公开(公告)号:US11198915B2
公开(公告)日:2021-12-14
申请号:US15892122
申请日:2018-02-08
Applicant: Ford Motor Company
Inventor: Raj Sohmshetty , Constantin Chiriac , Mikhail Minevich , Jason Balzer , S. George Luckey, Jr.
IPC: C21D6/00 , C22C38/00 , C21D1/18 , C21D1/58 , C21D1/60 , C21D1/667 , C21D1/673 , C22C38/02 , C22C38/04
Abstract: A method of quenching a press hardenable steel is provided. The method includes an initial step of die quenching a part stamped within a stamping die followed by a partial quenching after the initial step of die quenching. In various methods, the press hardenable steel is a 36MnB5 grade steel and/or the initial step of die quenching is performed at a temperature of approximately 200° C.±10° C. in a die configured for 36MnB5 grade steel. At least one method further includes opening the die followed by the partial quenching, the partial quenching comprising spraying a cooling liquid onto the part to reduce a temperature of the part below approximately 130° C.±10° C., with the option of spraying to reduce the temperature of the part below approximately 100° C.±10° C.
-
公开(公告)号:US20190241987A1
公开(公告)日:2019-08-08
申请号:US15892122
申请日:2018-02-08
Applicant: Ford Motor Company
Inventor: Raj Sohmshetty , Constantin Chiriac , Mikhail Minevich , Jason Balzer , S. George Luckey, JR.
CPC classification number: C21D6/008 , C21D1/18 , C21D1/58 , C21D1/60 , C21D1/667 , C21D1/673 , C21D6/005 , C22C38/02 , C22C38/04
Abstract: A method of quenching a press hardenable steel is provided. The method includes an initial step of die quenching a part stamped within a stamping die followed by a partial quenching after the initial step of die quenching. In various methods, the press hardenable steel is a 36MnB5 grade steel and/or the initial step of die quenching is performed at a temperature of approximately 200° C.±10° C. in a die configured for 36MnB5 grade steel. At least one method further includes opening the die followed by the partial quenching, the partial quenching comprising spraying a cooling liquid onto the part to reduce a temperature of the part below approximately 130° C.±10° C., with the option of spraying to reduce the temperature of the part below approximately 100° C.±10° C.
-