公开(公告)号:US4123257A
公开(公告)日:1978-10-31
申请号:US806096
申请日:1977-06-13
CPC分类号: C21B3/04 , C22B1/242 , C22B7/001 , Y02P10/214 , Y02W30/542 , Y10S75/961 , Y10S75/962
摘要: A method of treating a plating sludge is disclosed, wherein a plating sludge, whose water content is decreased to not higher than 10% by weight, is mixed with scale, dust, both of which are formed in the alloy steel-making step, a binder and a carbonaceous material, and water is added to the mixture to adjust the water content of the mixture to 7-30% by weight, the mixture is kneaded and then molded into a briquet, and the briquet is subjected to a strength-improving treatment. The resulting briquet can be used as a raw material for ferroalloy. When the briquet is subjected to a reduction smelting to recover a metal, the metal can be used as a raw material for alloy steel.
摘要翻译: 公开了一种处理电镀污泥的方法,其中将水含量降低至不高于10重量%的电镀污泥与在合金制钢步骤中形成的氧化皮,灰尘, 粘合剂和碳质材料,向混合物中加入水以将混合物的含水量调节至7-30重量%,将混合物捏合,然后模压成团块,并将坯料进行强度提高 治疗。 所得到的砖块可用作铁合金的原料。 当坯料进行还原熔炼以回收金属时,金属可以用作合金钢的原料。
-
公开(公告)号:US4004918A
公开(公告)日:1977-01-25
申请号:US586375
申请日:1975-06-12
申请人: Hiroshi Fukuoka , Teruhiko Kameyama , Yuji Takahashi , Kenji Nicho , Tatsuo Misawa , Tsuneyuki Inoue , Kimiaki Imai
发明人: Hiroshi Fukuoka , Teruhiko Kameyama , Yuji Takahashi , Kenji Nicho , Tatsuo Misawa , Tsuneyuki Inoue , Kimiaki Imai
CPC分类号: C22B7/02 , C21B11/10 , C21B13/0006 , C22B1/242 , Y02P10/214 , Y02P10/224 , Y02P10/23
摘要: A method of treating waste produced during stainless steel making is disclosed. The method comprises the steps of kneading a sludge cake with a mixture of dust and scale to obtain a kneaded mass, adding an organic binder and eventually adding water with an inorganic binder to said kneaded mass, shaping said kneaded mass into a briquette, and heating said briquette at a low temperature. The briquette obtained can be used as a ferroalloy making raw material.Metal oxides contained in the briquette are reduced by a dry reduction refining added with a carbonaceous reducing agent and eventually with a flux to separate usable metals.
摘要翻译: 公开了一种处理在不锈钢制造过程中产生的废弃物的方法。 该方法包括以下步骤:将污泥饼与粉尘和水垢的混合物捏合以获得捏合物料,加入有机粘合剂,最后用无机粘合剂加水至所述捏合物料中,将所述捏合物料成型为团块,加热 在低温下表示团块。 获得的煤块可以用作铁合金原料。
-
公开(公告)号:US4027095A
公开(公告)日:1977-05-31
申请号:US549477
申请日:1975-02-13
CPC分类号: C21C5/5264 , C21B13/0046 , C21B13/006 , C21B13/12 , C21C5/5229 , C21C7/10 , C21C5/5294 , C21C7/0075 , Y02P10/136 , Y02P10/216
摘要: A hermetically sealed arc furnace for producing stainless steel is disclosed which makes use, as a main raw material, a semi-reduced chrome ore pellet and a reduced iron ore pellet and by which these pellets are melted, decarburized and finally refined under a reduced pressure said hermetically sealed arc furnace capable of adjusting its interior reduced pressure, and particularly including a vacuum-tight seal between the furnace lid and furnace body, a telescopically sealed gap between the lid and an electrode extending therethrough and an exhaust opening detachably connected to a vacuum pump for reducing the internal pressure within the furnace.
摘要翻译: 公开了一种用于生产不锈钢的气密电弧炉,其以主要原料为半还原铬矿颗粒和还原铁矿石颗粒,将这些颗粒熔融,脱碳,最后在减压下精炼 所述气密电弧炉能够调节其内部减压,并且特别地包括在炉盖和炉体之间的真空密封,盖和延伸穿过其间的电极之间的可伸缩密封的间隙和可拆卸地连接到真空的排气口 泵用于降低炉内的内部压力。
-
-