公开(公告)号:US20150038624A1
公开(公告)日:2015-02-05
申请号:US14382812
申请日:2012-12-12
Applicant: Exxonmobil Chemical Patents Inc.
Inventor: Gerd A. Allermann , Danny Van Hoyweghen , Steven A. Best , Anthony Poloso , Nicolas M. De Ketelaere
IPC: C08J3/00 , C09D123/06 , C08J3/20
CPC classification number: C08J3/005 , C08F8/00 , C08F2810/10 , C08F2810/40 , C08J3/20 , C08J2323/06 , C09D123/06 , H01B3/441 , C08F8/50 , C08F8/06 , C08F210/16 , C08F210/14 , C08F2500/12
Abstract: Processes are disclosed for oxygen-tailoring polyethylene, particularly polyethylenes suitable for wire and cable applications. One process includes conveying a first polyethylene having a melt index ≦5.0 and an MWD ≦5.0 through mixing or extrusion apparatus having a feed zone, a melt-mixing zone downstream of the feed zone, and a melt zone downstream of the melt-mixing zone, wherein the temperature of the first polyethylene in the melt zone ranges from about 180° C. to about 300° C.; and contacting the first polyethylene with an amount of an oxygen-containing gas having at least about 20.0 parts by weight oxygen per million per parts by weight of the first polyethylene (ppm (wt) O2). Polyethylene compositions having improved properties, particularly for wire and cable applications are disclosed.
Abstract translation: 公开了用于氧气聚乙烯,特别是适用于电线和电缆应用的聚乙烯的方法。 一种方法包括通过具有进料区,进料区下游的熔融混合区和熔融区下游的熔融区的混合或挤出装置输送具有熔体指数为< E1和5.0 | MWD&NlE; 5.0的第一聚乙烯, 混合区,其中熔融区中第一聚乙烯的温度为约180℃至约300℃; 并且将第一聚乙烯与一定量的含氧气体接触,所述含氧气体具有至少约20.0重量份的氧每百万重量份的第一聚乙烯(ppm(重量)O 2))。 公开了具有改进的性能,特别是用于电线和电缆应用的聚乙烯组合物。
-
公开(公告)号:US09284415B2
公开(公告)日:2016-03-15
申请号:US14382812
申请日:2012-12-12
Applicant: ExxonMobil Chemical Patents Inc.
Inventor: Gerd A. Allermann , Danny Van Hoyweghen , Steven A. Best , Anthony Poloso , Nicolas M. De Ketelaere
IPC: C08J3/00 , C08J3/20 , C09D123/06 , H01B3/44
CPC classification number: C08J3/005 , C08F8/00 , C08F2810/10 , C08F2810/40 , C08J3/20 , C08J2323/06 , C09D123/06 , H01B3/441 , C08F8/50 , C08F8/06 , C08F210/16 , C08F210/14 , C08F2500/12
Abstract: Processes are disclosed for oxygen-tailoring polyethylene, particularly polyethylenes suitable for wire and cable applications. One process includes conveying a first polyethylene having a melt index ≦5.0 and an MWD ≦5.0 through mixing or extrusion apparatus having a feed zone, a melt-mixing zone downstream of the feed zone, and a melt zone downstream of the melt-mixing zone, wherein the temperature of the first polyethylene in the melt zone ranges from about 180° C. to about 300° C.; and contacting the first polyethylene with an amount of an oxygen-containing gas having at least about 20.0 parts by weight oxygen per million per parts by weight of the first polyethylene (ppm (wt) O2). Polyethylene compositions having improved properties, particularly for wire and cable applications are disclosed.
Abstract translation: 公开了用于氧气聚乙烯,特别是适用于电线和电缆应用的聚乙烯的方法。 一种方法包括通过具有进料区,进料区下游的熔融混合区和熔融区下游的熔融区的混合或挤出装置输送具有熔体指数为< E1和5.0 | MWD&NlE; 5.0的第一聚乙烯, 混合区,其中熔融区中第一聚乙烯的温度为约180℃至约300℃; 并且将第一聚乙烯与一定量的含氧气体接触,所述含氧气体具有至少约20.0重量份的氧每百万重量份的第一聚乙烯(ppm(重量)O 2))。 公开了具有改进性能的聚乙烯组合物,特别是用于电线和电缆应用。
-