公开(公告)号:US20120186763A1
公开(公告)日:2012-07-26
申请号:US13438137
申请日:2012-04-03
IPC分类号: D21H19/80
摘要: A method for coating paperboard including the steps of preparing a paperboard substrate having a basis weight of at least about 85 pounds per 3000 ft2, with the proviso that the paperboard substrate is not subjected to a wet stack calendering process, applying a basecoat to at least one surface of the paperboard substrate to form a coated paperboard structure, the basecoat including at least one pigment, the pigment having a sediment void volume of at least about 45 percent, and applying a top coat over the basecoat of the coated paperboard structure to form a top-coated paperboard structure having an outermost coating surface, wherein the outermost coating surface has a Parker Print Surf smoothness of at most about 3 microns.
摘要翻译: 一种用于涂布纸板的方法,包括以下步骤:制备基重为至少约85磅/ 3000ft 2的纸板基材,条件是纸板基材不经受湿叠层压延方法,至少应用底涂层 纸板基材的一个表面以形成涂布的纸板结构,底涂层包括至少一种颜料,颜料具有至少约45%的沉积物空隙体积,并且在涂布纸板结构的底涂层上涂覆顶涂层以形成 具有最外涂层表面的顶涂纸板结构,其中最外涂层表面具有至多约3微米的Parker Print Surf平滑度。
-
公开(公告)号:US08187420B2
公开(公告)日:2012-05-29
申请号:US13225594
申请日:2011-09-06
IPC分类号: D21F11/00
摘要: A method for coating paperboard including the steps of preparing a paperboard substrate having a basis weight of at least about 85 pounds per 3000 ft2, with the proviso that the paperboard substrate is not subjected to a wet stack calendering process, applying a basecoat to at least one surface of the paperboard substrate to form a coated paperboard structure, the basecoat including at least one pigment, the pigment having a sediment void volume of at least about 45 percent, and applying a top coat over the basecoat of the coated paperboard structure to form a top-coated paperboard structure having an outermost coating surface, wherein the outermost coating surface has a Parker Print Surf smoothness of at most about 3 microns.
摘要翻译: 一种用于涂布纸板的方法,包括以下步骤:制备基重为至少约85磅/ 3000ft 2的纸板基材,条件是纸板基材不经受湿叠层压延方法,至少应用底涂层 纸板基材的一个表面以形成涂布的纸板结构,底涂层包括至少一种颜料,颜料具有至少约45%的沉积物空隙体积,并且在涂布纸板结构的底涂层上涂覆顶涂层以形成 具有最外涂层表面的顶涂纸板结构,其中最外涂层表面具有至多约3微米的Parker Print Surf平滑度。
-
公开(公告)号:US07749583B2
公开(公告)日:2010-07-06
申请号:US12412773
申请日:2009-03-27
申请人: Gary P. Fugitt , Terrell J. Green , Steve G. Bushhouse , Steven Parker , Jason Richard Hogan , Wei-Hwa Her , Scott Ginther
发明人: Gary P. Fugitt , Terrell J. Green , Steve G. Bushhouse , Steven Parker , Jason Richard Hogan , Wei-Hwa Her , Scott Ginther
IPC分类号: D21H11/20
CPC分类号: D21H19/20 , D21H11/04 , D21H17/63 , D21H17/67 , D21H19/36 , D21H19/54 , Y10T428/1303 , Y10T428/31971 , Y10T428/31978 , Y10T428/31982 , Y10T428/31993
摘要: A paperboard including a solid bleached sulfate paperboard substrate and a coating applied to the paperboard substrate to form a coated structure, the coated structure having a basis weight, a caliper thickness and a Parker Print Surf smoothness, the Parker Print Surf smoothness being at most about 3 microns, the basis weight being at most about Y1 pounds per 3000 ft2, wherein Y1 is a function of the caliper thickness (X) in points and is calculated as follows: Y1=3.79+13.43X−0.1638X2.
摘要翻译: 一种纸板,包括固体漂白硫酸纸纸板基材和涂布在纸板基材上以形成涂层结构的涂层,该涂层结构具有基重,厚度厚度和Parker Print Surf平滑度,Parker Print Surf平滑度最多约为 3微米,单位面积重量最大为每立方英尺约1磅,其中Y1是以钳形厚度(X)为单位的函数,其计算方法如下:Y1 = 3.79 + 13.43X-0.1638X2。
-
公开(公告)号:US20090239047A1
公开(公告)日:2009-09-24
申请号:US12326430
申请日:2008-12-02
CPC分类号: D21H19/44 , C01P2004/20 , C01P2004/54 , C01P2004/61 , C09C1/0081 , C09C1/021 , C09C1/42 , C09D5/028 , C09D17/004 , D21H11/04 , D21H17/63 , D21H17/67 , D21H17/675 , D21H17/69 , D21H19/36 , D21H19/38 , D21H19/385 , D21H19/40 , D21H23/30 , D21H25/005 , G01F17/00 , Y10T428/24901 , Y10T428/25
摘要: A basecoat including a pigment blend of a coarse ground calcium carbonate and a hyperplaty clay having an average aspect ratio of at least about 40:1.
摘要翻译: 包括粗磨碳酸钙和平均长径比为至少约40:1的超平坦粘土的颜料混合物的底漆。
-
公开(公告)号:US08313614B2
公开(公告)日:2012-11-20
申请号:US13438137
申请日:2012-04-03
IPC分类号: D21F11/00
摘要: A method for coating paperboard including the steps of preparing a paperboard substrate having a basis weight of at least about 85 pounds per 3000 ft2, with the proviso that the paperboard substrate is not subjected to a wet stack calendering process, applying a basecoat to at least one surface of the paperboard substrate to form a coated paperboard structure, the basecoat including at least one pigment, the pigment having a sediment void volume of at least about 45 percent, and applying a top coat over the basecoat of the coated paperboard structure to form a top-coated paperboard structure having an outermost coating surface, wherein the outermost coating surface has a Parker Print Surf smoothness of at most about 3 microns.
