologies LLC
Inventor: Peter S. Martin , Yijian Lin , Angela I. Padilla-Acevedo , Roger L. Kuhlman , Shadid Askar , Mridula Kapur , Todd A. Hogan , Joel D. Wieliczko , Chuan C. He
IPC: C08F210/16 , C08F4/6592
Abstract: In various embodiments, a polyethylene formulation has a density of greater than 0.940 g/cm3 when measured according to ASTM D792, and a high load melt index (I21) of 1.0 g/10 min to 10.0 g/10 min when measured according to ASTM D1238 at 190° C. and a 21.6 kg load. Moreover, the polyethylene formulation has a peak molecular weight (Mp(GPC)) of less than 50,000 g/mol, a number average molecular weight (Mn(GPC)) of less than 30,000 g/mol, and a weight fraction (w1) of molecular weight (MW) less than 10,000 g/mol of less than or equal to 10.5 wt %, as determined by Gel Permeation Chromatography (GPC). Articles made from the polyethylene formulation, such as articles made by blow molding processes are also provided.
-
-