Method of making high performance activated aluminum sesquichlorohydrate powders
    4.
    发明授权
    Method of making high performance activated aluminum sesquichlorohydrate powders 有权
    制备高性能活性铝倍半水合物粉末的方法

    公开(公告)号:US09572758B2

    公开(公告)日:2017-02-21

    申请号:US14755138

    申请日:2015-06-30

    发明人: Zijun Li

    摘要: Activated aluminum sesquichlorohydrate (AASCH) powders and method of making are disclosed. The AASCH powder has Al:Cl atomic ratio of from about 1.60 to about 1.90 and Band III polymer concentration of at least about 20% and Band IV polymer concentration of at least about 15% when analyzed with Size Exclusion Chromatogram (SEC) operated by High Performance Liquid Chromatograph (HPLC). The method of making the active comprises (a) diluting the concentrated aluminum sesquichlorohydrate (ASCH) solution to from about 10% to about 25% by weight and (b) heating the diluted solution to obtain a Band III polymer concentration of at least about 20% and a Band IV polymer concentration of at least about 15%, and (c) drying the heated solution to powders having Al:Cl ratio of about 1.60 to about 1.90 and (d) optionally screen or light mill the powders to free flowing spherical particles.

    摘要翻译: 公开了活性铝倍半水合物(AASCH)粉末和制备方法。 AASCH粉末具有约1.60至约1.90的Al:Cl原子比和至少约20%的Band III聚合物浓度,并且当用高度操作的尺寸排阻色谱(SEC)分析时,带IV聚合物浓度为至少约15% 高效液相色谱(HPLC)。 制备活性物质的方法包括(a)将浓缩的倍半氯化铝浓缩物(ASCH)溶液稀释至约10重量%至约25重量%,和(b)加热稀释溶液以获得至少约20的Band III聚合物浓度 %,并且带IV聚合物浓度为至少约15%,和(c)将加热的溶液干燥至Al:Cl比为约1.60至约1.90的粉末,和(d)任选地将粉末筛选或轻轻研磨成自由流动的球形 粒子。