Abstract:
The carbon black composition includes carbon black and an amine compound denoted by formula (1) in a solvent: wherein, in formula (1), n denotes an integer falling within a range of 2 to 4, each of U, V, X, and Y independently denotes a substituent that comprises at least one carbon atom and binds, through the carbon atom, to a carbon atom to which the substituent substitutes, and each of W and Z independently denotes a hydrogen atom or a substituent.
Abstract:
The magnetic tape includes a non-magnetic support; and a magnetic layer containing a ferromagnetic powder, in which, in a small-angle X-ray scattering spectrum obtained by small-angle X-ray scattering measurement of the non-magnetic support, in a region where a q-value is 0.01 to 0.10 Å−1, a ratio Imax/Imin of a scattering intensity Imax at a q-value qmax of a maximal value of a scattering intensity change rate to a scattering intensity Imin at a q-value qmin of a minimal value of the scattering intensity change rate is 2.7 or more, and qmin
Abstract:
The magnetic tape includes a non-magnetic support, and a magnetic layer including a ferromagnetic powder. The non-magnetic support is a polyamide support, and a deformation rate ratio of a deformation rate in a width direction to a deformation rate in a longitudinal direction of the magnetic tape, (the deformation rate in the width direction/the deformation rate in the longitudinal direction), is 0.45 or less, the deformation rates each being measured after a load is applied in the longitudinal direction of the magnetic tape for 96 hours.
Abstract:
A magnetic tape management device includes a processor. The processor acquires a temperature and humidity of an environment in which a magnetic tape is stored, derives a specific enthalpy using the temperature and the humidity, and performs management processing on the magnetic tape in accordance with the specific enthalpy.
Abstract:
The magnetic tape includes a non-magnetic support, and a magnetic layer including a ferromagnetic powder. The non-magnetic support is a polyethylene naphthalate support, and a deformation rate ratio of a deformation rate in a width direction to a deformation rate in a longitudinal direction of the magnetic tape, (the deformation rate in the width direction/the deformation rate in the longitudinal direction), is 0.42 or less, the deformation rates each being measured after a load is applied in the longitudinal direction of the magnetic tape for 96 hours.
Abstract:
The magnetic recording medium includes: a non-magnetic support; and a magnetic layer including a ferromagnetic powder and a binding agent on the non-magnetic support, in which the magnetic layer further includes a compound including a polyalkyleneimine chain and a vinyl polymer chain. The composition for a magnetic recording medium includes: ferromagnetic powder; and a compound including a polyalkyleneimine chain and a vinyl polymer chain.
Abstract:
The magnetic recording medium includes: a non-magnetic support; and a magnetic layer including a ferromagnetic powder and a binding agent on the non-magnetic support, in which the magnetic layer further includes a compound including a polyalkyleneimine chain and a vinyl polymer chain. The composition for a magnetic recording medium includes: ferromagnetic powder; and a compound including a polyalkyleneimine chain and a vinyl polymer chain.
Abstract:
The magnetic tape includes: a non-magnetic support; and a magnetic layer including ferromagnetic powder, in which a change amount of a loss tangent tan δ at a measurement temperature in a range of 50° C. to 100° C. before and after heating at 70° C. for 10 hours is 0.000 or more and 0.012 or less.