公开(公告)号:US5263256A
公开(公告)日:1993-11-23
申请号:US870364
申请日:1992-04-17
Applicant: Hoang M. Trankiem
Inventor: Hoang M. Trankiem
IPC: B05D3/06 , B05D20060101 , B05D1/06 , B05D5/08 , B05D7/14 , B26B21/60 , C08F8/50 , C09D127/12
CPC classification number: B26B21/60 , B05D5/086 , C08J3/28 , B05D2202/00 , B05D2506/15 , C08J2327/18 , Y10T428/3154 , Y10T428/31544
Abstract: The present invention relates to an improved method of forming a polyfluorocarbon coating on a razor blade cutting edge comprising the steps of subjecting a fluorocarbon polymer having a molecular weight of at least about 1,000,000 to ionizing radiation to reduce the average molecular weight to from about 700 to about 700,000; dispersing the irradiated fluorocarbon polymer in an aqueous solution; coating said razor blade cutting edge with the dispersion; and heating the coating obtained to melt, partially melt or sinter the fluorocarbon polymer.
Abstract translation: 本发明涉及一种在剃刀刀片切割刃上形成多氟碳涂层的改进方法,包括以下步骤:使具有至少约1,000,000分子量的氟烃聚合物电离辐射以将平均分子量降低至约700至 约70万; 将被照射的氟碳聚合物分散在水溶液中; 用分散体涂抹剃刀刀片切割刃; 并加热所得到的用于熔融,部分熔融或烧结氟碳聚合物的涂层。
-
2.
公开(公告)号:US5477756A
公开(公告)日:1995-12-26
申请号:US125096
申请日:1993-09-22
Applicant: Hoang M. Trankiem , Manohar S. Grewal
Inventor: Hoang M. Trankiem , Manohar S. Grewal
Abstract: A method of manufacturing a razor blade is disclosed wherein a polymer material is coated onto the blade edge. The polymer material is applied to the blade edge in a coating solution after which the blade is heated to melt the polymer via a radio frequency source, preferably a microwave source.
Abstract translation: 公开了一种制造剃刀刀片的方法,其中将聚合物材料涂覆到刀刃上。 将聚合物材料施加到涂布溶液中的叶片边缘上,然后通过射频源,优选微波源将叶片加热熔融聚合物。
-
公开(公告)号:US5101565A
公开(公告)日:1992-04-07
申请号:US741843
申请日:1991-08-07
Applicant: Hoang M. Trankiem
Inventor: Hoang M. Trankiem
Abstract: Improved razor blades and methods for producing the blades. The cutting edge regions of the blades include a solid adherent coating which is the residue of a heated mixture of a fluorocarbon polymer and a silane. The mixture is applied to the cutting edge regions of the blade and heated to a temperature sufficient to melt the fluorocarbon. The coatings achieved in the practice of the invention provide blades having improved shaving performance characteristics for the blade.
Abstract translation: 改进的刀片和生产刀片的方法。 叶片的切割边缘区域包括固体粘附涂层,其是氟碳聚合物和硅烷的加热混合物的残余物。 将混合物施加到叶片的切割边缘区域并加热到足以熔化碳氟化合物的温度。 在本发明的实践中实现的涂层提供了具有改进的刮刀性能特征的刀片。
-
-