公开(公告)号:US3321828A
公开(公告)日:1967-05-30
申请号:US16392262
申请日:1962-01-02
Applicant: GEN ELECTRIC
Inventor: JOHN MILLER CLARENCE
CPC classification number: B23K35/38 , B23K1/19 , B23K35/284 , B23K35/286 , B23K2201/02 , B23K2201/14 , Y10S428/938 , Y10S428/939 , Y10T428/12764
Abstract: Members of Al or Al alloy are brazed together by providing at the juncture a brazing material having a melting point between 550 DEG C. and the melting point of the member having the lowest melting point and comprising at most 15% Si, at least 0.4% Mg, o-25% Cu, the balance Al, producing a non-oxidizing atmosphere at the juncture and heating to the brazing temperature. Some or all of the components of the brazing material may be included in the members to be joined and additional components may be as sheet, powder or wire.
-
公开(公告)号:US3378914A
公开(公告)日:1968-04-23
申请号:US57377466
申请日:1966-08-08
Applicant: GEN ELECTRIC
Inventor: JOHN MILLER CLARENCE
CPC classification number: B23K35/38 , B23K1/19 , B23K35/284 , B23K35/286 , B23K2201/02 , B23K2201/14 , Y10S428/938 , Y10S428/939 , Y10T428/12764
Abstract: Members of Al or Al alloy are brazed together by providing at the juncture a brazing material having a melting point between 550 DEG C. and the melting point of the member having the lowest melting point and comprising at most 15% Si, at least 0.4% Mg, o-25% Cu, the balance Al, producing a non-oxidizing atmosphere at the juncture and heating to the brazing temperature. Some or all of the components of the brazing material may be included in the members to be joined and additional components may be as sheet, powder or wire.
-
公开(公告)号:US3373482A
公开(公告)日:1968-03-19
申请号:US61613466
申请日:1966-09-19
Applicant: GEN ELECTRIC
Inventor: JOHN MILLER CLARENCE
CPC classification number: B23K1/19 , B23K35/286 , B23K35/38 , B23K2201/14
-
公开(公告)号:US3373483A
公开(公告)日:1968-03-19
申请号:US61613566
申请日:1966-09-19
Applicant: GEN ELECTRIC
Inventor: JOHN MILLER CLARENCE
IPC: B23K35/28
CPC classification number: B23K35/286
-
公开(公告)号:US3322517A
公开(公告)日:1967-05-30
申请号:US33002763
申请日:1963-12-12
Applicant: GEN ELECTRIC
Inventor: JOHN MILLER CLARENCE
CPC classification number: B23K35/38 , B23K1/19 , B23K35/284 , B23K35/286 , B23K2201/02 , B23K2201/14 , Y10S428/938 , Y10S428/939 , Y10T428/12764
Abstract: Members of Al or Al alloy are brazed together by providing at the juncture a brazing material having a melting point between 550 DEG C. and the melting point of the member having the lowest melting point and comprising at most 15% Si, at least 0.4% Mg, o-25% Cu, the balance Al, producing a non-oxidizing atmosphere at the juncture and heating to the brazing temperature. Some or all of the components of the brazing material may be included in the members to be joined and additional components may be as sheet, powder or wire.
-
-
-
-