-
公开(公告)号:US20120145040A1
公开(公告)日:2012-06-14
申请号:US13404151
申请日:2012-02-24
IPC分类号: C09C1/02
CPC分类号: D21H19/44 , C01P2004/20 , C01P2004/54 , C01P2004/61 , C09C1/0081 , C09C1/021 , C09C1/42 , C09D5/028 , C09D17/004 , D21H11/04 , D21H17/63 , D21H17/67 , D21H17/675 , D21H17/69 , D21H19/36 , D21H19/38 , D21H19/385 , D21H19/40 , D21H23/30 , D21H25/005 , G01F17/00 , Y10T428/24901 , Y10T428/25
摘要: A basecoat including a pigment blend that includes a ground calcium carbonate component and a hyperplaty clay component, wherein the ground calcium carbonate component has a coarse particle size distribution, and wherein the hyperplaty clay component has an average aspect ratio of at least about 40:1.
摘要翻译: 一种底涂层,其包括含有研磨碳酸钙组分和高度粘土组分的颜料共混物,其中研磨的碳酸钙组分具有粗大的粒度分布,并且其中所述超平坦粘土组分的平均纵横比为至少约40:1 。
-
公开(公告)号:US08142887B2
公开(公告)日:2012-03-27
申请号:US12326430
申请日:2008-12-02
IPC分类号: B32B5/16
CPC分类号: D21H19/44 , C01P2004/20 , C01P2004/54 , C01P2004/61 , C09C1/0081 , C09C1/021 , C09C1/42 , C09D5/028 , C09D17/004 , D21H11/04 , D21H17/63 , D21H17/67 , D21H17/675 , D21H17/69 , D21H19/36 , D21H19/38 , D21H19/385 , D21H19/40 , D21H23/30 , D21H25/005 , G01F17/00 , Y10T428/24901 , Y10T428/25
摘要: A basecoat including a pigment blend of a coarse ground calcium carbonate and a hyperplaty clay having an average aspect ratio of at least about 40:1.
摘要翻译: 包括粗磨碳酸钙和平均长径比为至少约40:1的超平坦粘土的颜料混合物的底漆。
-
公开(公告)号:US20110315332A1
公开(公告)日:2011-12-29
申请号:US13225594
申请日:2011-09-06
IPC分类号: D21H23/24
摘要: A method for coating paperboard including the steps of preparing a paperboard substrate having a basis weight of at least about 85 pounds per 3000 ft2, with the proviso that the paperboard substrate is not subjected to a wet stack calendering process, applying a basecoat to at least one surface of the paperboard substrate to form a coated paperboard structure, the basecoat including at least one pigment, the pigment having a sediment void volume of at least about 45 percent, and applying a top coat over the basecoat of the coated paperboard structure to form a top-coated paperboard structure having an outermost coating surface, wherein the outermost coating surface has a Parker Print Surf smoothness of at most about 3 microns.
摘要翻译: 一种用于涂布纸板的方法,包括以下步骤:制备基重为至少约85磅/ 3000ft 2的纸板基材,条件是纸板基材不经受湿叠层压延方法,至少应用底涂层 纸板基材的一个表面以形成涂布的纸板结构,底涂层包括至少一种颜料,颜料具有至少约45%的沉积物空隙体积,并且在涂布纸板结构的底涂层上涂覆顶涂层以形成 具有最外涂层表面的顶涂纸板结构,其中最外涂层表面具有至多约3微米的Parker Print Surf平滑度。
-
公开(公告)号:US08025763B2
公开(公告)日:2011-09-27
申请号:US12408197
申请日:2009-03-20
IPC分类号: D21H11/00
摘要: A method for coating paperboard including the steps of preparing a web of cellulosic fibers, the web having a basis weight of at least about 85 pounds per 3000 ft2, calendering the web at least once to form a paperboard substrate, wherein each of the calendering steps is performed without substantially introducing moisture to the web, and applying a basecoat to at least one surface of the paperboard substrate to form a coated paperboard structure, the basecoat including at least one pigment, the pigment having a sediment void volume of at least about 45 percent, wherein the coated paperboard structure has a Parker Print Surf smoothness of at most about 3 microns.
摘要翻译: 一种用于涂布纸板的方法,包括以下步骤:制备纤维素纤维网,所述幅材具有至少约85磅/ 3000ft 2的基重,至少一次压延幅材以形成纸板基底,其中每个压延步骤 在基本上不向所述幅材引入水分的情况下进行,并且将底涂层施加到所述纸板基材的至少一个表面以形成涂布纸板结构,所述底涂层包括至少一种颜料,所述颜料具有至少约45的沉淀物空隙体积 百分比,其中涂布纸板结构具有至多约3微米的Parker Print Surf平滑度。
-
公开(公告)号:US20090236062A1
公开(公告)日:2009-09-24
申请号:US12408197
申请日:2009-03-20
摘要: A method for coating paperboard including the steps of preparing a web of cellulosic fibers, the web having a basis weight of at least about 85 pounds per 3000 ft2, calendering the web at least once to form a paperboard substrate, wherein each of the calendering steps is performed without substantially introducing moisture to the web, and applying a basecoat to at least one surface of the paperboard substrate to form a coated paperboard structure, the basecoat including at least one pigment, the pigment having a sediment void volume of at least about 45 percent, wherein the coated paperboard structure has a Parker Print Surf smoothness of at most about 3 microns.