1.
公开(公告)号:US11655309B2
公开(公告)日:2023-05-23
申请号:US16348586
申请日:2017-11-09
发明人: Wenlai Feng , Haining An , Michael Eugene Donelson , Thomas Joseph Pecorini , Robert Ellis McCrary , Douglas Weldon Carico , Spencer Allen Gilliam
IPC分类号: C08B3/16 , C08K5/1515 , C08K5/526 , C08L1/10 , C08L1/14 , C08L1/12 , C08L1/02 , B29C45/00 , C08B3/06 , C08K5/00 , B29K1/00 , B29K105/00 , B29C45/78
CPC分类号: C08B3/16 , B29C45/0001 , C08B3/06 , C08K5/1515 , C08K5/526 , C08L1/02 , C08L1/10 , C08L1/12 , C08L1/14 , B29C45/78 , B29C2945/76498 , B29C2945/76531 , B29C2945/76561 , B29C2945/76668 , B29K2001/12 , B29K2105/0038 , B29K2995/0017 , B29K2995/0056 , C08K5/0016 , C08L2205/02 , C08L2205/06 , C08L1/14 , C08K5/107 , C08L1/14 , C08L25/08 , C08L1/14 , C08K5/107 , C08L25/08 , C08L1/14 , C08L75/04 , C08L1/14 , C08L25/08
摘要: A shaped article comprising a polymer-based resin derived from cellulose, wherein the polymer-based resin has an HDT of at least 95° C., a bio-derived content of at least 20 wt %, a notched izod impact strength of greater than 80 J/m and at least one of the following properties chosen from: flexural modulus of greater than 1900 MPa; a spiral flow length or at least 3.0 cm; a flex creep deflection of less than 12 mm; a transmission of at least 70%; a ΔE value of less than 25; or an L* color of at least 85.
-
2.
公开(公告)号:US10919984B2
公开(公告)日:2021-02-16
申请号:US16348550
申请日:2017-11-09
发明人: Wenlai Feng , Haining An , Michael Eugene Donelson , Thomas Joseph Pecorini , Robert Ellis McCrary , Douglas Weldon Carico , Spencer Allen Gilliam
IPC分类号: B32B7/02 , C08B3/16 , C08K5/1515 , C08K5/526 , C08L1/10 , C08L1/14 , C08L1/12 , C08L1/02 , B29C45/00 , C08B3/06 , C08K5/00 , B29K1/00 , B29K105/00
摘要: An injection molded article comprising a thin-walled body portion formed from a polymer-based resin derived from cellulose, wherein the thin-walled body portion comprises: i. a gate position; ii. a last fill position; iii. a flow length to wall thickness ratio greater than or equal to 100, wherein the flow length is measured from the gate position to the last fill position; and iv. a wall thickness less than or equal to about 2 mm; and wherein the polymer-based resin has an HDT or at least 95° C., a bio-derived content of at least 20 wt %, and a spiral flow length of at least 3.0 cm, when the polymer-based resin is molded with a spiral flow mold with the conditions of a barrel temperature of 238° C., a melt temperature of 246° C., a molding pressure of 13.8 MPa, a mold thickness of 0.8 mm, and a mold width of 12.7 mm.
-