摘要:
An atmospheric leaching process for the recovery of a nickel and cobalt from a lateritic ore, said process including the steps: (a) preparing a slurry of the lateritic ore with saline or hypersaline water having a total dissolved solids (TDS) content greater than 30 g/L; (b) leaching the slurry of the lateritic ore with sulfuric acid at atmospheric pressure, (c) recovering nickel and cobalt from the resultant leachate.
摘要翻译:一种用于从红土矿石中回收镍和钴的大气浸出方法,所述方法包括以下步骤:(a)制备具有大于30的总溶解固体(TDS)含量的盐水或高浓度水的红土矿石浆料 g / L; (b)在大气压下用硫酸浸出红土矿石浆液,(c)从所得浸出液中回收镍和钴。
摘要:
An atmospheric leaching process for the recovery of a nickel and cobalt from a lateritic ore includes (a) preparing a slurry of the lateritic ore with saline or hypersaline water having a total dissolved solids (TDS) content greater than 30 g/L; (b) leaching the slurry of the lateritic ore with sulfuric acid at atmospheric pressure, and (c) recovering nickel and cobalt from the resultant leachate.
摘要:
A method for separating nickel containing lateritic ore into limonite and saprolite fractions that includes subjecting a lateritic ore slurry to a size separation procedure to separate the limonite and saprolite fractions on a selected threshold particle size basis and determining a threshold particle size based on an analysis of particle size fractions by determining a particle size where substantially all of the particles having a characteristic compositional range of at least one indicator element for limonite are smaller than the determined threshold particle size, and/or substantially all of the particles having a compositional range of at least one indicator element for saprolite are larger than a determined threshold particle size.