1.
公开(公告)号:US20250023092A1
公开(公告)日:2025-01-16
申请号:US18352096
申请日:2023-07-13
Applicant: GM GLOBAL TECHNOLOGY OPERATIONS LLC
Inventor: Gongshin QI , Chuanlong Wang , Devendrasinh Darbar , Wei Li
IPC: H01M10/0525 , H01M4/36 , H01M4/505 , H01M4/583 , H01M10/0567 , H01M10/0568 , H01M10/0569
Abstract: A battery that cycles lithium ions includes a positive electrode and an electrolyte infiltrating the positive electrode. The positive electrode includes an electroactive material comprising a lithium-and manganese-rich oxide. The electrolyte includes an organic solvent, an inorganic lithium salt, and a functional additive comprising lithium fluoride (LiF), lithium phosphate (Li3PO4), or a combination thereof.
-
2.
公开(公告)号:US20240360003A1
公开(公告)日:2024-10-31
申请号:US18306910
申请日:2023-04-25
Applicant: GM GLOBAL TECHNOLOGY OPERATIONS LLC
Inventor: Gongshin QI , Devendrasinh Darbar , Raneen Taha , Wei Li
IPC: C01G53/00
CPC classification number: C01G53/50 , C01G53/006 , C01P2004/90 , C01P2006/40
Abstract: A positive electrode material including a layered lithium- and manganese-rich nickel oxide (LMR) doped with an alkali metal and/or an alkaline earth metal. The positive electrode material may be manufactured by preparing a mixture comprising a transition metal carbonate, a dopant metal carbonate, and a lithium source, and then calcining the mixture to form the alkali metal and/or alkaline earth metal-doped LMR.
-
公开(公告)号:US20250105270A1
公开(公告)日:2025-03-27
申请号:US18471510
申请日:2023-09-21
Applicant: GM Global Technology Operations LLC
Inventor: Vamakshi Yadav , Devendrasinh Darbar , Raneen Taha , Wei Li
IPC: H01M4/505 , H01M4/04 , H01M10/0525
Abstract: A cathode active particles for use in a cathode of a lithium ion battery comprising a core includes a lithium-manganese-rich oxide and a coating on the core, wherein the coating includes a lithium manganese spinel. The cathode active particle can be made by preparing a dispersion of particles comprising a lithium-manganese-rich metal oxide in an aqueous solution of a salt of a transition metal oxide. The dispersion is mixed, and heated to a temperature in a range of 60 to 125° C. The solids are separated from the dispersion, and calcined. The cathode active particles can be used in cathode and in a battery comprising such cathode.
-
-