摘要:
Thermoplastic block copolymers of the idealized formulae (I)A--B--A; B--A--B or (A--B).sub.x (I)in whichx=1 to 40,and whereinA is the radical of a homopolymer of styrene, vinylnaphthalene, butadiene and isoprene, andB the radical of a homopolymer of a cyclic polycarbonate or lactone,the average molecular weight of blocks A and B being greater than 800, and a process for the preparation of these blocks copolymers in several reaction stages.
摘要:
Process for the polymerization of cyclic aliphatic carbonates in the presence of aprotic organic solvents with exclusion of atmospheric oxygen and atmospheric moisture, wherein organometallic compounds of elements of main group 1 of the periodic table are used as initiators, the monomer/solvent ratio is in the range from 1 part by weight to 50 parts by weight of monomer per 100 parts by weight of solvent and the polymerization temperature is between -100.degree. C. and +20.degree. C.
摘要:
Multi-block copolymers of recurring structural units of polysiloxanes and recurring structural units of aliphatic polyesters, polyethers or polyetheresters with rubber properties, the individual polymeric blocks constituting rubber-type products with glass transition temperatures below practical usefulness and a process for their production.
摘要:
The invention relates to new block copolymers consisting of recurring polysiloxane blocks and recurring conjugated diene homo-or copolymer blocks with particularly good rubber properties, in particular at low temperatures.
摘要:
Block copolymers of recurring structural units of the series of polysiloxanes and recurring structural units of the series of aliphatic polyesters, polyethers or polyetheresters with rubber properties, the polymeric block-forming polymers in each case producing rubber-type products with glass transition temperatures below practical temperatures of use and a process for the production thereof.
摘要:
Thermoplastic moulding materials consisting of(1) 70 to 99.9% by weight of a cellulose ester or cellulose mixed ester(2) 0.1 to 30% by weight of a rubber polymer built up in the form of blocks from recurring structural units (I) with molecular weights of 10,000 to 1,000,000--A--B-- IwhereinA denotes bifunctional polysiloxane segements of the formula--(R.sup.1)(R.sup.2)SiO--.sub.x IIin whichR.sup.1 and R.sup.2 =aryl (in particular phenyl) or alkyl (in particular methyl) andx is a number such that the molecular weight is .gtoreq.500, andB denotes bifunctional aliphatic polyester and/or aliphatic polyester segments with molecular weights of .gtoreq.800,and the glass transition temperatures of the polymeric blocks A and B are less than 20.degree. C., which contains additionally(3) 0 to 30% by weight based on the mixture of (1) and (2) of a plasticizer.
摘要:
Crosslinked copolymers ofA) cyclic aliphatic esters andB) cyclic aliphatic carbonatesin which part of B contains crosslinking-active side groups,their production and their use for the production of films.
摘要:
Polymer dihydroxy compounds corresponding to the following formula ##STR1## in whichR.sup.1, R.sup.2, R.sup.3 =H or C.sub.1 -C.sub.4 alkyl,R.sup.4 =H or C.sub.1 -C.sub.4 alkyl,R.sup.5 =--C.sub.6 H.sub.5, --C.sub.6 H.sub.4 CH.sub.3, --CH.dbd.CH.sub.2, or --CO.sub.2 R.sup.7,R.sup.6 =C.sub.1 -C.sub.4 alkyl, aryl, or H,R.sup.7 =C.sub.1 -C.sub.4 alkyl,m=0 or 1,n=5 to 100,q=0 or 1,a process for their production and their use in thermoplastic molding compositions.
摘要翻译:对应于下式的化合物二羟基化合物,其中R1,R2,R3 = H或C1-C4烷基,R4 = H或C1-C4烷基,R5 = -C6H5,-C6H4CH3,-CH = CH2或 - CO 2 R 7,R 6 = C 1 -C 4烷基,芳基或H,R 7 = C 1 -C 4烷基,m = 0或1,n = 5〜100,q = 0或1,其制备方法及其在热塑性成型 组合物。
摘要:
A process for antifelt finishing of wool material composed of especially animal hairs by means of a low temperature plasma treatment, characterized in that moist wool material having a water content of 4 to 40% by weight is exposed, prior to further processing into textile fabrics or webs, to a high frequency discharge having a frequency of 1 kHz to 3 GHz and a discharge power density of 0.001 to 3 W/cm.sup.3 at a pressure of 10.sup.-2 to 10 mbar for a period of 1 to 600 sec in the presence or absence of non-polymerized gases.